PL409170A1 - Method for obtaining polymer material for the production of the sliding pair elements - Google Patents

Method for obtaining polymer material for the production of the sliding pair elements

Info

Publication number
PL409170A1
PL409170A1 PL409170A PL40917014A PL409170A1 PL 409170 A1 PL409170 A1 PL 409170A1 PL 409170 A PL409170 A PL 409170A PL 40917014 A PL40917014 A PL 40917014A PL 409170 A1 PL409170 A1 PL 409170A1
Authority
PL
Poland
Prior art keywords
production
oil
polymer material
sliding pair
obtaining polymer
Prior art date
Application number
PL409170A
Other languages
Polish (pl)
Other versions
PL226277B1 (en
Inventor
Adam Koniuszy
Tomasz Stawicki
Wiesław Janicki
Paweł Sędłak
Original Assignee
Zachodniopomorski Uniwersytet Technologiczny W Szczecinie
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zachodniopomorski Uniwersytet Technologiczny W Szczecinie filed Critical Zachodniopomorski Uniwersytet Technologiczny W Szczecinie
Priority to PL409170A priority Critical patent/PL226277B1/en
Publication of PL409170A1 publication Critical patent/PL409170A1/en
Publication of PL226277B1 publication Critical patent/PL226277B1/en

Abstract

Sposób otrzymywania materiału polimerowego do wytwarzania elementów par ślizgowych, charakteryzuje się tym, że materiał wykonany z polietylenu PE 300 HD, zanurza się w kąpieli olejowej, w zmodyfikowanym siarką oleju roślinnym i przez 8-20 godziny poddaje nasycaniu tym olejem w temperaturze od 90°C do 115°C, aż do uzyskania równomiernego nasycenie w ilości od 1,5-8% masy początkowej materiału. Stosuje się olej rzepakowy zmodyfikowany siarką w zakresie od 0,1 do 5%. Korzystnie przed kąpielą olejową materiał przemywa się w benzynie ekstrakcyjnej, suszy się i poddaje wygrzewaniu przez 1 godzinę w temperaturze 95°C.The method of obtaining polymeric material for the production of sliding vapor elements is characterized by the fact that the material made of polyethylene PE 300 HD is immersed in an oil bath, in a sulfur-modified vegetable oil and subjected to saturation with this oil at a temperature of 90 ° C up to 115 ° C, until uniform saturation is obtained in an amount of 1.5-8% of the initial mass of the material. Sulfur-modified rapeseed oil is used in the range of 0.1 to 5%. Preferably, the material is washed in extraction naphtha, dried and soaked for 1 hour at 95 ° C before the oil bath.

PL409170A 2014-08-13 2014-08-13 Method for obtaining polymer material for the production of the sliding pair elements PL226277B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL409170A PL226277B1 (en) 2014-08-13 2014-08-13 Method for obtaining polymer material for the production of the sliding pair elements

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL409170A PL226277B1 (en) 2014-08-13 2014-08-13 Method for obtaining polymer material for the production of the sliding pair elements

Publications (2)

Publication Number Publication Date
PL409170A1 true PL409170A1 (en) 2016-02-15
PL226277B1 PL226277B1 (en) 2017-07-31

Family

ID=55299104

Family Applications (1)

Application Number Title Priority Date Filing Date
PL409170A PL226277B1 (en) 2014-08-13 2014-08-13 Method for obtaining polymer material for the production of the sliding pair elements

Country Status (1)

Country Link
PL (1) PL226277B1 (en)

Also Published As

Publication number Publication date
PL226277B1 (en) 2017-07-31

Similar Documents

Publication Publication Date Title
HUE057477T2 (en) Process for the treatment of lignocellulosic biomass by impregnation
HUE051670T2 (en) Process for the treatment of lignocellulosic biomass by impregnation and steam blasting
SI3728410T1 (en) Lignocellulosic biomass treatment process
EP3666785A4 (en) METHOD OF MANUFACTURING MODIFIED LIGNIN, MODIFIED LIGNIN AND MODIFIED LIGNIN RESIN COMPOSITION
EP3318587A4 (en) HYDROGENATED PETROLEUM RESIN AND METHOD FOR PRODUCING THE SAME AND USE THEREOF
PL3490575T3 (en) PLANT EXTRACT WITH HIGHLY CONCENTRATED SAFRANAL, METHOD OF PRODUCTION AND APPLICATION
BR112016030664A2 (en) method for producing furfural from pentosan-containing biomass material
EP3349228A4 (en) ELECTROCONDUCTIVE POLYMER SOLUTION, CAPACITOR AND METHOD FOR PRODUCING CAPACITOR
BR112018005499A2 (en) methods of treating intraocular pressure with tie-2 activators.
EP3702434A4 (en) LUBRICANT COMPOSITION AND ITS PRODUCTION PROCESS
SI3177672T1 (en) Energy-efficient and environmentally friendly process for the production of furfural from lignocellulosic material
HUE057478T2 (en) Process for the treatment of lignocellulosic biomass
ES1156810Y (en) MACHINE FOR THE PRODUCTION OF PLANTS OR LEGAL VEGETABLE GRAFT
EP3354666A4 (en) POLYACRYLAMIDE RESIN, PAPER MAKING ADDITIVE AND PAPER
EP3473696A4 (en) DEVICE AND METHOD FOR PRODUCING BIOFUEL WITH ULTRA LOW SULFUR CONTENT
EP3088491A4 (en) OIL COKE AND PROCESS FOR PRODUCING THE SAME
EP3354731A4 (en) LINALOOL COMPOSITION AND METHOD FOR PRODUCING THE SAME
PL3250042T3 (en) COMPOSITION, METHOD, USE AND PRODUCTION
MX390587B (en) STABLE ETHYLSILICATE POLYMERS AND THEIR MANUFACTURING METHOD.
MX384711B (en) PROCESS FOR PREPARING A POLYMERIC POLYOL.
EP3709425A4 (en) POLYMERIC ELECTROLYTE AND ASSOCIATED PRODUCTION PROCESS
EP3663285C0 (en) FORMYLPYRIDINE DERIVATIVE WITH FGFR4-INHIBITING EFFECT, PRODUCTION METHOD THEREOF AND USE THEREOF
EP3706143A4 (en) SOLID ELECTROLYTE, ELECTRODE, ELECTRICITY STORAGE ELEMENT AND PROCESS FOR PRODUCING SOLID ELECTROLYTE
PL409170A1 (en) Method for obtaining polymer material for the production of the sliding pair elements
EP3372309A4 (en) NICKEL DIATOMATE LAND CATALYST AND PROCESS FOR PRODUCING THE SAME