PL98173B1 - Sposob wytwarzania podpalki - Google Patents
Sposob wytwarzania podpalki Download PDFInfo
- Publication number
- PL98173B1 PL98173B1 PL18096375A PL18096375A PL98173B1 PL 98173 B1 PL98173 B1 PL 98173B1 PL 18096375 A PL18096375 A PL 18096375A PL 18096375 A PL18096375 A PL 18096375A PL 98173 B1 PL98173 B1 PL 98173B1
- Authority
- PL
- Poland
- Prior art keywords
- manufacturing
- fire light
- producing
- mixing
- firestarter
- Prior art date
Description
Przedmiotem wynalazku jest sposób wytwarzania podpalki z odpadów drzewnych.Znany jest na przyklad z polskiego opisu patentowego nr 50037 sposób wytwarzania podpalki z odpadów drzewnych polegajacy na mieszaniu tych odpadów z lepiszczem oraz materialów ulatwiajacych zapalenie podpalki i prasowaniu tej mieszaniny na okreslone ksztaltki.Celem wynalazku jest opracowanie sposobu wytwarzania podpalki o niskiej temperaturze zaplonu, nie wydzielajacej w procesie spalania nieprzyjemnej woni i wyeliminowanie operacji prasowania.Sposób wytwarzania podpalki wedlug wynalazku polega na tym, ze do podgrzanego powyzej temperatury topnienia gaczu dodaje sie trocin o wilgotnosci korzystnie ponizej 16%, w ilosci 35-75%. Po wymieszaniu otrzymany material nabija sie w oslonke wykonana najkorzystniej z folii z tworzywa sztucznego, a nastepnie tnie na odcinki.Sposób wedlug wynalazku ilustruje ponizszy przyklad. Do mieszalnika wprowadzono 80 kg trocin o wilgotnosci 15% oraz 100 kg gaczu barisolowego, podgrzanego do temperatury 75°C. Po dokladnym wymieszaniu otrzymany material przesypano do wytlaczarki i za jej posrednictwem nabito w oslonke wykonana z folii poliamidowej, a nastepnie pocieto na odcinki o dlugosci Im. Otrzymana podpalka posiada niska temperature zaplonu i spala sie latwo bez wydzielania nieprzyjemnych woni oraz dymu.W celu przedluzenia cyklu spalania podpalki nalezy zwiekszyc ilosc trocin w stosunku do ilosci gaczu. Do zapalania wegla lub koksu nalezy uzyc podpalki o masie okolo 0,05 kg. PL
Claims (1)
1. Zastrzezenie patentowe Sposób wytwarzania podpalki z odpadów drzewnych, znamienny tym, ze do podgrzanego powyzej temperatury topnienia gaczu dodaje sie trocin o wilgotnosci korzystnie ponizej 16%;, w ilosci 35-75% i po wymieszaniu otrzymany material nabija sie w oslonke, wykonana najkorzystniej z folii, po czym tnie na okreslone odcinki. PL