Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Priority claimed from DE200810026888external-prioritypatent/DE102008026888B4/en
Priority claimed from DE200810026887external-prioritypatent/DE102008026887B4/en
Priority claimed from DE102008048839Aexternal-prioritypatent/DE102008048839A1/en
Application filed by Tridelta Weichferrite GmbhfiledCriticalTridelta Weichferrite Gmbh
Priority claimed from EP09160189.8Aexternal-prioritypatent/EP2131373B1/en
Publication of PL2131373T3publicationCriticalpatent/PL2131373T3/en
Soft magnetic material i.e. manganese zinc ferrite for e.g. transformer, has nano-fraction of soft magnetic material particles with particle size in range of ten to two hundred nano meter, where material is produced by spray drying