PL429128A1 - Sposób spawania i obróbki cieplnej złącza spawanego blach z niskostopowej, trudnościeralnej stali - Google Patents
Sposób spawania i obróbki cieplnej złącza spawanego blach z niskostopowej, trudnościeralnej staliInfo
- Publication number
- PL429128A1 PL429128A1 PL429128A PL42912819A PL429128A1 PL 429128 A1 PL429128 A1 PL 429128A1 PL 429128 A PL429128 A PL 429128A PL 42912819 A PL42912819 A PL 42912819A PL 429128 A1 PL429128 A1 PL 429128A1
- Authority
- PL
- Poland
- Prior art keywords
- max
- wear
- alloy
- low
- resistant steel
- Prior art date
Abstract
Sposób spawania i obróbki cieplnej złącza spawanego blach Brinar 500 z niskostopowej, trudnościeralnej stali, przedstawiony na rysunku, w którym niskostopową, trudnościeralną blachę o grubości od 6 do 12 mm i wyrażonym w procencie wagowym składzie chemicznym: C – 0,25÷0,28; Si - 0,60÷0,68; Mn – 0,90÷1,00; P- max. 0,020; S - max. 0,005; Cr – 0,84÷0,90; Ni - max 0,02; Mo – 0,20÷0,25; Al - max. 0,10; B – max. 0,0008, o równoważniku węgla CEV ≤ 0,65, spawa się metodą MAG (135) stopiwem w proporcji: 8÷12% stopiwa G3Si1 zgodnie z normą EN ISO 14341-A oraz 88÷92% stopiwa GMn4Ni2CrMo zgodnie z normą EN-ISO 16834-A, stosując parametry spawania: prędkość v ≤ 5 mm/s; znamionowy prąd łuku elektrycznego I = 80÷170 A; napięcie łuku elektrycznego U = 18÷28 V; energia liniowa Q ≤ 1,0 kJ/mm; temperatura międzywarstwowa w zakresie Ti < 250°C; przepływ gazu osłonowego w postaci mieszanki Ar + 18% CO2, przepuszczanego w ilości 15 l/min, charakteryzuje się tym, że otrzymane złącze spawane poddaje się normalizowaniu poprzez austenityzowanie w temperaturze 900 ÷ 920°C przez 60 min z chłodzeniem na wolnym powietrzu; kolejno hartowaniu poprzez austenityzowanie w temperaturze 920÷930°C przez 15÷20 min, a następnie chłodzenie w wodzie o temperaturze ≤ 30°C; oraz odpuszczaniu w temperaturze 150°C przez 120 min, po którym złącze chłodzi się na powietrzu.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL429128(22)20190304A PL238090B1 (pl) | 2019-03-04 | 2019-03-04 | Sposób spawania i obróbki cieplnej złącza spawanego blach z niskostopowej, trudnościeralnej stali |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL429128(22)20190304A PL238090B1 (pl) | 2019-03-04 | 2019-03-04 | Sposób spawania i obróbki cieplnej złącza spawanego blach z niskostopowej, trudnościeralnej stali |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| PL429128A1 true PL429128A1 (pl) | 2020-09-07 |
| PL238090B1 PL238090B1 (pl) | 2021-07-05 |
Family
ID=72291489
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PL429128(22)20190304A PL238090B1 (pl) | 2019-03-04 | 2019-03-04 | Sposób spawania i obróbki cieplnej złącza spawanego blach z niskostopowej, trudnościeralnej stali |
Country Status (1)
| Country | Link |
|---|---|
| PL (1) | PL238090B1 (pl) |
Family Cites Families (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN102418036B (zh) * | 2011-06-29 | 2013-07-03 | 南阳汉冶特钢有限公司 | 一种低温压力容器用15MnNiDR低合金钢板及其生产方法 |
| CN103290182A (zh) * | 2013-05-27 | 2013-09-11 | 英山华茂船舶舾装设备有限公司 | 低合金钢铸件的热处理工艺 |
| CN107385156B (zh) * | 2017-06-29 | 2019-01-15 | 江南工业集团有限公司 | 30CrMnSiA钢的强韧化复合热处理方法 |
-
2019
- 2019-03-04 PL PL429128(22)20190304A patent/PL238090B1/pl unknown
Also Published As
| Publication number | Publication date |
|---|---|
| PL238090B1 (pl) | 2021-07-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN105057849B (zh) | 一种1100MPa级热轧超高强高韧钢不预热焊接方法 | |
| CN106346167B (zh) | 一种马氏体耐热钢焊接用焊条 | |
| CN106868425B (zh) | 一种改善690MPa级低C中Mn高强韧中厚板焊接接头低温冲击韧性的焊后热处理方法 | |
| CN102615450A (zh) | 一种超级马氏体不锈钢用实芯焊丝及其制备方法 | |
| CA2714894A1 (en) | Fire-resistant steel material superior in weld heat affected zone reheat embrittlement resistance and low temperature toughness and method of production of same | |
| MX2021003753A (es) | Un metodo de conformado en caliente. | |
| CN113399864A (zh) | 用于t91和tp347h异种钢的焊接方法和焊丝 | |
| MX2021014596A (es) | Soldadura por puntos de resistencia, metodo de soldadura por puntos de resistencia, junta soldada por puntos de resistencia y metodo para fabricar la junta soldada por puntos de resistencia. | |
| JP2017186650A (ja) | 耐酸露点腐食性に優れる溶接鋼管およびその製造法並びに熱交換器 | |
| CN107081508A (zh) | 厚度在15‑20mm的高性能超快冷X70钢的双丝埋弧焊接方法 | |
| PL429128A1 (pl) | Sposób spawania i obróbki cieplnej złącza spawanego blach z niskostopowej, trudnościeralnej stali | |
| JP4951997B2 (ja) | 引張強さが550MPa以上の高張力鋼板の製造方法。 | |
| US20170029923A1 (en) | Weld metal having excellent strength, toughness and sr cracking resistance | |
| PL429129A1 (pl) | Sposób spawania i obróbki cieplnej złącza spawanego blach z niskostopowej, trudnościeralnej stali z borem | |
| Omajane et al. | Weldability of thermo-mechanically rolled steels used in oil and gas offshore structures | |
| PL429407A1 (pl) | Sposób spawania i obróbki cieplnej blach z niskostopowej, martenzytycznej stali odpornej na zużywanie ścierne z borem | |
| PL429400A1 (pl) | Sposób spawania i obróbki cieplnej wysokowytrzymałych blach z martenzytycznej stali odpornej na zużywanie ścierne z borem | |
| WO2021153559A1 (ja) | 溶接鋼管およびその製造方法 | |
| Godin et al. | On-site post-weld heat treatment of welds made of 410NiMo Steel | |
| PL446047A1 (pl) | Sposób spawania i obróbki cieplnej połączeń spawanych stali martenzytycznej z borem | |
| CN103459637B (zh) | 板厚方向的抗疲劳特性优异的厚钢板及其制造方法和使用该厚钢板的角焊接头 | |
| PL431841A1 (pl) | Sposób spawania i obróbki cieplnej martenzytycznej stali borowej o podwyższonej odporności na zużywanie ścierne | |
| Chovet et al. | Effect of various factors on toughness in P92 SAW weld metal | |
| PL446046A1 (pl) | Sposób spawania i obróbki cieplnej połączeń spawanych stali martenzytycznej z borem | |
| RU2458176C1 (ru) | Хладостойкая сталь высокой прочности |