PL11952B1 - Sposób ulepszania rur wiertniczych i zerdzi plóczkowych. - Google Patents
Sposób ulepszania rur wiertniczych i zerdzi plóczkowych. Download PDFInfo
- Publication number
- PL11952B1 PL11952B1 PL11952A PL1195229A PL11952B1 PL 11952 B1 PL11952 B1 PL 11952B1 PL 11952 A PL11952 A PL 11952A PL 1195229 A PL1195229 A PL 1195229A PL 11952 B1 PL11952 B1 PL 11952B1
- Authority
- PL
- Poland
- Prior art keywords
- pipes
- upgrade
- way
- drill pipes
- filament rods
- Prior art date
Description
Przedmiotem niniejszego wynalazku jest sposób ulepszania rur wiertniczych i zerdzi plóczkowych po ich wykonczeniu zapomoca walcowania. Rury wiertnicze oraz zerdzie musza posiadac wielka wy¬ trzymalosc na rozciaganie i na zewnetrzne cisnienie, oraz musza byc zupelnie wolne od naprezen wewnetrznych.Nowy sposób ulepszenia takich rur, w celu podwyzszenia ich granicy plynnosci, zwiekszania ich ciagliwosci i odpornosci na obciazenie dlugotrwale wszelkiego rodza¬ ju, polega na hartowaniu ich na powietrzu w wadzie lub oliwie, poczem rury te podda¬ je sie jeszcze ewentualnie odpuszczaniu, zaleznie od celu do jakiego rury maja byc uzyte i od ich skladu chemicznego, W ra¬ zie potrzeby mozna potem zastosowac je¬ szcze powtórne hartowanie. Rury te sa wykonywane z zelaza lub stali i moga za¬ wierac domieszki uszlachetniajace oraz do¬ wolna ilosc C. PL
Claims (1)
1. Zastrzezenie patentowe. Sposób ulepszania rur wiertniczych i zerdzi plóczkowych, uzywanych w wiert¬ nictwie, znamienny tern, ze w celu osiagnie¬ cia wysokiej granicy plynnosci, wielkiej ciagliwosci i odpornosci przeciw obciaze¬ niom dlugotrwalym wszelkiego rodzaju, poddaje sie itakie rury hartowaniu, a po- zatem, zaleznie od celu do jakiego rury maja byc uzyte i od ich skladu chemicz¬ nego, odpuszczaniu, po którem moze na¬ stapic powtórne hartowanie. Mannesmannrohren-Werke. Zastepca: Dr, inz. M. Kryzan, rzecznik patentowy. Druk L. Boguslawskiego, Warszawa, PL