PL204604B1 - Method of obtaining high-duty cast iron castings using casting moulds - Google Patents
Method of obtaining high-duty cast iron castings using casting mouldsInfo
- Publication number
- PL204604B1 PL204604B1 PL357961A PL35796102A PL204604B1 PL 204604 B1 PL204604 B1 PL 204604B1 PL 357961 A PL357961 A PL 357961A PL 35796102 A PL35796102 A PL 35796102A PL 204604 B1 PL204604 B1 PL 204604B1
- Authority
- PL
- Poland
- Prior art keywords
- cast iron
- obtaining high
- castings
- casting
- iron castings
- Prior art date
Description
Opis wynalazkuDescription of the invention
Przedmiotem wynalazku jest sposób otrzymywania odlewów w formie odlewniczej z wysokojakościowego żeliwa.The subject of the invention is a method of obtaining castings in a casting mold from high-quality cast iron.
W celu otrzymania odlewów z żeliwa wysokojakoś ciowego niezbę dnym jest wykonanie dwóch podstawowych operacji technologicznych dla ciekłego żeliwa wyjściowego, najpierw sferoidyzację, a następnie modyfikację. Tak przygotowane żeliwo jest wlewane do form odlewniczych. Znane sposoby sferoidyzacji żeliwa wyjściowego przeprowadza się poza formą odlewniczą, w kadzi odlewniczej. Modyfikację ż eliwa przeprowadza się w kadzi odlewniczej wsypując modyfikator do kadzi lub w czasie przelewania żeliwa, wsypując modyfikator na strugę przelewanego ciekłego metalu. Otrzymane w ten sposób żeliwo wysokojakościowe wlewa się do formy odlewniczej otrzymując odlewy z żeliwa wysokojakościowego. Jednym z warunków uzyskania wysokiej jakości odlewów z żeliwa sferoidalnego jest konieczność rozlania całej porcji tak przygotowanego ciekłego żeliwa do form odlewniczych w czasie kilkunastu minut od chwili wykonania operacji sferoidyzacji z uwagi na zanikający w tym czasie efekt sferoidyzacji. W celu przedłużenia czasu trwania efektu sferoidyzacji zwiększa się ilość dodawanego sferoidyzatora, a większa ilość sferoidyzatora z kolei powoduje oprócz powiększenia kosztów produkcji, także występowania różnic w skł adzie chemicznym pomię dzy odlewami otrzymywanymi z pierwszych porcji ż eliwa a ostatnimi co wpływa na brak stabilizacji parametrów technologicznych wykonywanych odlewów. Innymi niepożądanymi zjawiskami to wydłużenie czasu przebiegu wszystkich operacji technologicznych, znaczny spadek temperatury ciekłego żeliwa.In order to obtain high-quality cast iron castings, it is necessary to perform two basic technological operations for the liquid starting cast iron, first spheroidization and then modification. The cast iron prepared in this way is poured into casting molds. Known methods of spheroidizing the starting cast iron are carried out outside the casting mold in a casting ladle. The modification of the cast iron is carried out in the casting ladle by pouring the modifier into the ladle or while pouring the cast iron by pouring the modifier onto the stream of poured liquid metal. The high-quality cast iron obtained in this way is poured into a casting mold to obtain high-quality cast iron castings. One of the conditions for obtaining high-quality ductile iron castings is the need to pour the entire portion of the liquid cast iron prepared in this way into the casting molds within several minutes from the time of the spheroidization operation due to the disappearing spheroidization effect during this time. In order to extend the duration of the spheroidization effect, the amount of spheroidizer added is increased, and the greater amount of spheroidizer, in turn, causes, in addition to increasing production costs, also differences in the chemical composition between the castings obtained from the first portions of iron and the last ones, which affects the lack of stabilization of technological parameters castings made. Other undesirable phenomena are the prolongation of the course of all technological operations, a significant drop in the temperature of the liquid cast iron.
Sposób otrzymywania odlewów z wysokojakościowego żeliwa w formie odlewniczej według wynalazku polega na jednoczesnym przeprowadzeniu operacji sferoidyzacji i modyfikacji żeliwa bezpośrednio w formie odlewniczej podczas zalewania formy ciekłym żeliwem wyjściowym. W sposobie według wynalazku wlewa się ciekłe żeliwo wyjściowe do formy odlewniczej poprzez wlew główny i układ zalewania, w którym znajduje się pierwsza komora reakcyjna z umieszczonym w niej sferoidyzatorem przylegającym bezpośrednio do ceramicznego filtra, następnie żeliwo przepływa przez drugą komorę reakcyjną z umieszczonym w niej modyfikatorem przylegającym do filtra ceramicznego, a następnie wlewami doprowadzającymi wpływa do wnęki formy odtwarzającej kształt odlewu. Żeliwo wyjściowe przepływając w formie przez pierwszą komorę reakcyjną, reaguje z zaprawą sferoidyzującą, powodującą sferoidyzację grafitu, następnie przepływając przez filtr ceramiczny oczyszcza się z pochodzących z kadzi zanieczyszczeń niemetalicznych w postaci zapiaszczeń, zażużleń, a także z nieprzereagowanej zaprawy sferoidyzującej oraz z produktów reakcji żeliwa z zaprawą . Z kolei w drugiej komorze ż eliwo ulega modyfikacji, a filtracja pozbawia żeliwo niepożądanych zanieczyszczeń niemetalicznych powstających podczas modyfikacji oraz pozostałych zanieczyszczeń niewychwyconych przez pierwszy filtr. Proces modyfikacji eliminuje powstawanie cementytu w ściankach odlewu, a zwłaszcza w odlewach cienkościennych. Zainstalowane filtry ceramiczne oprócz funkcji filtrowania powodują zmianę charakteru przepływu ciekłego żeliwa w formie z turbulentnego na laminarny, efektem tego jest mniejsze wymywanie z układu wlewowego i z wnęki formy masy formierskiej przez ciekłe żeliwo. W wyniku zastosowania filtrów ceramicznych mniejsza jest ilość braków odlewniczych spowodowanych wtrąceniami niemetalicznymi, odlewy charakteryzują się lepszymi własnościami mechanicznymi, lepszą obrabialnością. W sposobie według wynalazku w jednej operacji technologicznej zalewania odlewu ciekłym żeliwem przeprowadza się proces sferoidyzacji, modyfikacji i podwójnej filtracji ciekłego żeliwa otrzymując odlewy z żeliwa wysokojakościowego o wysokich własnościach mechanicznych.The method of obtaining high-quality cast iron castings in a casting mold according to the invention consists in simultaneously carrying out the spheroidization and modification of the cast iron directly in the casting mold while pouring the liquid starting cast iron into the mold. In the method according to the invention, liquid stock cast iron is poured into the casting mold through the main head and pouring system, which includes a first reaction chamber with a spheroidizer placed therein adjacent to the ceramic filter, then the cast iron flows through the second reaction chamber with a modifier adhering therein. into the ceramic filter, and then flows through inlets into the mold cavity reproducing the shape of the casting. The initial cast iron, flowing in the mold through the first reaction chamber, reacts with the spheroidizing mortar, causing spheroidization of graphite, then, flowing through the ceramic filter, it is cleaned of non-metallic impurities from the ladle in the form of sand, slag, and unreacted spheroidizing mortar and the reaction products of cast iron with mortar. In turn, in the second chamber, the cast iron is modified, and the filtration deprives the cast iron of undesirable non-metallic impurities formed during the modification and other impurities not caught by the first filter. The modification process eliminates the formation of cementite in the walls of the casting, especially in thin-walled castings. Installed ceramic filters, in addition to the filtering function, change the nature of the flow of liquid cast iron in the form from turbulent to laminar, which results in less leaching from the gating system and from the mold cavity by the liquid cast iron. As a result of the use of ceramic filters, the number of casting defects caused by non-metallic inclusions is smaller, castings are characterized by better mechanical properties and better machinability. In the method according to the invention, in one technological operation of pouring the casting with liquid cast iron, the process of spheroidization, modification and double filtration of the liquid cast iron is carried out, obtaining high-quality cast iron castings with high mechanical properties.
Przykład sposobu otrzymywanie odlewów z wysokojakościowego żeliwa w formie odlewniczej według wynalazku. 40 kg żeliwa wyjściowego o składzie w % wagowych: 3,74% C, 2,45% Si, 0,11% Mn, 0,04% P, 0,007% S i o temperaturze zalewania 1410°C z kadzi syfonowej wiewa się do wlewu formy. W pierwszej komorze żeliwo napotyka 100 g sferoidyzatora przyklejonego do piankowego filtra ceramicznego, zachodzi reakcja sferoidyzacji żeliwa. Z kolei żeliwo przepływa przez ceramiczny filtr piankowy do drugiej komory, a na ceramicznym filtrze piankowym osadzają się produkty reakcji sferoidyzacji i niemetaliczne zanieczyszczenia. W drugiej komorze żeliwo napotyka na przyklejony do piankowego filtra ceramicznego modyfikator w ilości 25 g. Żeliwo rozpuszcza modyfikator i przepływa przez ceramiczny filtr piankowy, na którym osadzają się zanieczyszczenia. Następnie żeliwo poprzez układ wlewowy wpływa do wnęki formy. Otrzymuje się odlew o wadze 26 kg, o następującym składzie chemicznym, w % wagowych: 3,72% C, 2,67% Si,Example of a method for obtaining high-quality cast iron castings in a casting mold according to the invention. 40 kg of initial cast iron with the composition in% by weight: 3.74% C, 2.45% Si, 0.11% Mn, 0.04% P, 0.007% S and the pouring temperature of 1410 ° C is blown from the siphon ladle to the filler forms. In the first chamber, the cast iron meets 100 g of spheroidizer stuck to the foam ceramic filter, the cast iron spheroidization reaction takes place. In turn, the cast iron flows through the ceramic foam filter into the second chamber, and the spheroidization reaction products and non-metallic impurities are deposited on the ceramic foam filter. In the second chamber, the cast iron encounters a modifier in the amount of 25 g adhered to the foam ceramic filter. Cast iron dissolves the modifier and flows through the ceramic foam filter on which the contaminants are deposited. Then the cast iron flows through the gating system into the mold cavity. A cast is obtained, weighing 26 kg, with the following chemical composition, in% by weight: 3.72% C, 2.67% Si,
PL 204 604 B1PL 204 604 B1
0,11% Mn, 0,34% P, 0,007% S i 0,026% Mg, natomiast własności mechaniczne próbek oddzielnie lanych typu Y2 - grubości 25 mm są następujące: wytrzymałość na rozciąganie Rm- = 471 MPa, umowna granica plastyczności R0,2 = 318 MPa, wydłużenie A5 = 21%, twardość HB = 175.0.11% Mn, 0.34% P, 0.007% S and 0.026% Mg, while the mechanical properties of separately cast Y2 samples - 25 mm thick are as follows: tensile strength Rm- = 471 MPa, yield strength R0.2 = 318 MPa, elongation A5 = 21%, hardness HB = 175.
Claims (1)