NL9201387A - Method and device for preserving paper documents and books - Google Patents

Method and device for preserving paper documents and books Download PDF

Info

Publication number
NL9201387A
NL9201387A NL9201387A NL9201387A NL9201387A NL 9201387 A NL9201387 A NL 9201387A NL 9201387 A NL9201387 A NL 9201387A NL 9201387 A NL9201387 A NL 9201387A NL 9201387 A NL9201387 A NL 9201387A
Authority
NL
Netherlands
Prior art keywords
deacidification
deacidification agent
archives
books
paper
Prior art date
Application number
NL9201387A
Other languages
Dutch (nl)
Original Assignee
Cornelis Jan Stadig
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Cornelis Jan Stadig filed Critical Cornelis Jan Stadig
Priority to NL9201387A priority Critical patent/NL9201387A/en
Publication of NL9201387A publication Critical patent/NL9201387A/en

Abstract

The invention relates to a method for preserving (conserving) archivalia (archive material) by bringing the archivalia to be preserved into substantially permanent contact with a gas- or vapour-forming deacidifying agent (deacidifier), the deacidifying agent being selected from the group consisting of ammonia, morpholine, cyclohexylamine carbonate. The archivalia are brought into contact with the gases or vapours formed by the deacidifying agent by the archivalia being placed in a gastight container at the bottom of which a reservoir with deacidifier is located. The invention further relates to a device for implementing the method.

Description

WERKWIJZE EN INRICHTING VOOR CONSERVERING VAN PAPIEREN DOCUMENTEN EN BOEKENMETHOD AND APPARATUS FOR CONSERVATION OF PAPER DOCUMENTS AND BOOKS

De onderhavige uitvinding heeft betrekking op een werkwijze en inrichting voor het conserveren van papieren documenten en boeken, verder te noemen archivalia.The present invention relates to a method and device for the preservation of paper documents and books, hereinafter referred to as archival materials.

Op dit moment vergaan in archieven en bibliotheken over de gehele wereld documenten en boeken, omdat de zuurgraad van het papier zo sterk toeneemt (waarbij de pH afneemt) , dat de papiercellulose wordt afgebroken, zodat het papier haar samenhang verliest en daardoor onhanteerbaar wordt.Currently, archives and libraries around the world are destroying documents and books because the acidity of the paper increases (with a decrease in pH) that the paper cellulose breaks down, causing the paper to lose its consistency and become unmanageable.

De oorzaak van dit verzuringsproces moet gezocht worden bij de uitvinding van de machinale papierfabricage rond 1800. Voor de zogeheten lijming van de te vormen pa-pierbaan bleek daarbij de toepassing van harsaluin noodzakelijk te zijn. Lijming is noodzakelijk omdat ongelijmd papier als vloeipapier werkt en dus onbeschrijfbaar is.The cause of this acidification process must be sought in the invention of mechanical papermaking around 1800. For the so-called gluing of the paper web to be formed, it appeared that the use of resin alum was necessary. Gluing is necessary because unglued paper acts as blotting paper and is therefore indescribable.

Voor 1800 werden voor het lijmen van handgeschept papier de gerede vellen gedompeld in een gelatineoplossing en vervolgens gedroogd. Harsaluinlijming bleek achteraf het grote nadeel te hebben dat zwavelzuur wordt afgesplitst. Dit zwavelzuur werkt destructief op de cellulose, de hoofdgrondstof van papier, terwijl gelatine dit bezwaar niet had.Before 1800, for gluing handmade paper, the finished sheets were dipped in a gelatin solution and then dried. In retrospect, resin alum gluing proved to have the major drawback that sulfuric acid is split off. This sulfuric acid has a destructive effect on cellulose, the main raw material of paper, while gelatin did not have this drawback.

Verder werd in de 19e eeuw de vraag naar papier zo groot, dat de beschikbare hoeveelheid lompen als cellulose-bron ontoereikend werd. Vanaf circa 1850 werden andere bronnen van cellulose gevonden, zoals allerlei houtsoorten, die door agressieve kookprocessen van de niet-cellulosebe-standdelen, zoals lignine en hemicellulose werden ontdaan. Lignine veroorzaakt het bruin worden van het papier. Deze behandelde cellulosesoorten zijn echter gevoeliger voor verzuring dan cellulose afkomstig van linnen- en katoenlom-pen daar zij door de kookprocessen al vrij ernstig zijn aangetast.In the 19th century, the demand for paper became so great that the available quantity of rags as a source of cellulose became insufficient. From about 1850, other sources of cellulose, such as all kinds of wood, were found, which were removed from the non-cellulose components, such as lignin and hemicellulose, by aggressive cooking processes. Lignin causes the paper to brown. However, these treated cellulosics are more sensitive to acidification than cellulose from linen and cotton rags since they have already been affected quite severely by the cooking processes.

Er zijn reeds verschillende methoden ontwikkeld om de in zure archivalia voorkomende zuren te neutraliseren. Waterige oplossingen van calciumbicarbonaat, magnesiumbicar- bonaat en calciumhydroxide zijn daartoe zeer geschikt.Various methods have already been developed to neutralize the acids found in acidic archives. Aqueous solutions of calcium bicarbonate, magnesium bicarbonate and calcium hydroxide are very suitable for this.

Helaas verliest nat papier een belangrijk deel van haar sterkte, hetgeen funest kan zijn voor archivalia die zich reeds in een slechte conditie bevinden. Een ander nadeel is het feit dat bij het waterig ontzuren van boeken het gehele boek uiteen genomen moet worden, waarna elke bladzijde ontzuurd en gedroogd moet worden, alvorens opnieuw tot een boek ingebonden te kunnen worden. Deze handmatige bewerkingen zijn sterk kostenverhogend.Unfortunately, wet paper loses an important part of its strength, which can be disastrous for archives that are already in poor condition. Another drawback is the fact that, in the case of aqueous deacidification of books, the entire book must be disassembled, after which each page must be deacidified and dried, before it can be bound again into a book. These manual operations greatly increase costs.

Een ontzuringsmethode die deze nadelen niet heeft is de bewerking met het indirekt werkende diethylzinkgas (DEZ). Deze ontzuringsmethode, die bekend staat onder de naam DEZ-methode, berust op de eigenschap van DEZ om in aanraking met een geringe hoeveelheid vocht in het papier te ontleden in etheengas en zinkoxide (ZnO), dat de zuren bindt. Om in het papier een zogeheten alkalische reserve te vormen wordt het ZnO met koolzuur omgezet in zinkcarbonaat. Deze buffer is noodzakelijk om eventueel later gevormde zuren, door bijvoorbeeld zure regen, te neutraliseren.A deacidification method that does not have these drawbacks is processing with the indirect acting diethyl zinc gas (DEZ). This deacidification method, known as the DEZ method, is based on the property of DEZ to decompose in contact with a small amount of moisture in the paper into ethylene gas and zinc oxide (ZnO), which binds the acids. In order to form a so-called alkaline reserve in the paper, the ZnO is converted into zinc carbonate with carbon dioxide. This buffer is necessary to neutralize any acids formed later, for example by acid rain.

Aangezien bij het natuurlijk evenwichtsvochtgehalte van papier (8-10% bij 65% relatieve vochtigheid) het DEZ een explosie kan veroorzaken, moet het papier voorgedroogd worden tot een zo laag mogelijk vochtgehalte. Deze geringe resthoeveelheid is echter al voldoende om het DEZ te ontleden in zinkoxide en ethaan.Since at the natural equilibrium moisture content of paper (8-10% at 65% relative humidity) the DEZ can cause an explosion, the paper must be pre-dried to the lowest possible moisture content. However, this small residual amount is already sufficient to decompose the DEZ into zinc oxide and ethane.

Onder verantwoordelijkheid van het Library of Congres (LOC, Verenigde Staten) zijn de afgelopen jaren een aantal ontzuringsproeven van boeken met DEZ uitgevoerd. Hierbij werd voor respectievelijk het voordrogen van de boeken, het impregneren in vacuüm met DEZ-gas, het omzetten van het gevormde zinkoxide met C02 in zinkcarbonaat en tenslotte voor het DEZ-vrij spoelen van tanks en boeken, gebruik gemaakt van gróte NASA vacuümtanks. Bij deze proeven zijn de laatste jaren enkele explosies opgetreden, die het DEZ-procedé in een ongunstig daglicht hebben geplaatst. Later is het project overgedragen aan Texas-Alkyls (AKZO) die een aantal verbeteringen heeft aangebracht, waardoor de kans op explosies veel minder zou zijn. J.C. Thomson be- schrijft in zijn publicatie "Mass-deacidification; Thoughts on the Cunha report", Restorator 9, nummer 3 (1988), p. 147-162, echter nog steeds een groot aantal nadelen van het procédé. Het is waarschijnlijk dat het DEZ-procédé in Europa weinig kans van slagen heeft, omdat de bewerking zal moeten plaats vinden in één centraal ontzuringsbedrijf. Dit brengt uiteraard een groot aantal logistieke problemen met zich mee. Daarbij komt dat in het algemeen bibliothecarissen en archivarissen het ontzuringsproces liefst in eigen huis zouden willen uitvoeren.In recent years, a number of deacidification tests of books with DEZ have been carried out under the responsibility of the Library of Congress (LOC, United States). For the pre-drying of the books, the impregnation in vacuum with DEZ gas, the conversion of the formed zinc oxide with CO2 into zinc carbonate and finally for the DEZ-free rinsing of tanks and books, large NASA vacuum tanks were used. These tests have seen a number of explosions in recent years, which have put the DEZ process in an unfavorable light. Later, the project was transferred to Texas-Alkyls (AKZO) who made a number of improvements that would reduce the chance of explosions. J.C. Thomson, in his publication "Mass-deacidification; Thoughts on the Cunha report", Restorator 9, number 3 (1988), p. 147-162, however, still many disadvantages of the process. It is likely that the DEZ process in Europe has little chance of success, because the processing will have to take place in one central deacidification company. This naturally entails a large number of logistical problems. In addition, in general, librarians and archivists would prefer to carry out the deacidification process in-house.

Bij een andere methode van niet-waterige ontzuring wordt gebruik gemaakt van de chemische verbinding methylme-thoxymagnesiumcarbonaat (MMMC) opgelost in een mengsel van methanol en Freon-113. Deze laatste stof staat bekend als CFK en tast de ozonlaag aan. Binnenkort zal het gebruik van CFK's dan ook verboden zijn. Het procédé is beschreven in U.S. octrooi 4.318.963. De werking van MMMC berust op haar eigenschap om te ontleden zodra het in aanraking komt met water, dat normaal in papier aanwezig is in een hoeveelheid van 8-10%. Hierbij ontstaan magnesiumhydroxide en magnesi-umcarbonaat, welke de zuren in het papier neutraliseren en een zogenaamde alkalische reserve vormen. Door het lage kookpunt van Freon van 40‘C is een MMMC-oplossing geschikt om te verspuiten met een spuitpistool ("Soft-spray-methode" genoemd), dat een fijne nevel vormt. Zodra deze in aanraking komt met het te ontzuren papieroppervlak, ontleedt het MMMC in haar componenten. Op deze manier kunnen behalve vlakke documenten ook boeken ontzuurd worden door blad voor blad te bespuiten. Het is duidelijk dat dit een zeer bewerkelijke methode is en ongeschikt voor massa-ontzuring.Another method of non-aqueous deacidification uses the chemical compound methyl methoxymagnesium carbonate (MMMC) dissolved in a mixture of methanol and Freon-113. The latter is known as CFC and affects the ozone layer. The use of CFCs will therefore soon be prohibited. The process is described in U.S. Pat. U.S. Patent 4,318,963. The action of MMMC is based on its ability to decompose as soon as it comes into contact with water, which is normally present in paper in an amount of 8-10%. This produces magnesium hydroxide and magnesium carbonate, which neutralize the acids in the paper and form what is known as an alkaline reserve. Freon's low boiling point of 40 "C makes an MMMC solution suitable for spraying with a spray gun (called" soft spray method "), which forms a fine mist. As soon as it comes into contact with the paper surface to be deacidified, the MMMC decomposes into its components. In this way, besides flat documents, books can also be deacidified by spraying sheet by sheet. It is clear that this is a very laborious method and unsuitable for mass deacidification.

Massa-ontzuring van boeken betekent het door middel van een ontzuringsvloeistof ontzuren en daarna drogen van een groot aantal boeken en/of documenten tegelijkertijd, in bijvoorbeeld een tank. Hierbij moeten de boeken bij indirecte procédés, zoals met DEZ en MMMC, eerst voorgedroogd worden tot een zo laag mogelijk vochtgehalte aangezien de ontzuringsvloeistoffen anders ter plekke van de bladzijranden van het boek het eerst zullen ontleden en een ongelijk matige pH verdeling zullen veroorzaken. Nu bevat cellulose 2 a 3% vastgehouden water dat zelfs in diep vacuüm boven 100°C niet verwijderd kan worden. Het voordrogen tot absoluut droog, is derhalve onmogelijk en het lijkt niet waarschijnlijk dat ontzuringsprocessen, waarbij het papier voorgedroogd moet worden, erg succesvol zullen zijn. Bij vlakke documenten die nooit voorgedroogd worden vormt de spuitnevel dan ook een alkalische geleiachtige laag met een hoge concentratie van magnesiumcarbonaat en magnesiumhydroxide en een hoge pH.Mass deacidification of books means deacidification by means of an deacidification liquid and then drying a large number of books and / or documents at the same time, for example in a tank. In indirect processes, such as with DEZ and MMMC, the books must first be pre-dried to the lowest possible moisture content, as otherwise the deacidification liquids will decompose first at the side edges of the book and cause an uneven pH distribution. Cellulose now contains 2 to 3% retained water that cannot be removed even in deep vacuum above 100 ° C. Pre-drying to absolute dryness is therefore impossible and it does not seem likely that deacidification processes requiring the paper to be pre-dried will be very successful. For flat documents that are never pre-dried, the spray forms an alkaline jelly-like layer with a high concentration of magnesium carbonate and magnesium hydroxide and a high pH.

Bij eigen proeven, waarbij de boeken voorgedroogd waren en daarna in een MMMC-oplossing gedompeld, bleek dat de ontzuring van de bladen ongelijkmatig verliep, hoewel de penetratie van het oplosmiddel wel goed was. De pH over het blad gemeten was dan ook ongelijkmatig (tabel 1).Own tests, in which the books were pre-dried and then immersed in an MMMC solution, showed that the deacidification of the sheets was uneven, although the penetration of the solvent was good. The pH measured over the leaf was therefore uneven (Table 1).

TABEL 1 pH verdeling over de bladzijden voor en na impregneren van een boek in gesloten toestand door middel van de MMMC-metho-de.TABLE 1 pH distribution over the pages before and after impregnation of a closed book by means of the MMMC method.

NIET BEHANDELD GEÏMPREGNEERD GEÏMPREGNEERDUNTREATED IMPREGNATED IMPREGNATED

EN GEDROOGD EN GEDROOGDAND DRIED AND DRIED

a.d. LUCHT ONDER VACUÜMa.d. AIR UNDER VACUUM

Figure NL9201387AD00051

Duidelijk blijkt uit tabel 1 dat alleen de randen van het > blad goed geneutraliseerd zijn, maar het middengedeelte niet. Vermoedelijk komt dit doordat de geringe hoeveelheid vastgebonden water van 2 & 3% die na voordroging in het papier achterblijft, al voldoende is om het MMMC te ontleden zodra haar oplossing met het papier in aanraking komt, dus bij de randen.It is clear from table 1 that only the edges of the> leaf are well neutralized, but the middle part is not. This is probably because the small amount of taped water of 2 & 3% that remains in the paper after pre-drying is already sufficient to decompose the MMMC as soon as its solution comes into contact with the paper, ie at the edges.

Andere problemen, die bij het impregneren van boeken met MMMC-oplossingen en in het algemeen met organische oplosmiddelen kunnen optreden zijn: het verweken van bepaalde lijmsoorten, het verkleuren van druk en grafiek en extractie van bruine verkleuring. Een ander probleem is het feit dat het tot nu toe niet gelukt is om de laatste resten methanol uit het papier te verwijderen, zelfs in diep vacuum, waardoor de behandelde boeken bij opslag gaan 'stinken'.Other problems that can arise when impregnating books with MMMC solutions and generally with organic solvents are: softening of certain glues, discolouration of pressure and graphics and extraction of brown discoloration. Another problem is the fact that until now it has not been possible to remove the last residues of methanol from the paper, even in deep vacuum, which causes the treated books to 'stink' on storage.

Uit het bovenstaande kan men dus concluderen dat oplossingen van MMMC in organische oplosmiddelen eveneens ongeschikt zijn voor massa-ontzuring van boeken.From the above it can thus be concluded that solutions of MMMC in organic solvents are also unsuitable for mass deacidification of books.

De onderhavige uitvinding heeft tot doel een werkwijze en inrichting te verschaffen voor het door middel van massa-ontzuring conserveren van archivalia, waarmee de hierboven geschetste problemen vermeden worden.The object of the present invention is to provide a method and apparatus for preserving archival materials by mass deacidification, thereby avoiding the above-outlined problems.

Dit wordt door de uitvinding bereikt door het in hoofdzaak permanent in contact brengen van de te conserveren archivalia met een gas- of dampvormend ontzuringsmiddel.This is achieved by the invention by substantially permanently contacting the preservatives to be preserved with a gas or vapor-forming deacidification agent.

Bij voorkeur wordt het gas- of dampvormend ontzuringsmiddel gekozen uit de groep die bestaat uit ammoniumbi-carbonaat, ammonia, morfoline, cyclohexylamine carbonaat. In het bijzonder komt in aanmerking ammoniakgas dat zich ontwikkelt uit ammonia, dit is een 25% oplossing in water. De meeste voorkeur gaat uit naar ammoniumbicarbonaat. Omdat dit een vaste stof is, die langzaam ammoniak afscheidt, treden geen problemen op met het vochtig worden van de archivalia en wordt ook de overheersende ammoniakgeur vermeden.Preferably, the gas or vapor-forming deacidification agent is selected from the group consisting of ammonium bicarbonate, ammonia, morpholine, cyclohexylamine carbonate. In particular ammonia gas that develops from ammonia, this is a 25% solution in water. Most preferred is ammonium bicarbonate. Since this is a solid which slowly secretes ammonia, there is no problem with the moistening of the archives and the predominant ammonia odor is also avoided.

I Genoemde ontzuringsmiddelen zijn op zichzelf reeds bekend. De moeilijkheid is dat de zuren die het verval van papier veroorzaken sterke zuren zijn en alleen met sterke basen geneutraliseerd kunnen worden. Bovengenoemde gasvormige basen zijn echter zwak, waardoor de werking slechts van > korte duur is. Door nu echter de archivalia in hoofdzaak permanent in contact te houden met het ontzuringsmiddel wordt een blijvende neutralisatie bereikt.Said deacidification agents are already known per se. The difficulty is that the acids that cause paper decay are strong acids and can only be neutralized with strong bases. However, the above-mentioned gaseous bases are weak, so that the action is only of short duration. However, by now keeping the archives substantially in permanent contact with the deacidification agent, a permanent neutralization is achieved.

De uitvinding verschaft verder een inrichting voor het uitvoeren van de werkwijze, omvattende een gasdichte houder, een reservoir voor ontzuringsmiddel en een gasdoor-latende afscheiding tussen het reservoir en de te conserveren van de archivalia.The invention further provides an apparatus for carrying out the method comprising a gas-tight container, a deacidification agent reservoir and a gas-permeable partition between the reservoir and the preservatives of the archives.

De archivalia worden bijvoorbeeld bewaard in gasdichte kartonnen archiefdozen, waarin op de bodem het poedervormige ammoniumbicarbonaat of een laag schuimrubber geïmpregneerd met 25% ammonia of morfoline geplaatst is. Hierboven bevindt zich een metalen rooster waarop de boeken rusten. In of op de archiefdoos kan zich eventueel een pH-indicator bevinden voor het aangeven van de concentratie van het ontzuringsmiddel.The archives are stored, for example, in gastight cardboard archive boxes, in which the powdered ammonium bicarbonate or a layer of foam rubber impregnated with 25% ammonia or morpholine is placed on the bottom. Above it is a metal grid on which the books rest. There may be a pH indicator in or on the archive box to indicate the concentration of the deacidification agent.

De onderhavige uitvinding wordt geïllustreerd door middel van bijgaande figuur, waarin een gedeeltelijk weggebroken perspectivisch aanzicht van een uitvoeringsvorm van een inrichting volgens de uitvinding getoond wordt.The present invention is illustrated by means of the accompanying figure, in which a partly broken away perspective view of an embodiment of a device according to the invention is shown.

In een archiefdoos 1, bijvoorbeeld uitgevoerd in gasdicht karton, bevindt zich een laag schuim 2. Het schuim is geïmpregneerd met ontzuringsmiddel en wordt afgedekt door middel van een bij voorkeur metalen rooster 3. Op het rooster bevinden zich de te behandelen boeken 4. In het deksel is een pH-indicator 5 opgenomen.A filing box 1, for instance made of gastight cardboard, contains a layer of foam 2. The foam is impregnated with deacidifying agent and is covered by means of a preferably metal grid 3. On the grid are the books to be treated 4. In the lid has a pH indicator 5 included.

Uit proefbehandelingen is gebleken dat de boeken binnen enkele uren met het neutraliserend gas zijn geïmpregneerd en dat de pH-verdeling over het blad goed is (tabel 2).Experimental treatments have shown that the books are impregnated with the neutralizing gas within a few hours and that the pH distribution over the sheet is good (Table 2).

TABEL 2 pH-verdeling over de bladzijden voor en na behandeling volgens de uitvindingTABLE 2 pH distribution over the pages before and after treatment according to the invention

NIET BEHANDELD BEHANDELDNOT TREATED TREATED

Figure NL9201387AD00071

Het is mogelijk de archivalia tijdens de opslag te gebruiken. Na de impregnering en voor gebruik dienen de objecten dan echter wel aan de lucht of in een geforceerde luchtstroom ontgast te worden. In deze toestand blijven de bladen enkele weken neutraal (pH circa 7,0). Hierna dienen zij weer in de archiefdozen geplaatst te worden.It is possible to use the archives during storage. However, after impregnation and before use, the objects must be degassed in the air or in a forced air flow. In this condition, the blades remain neutral for several weeks (pH about 7.0). After this they have to be placed back in the archive boxes.

Bovenbeschreven gasontzuring kan blijvend zijn of tijdelijk, bijvoorbeeld wanneer de archivalia geselecteerd worden voor een neutraliserende vloeistofimpregnatie, welke een blijvende ontzuring verschaft. Tot die tijd is het mogelijk met behulp van de onderhavige uitvinding op eenvoudige en relatief goedkope wijze het verval van het papier tot staan te brengen. De werkwijze kan daarnaast in elk archief uitgevoerd worden en vereist geen kostbare installatie en nauwelijks of geen extra ruimte.The gas deacidification described above can be permanent or temporary, for example when the archives are selected for a neutralizing liquid impregnation, which provides a permanent deacidification. Until then, it is possible with the aid of the present invention to stop the decay of the paper in a simple and relatively inexpensive manner. The method can also be carried out in any archive and requires no expensive installation and little or no extra space.

Claims (14)

1. Werkwijze voor het conserveren van archivalia, door het in hoofdzaak permanent in contact brengen van de te conserveren archivalia met een gas- of dampvormend ontzu-ringsmiddel.1. A method for the preservation of archival materials, by substantially permanently contacting the archival materials to be preserved with a gas- or vapor-forming degreaser. 2. Werkwijze volgens conclusie 1, met het kenmerk, dat het ontzuringsmiddel wordt gekozen uit de groep die bestaat uit ammoniumbicarbonaat, ammonia, morfoline, cyclo-hexylamine carbonaat.Process according to claim 1, characterized in that the deacidification agent is selected from the group consisting of ammonium bicarbonate, ammonia, morpholine, cyclohexylamine carbonate. 3. Werkwijze volgens conclusie 1 of 2, met het kenmerk, dat de archivalia in contact gebracht worden met door het ontzuringsmiddel gevormde gassen of dampen door het in een gasdichte houder, op de bodem waarvan zich een reservoir met ontzuringsmiddel bevindt, plaatsen van de archivalia.Method according to claim 1 or 2, characterized in that the archives are brought into contact with gases or vapors formed by the deacidification agent by placing the archives in a gastight container, on the bottom of which is a reservoir with deacidification agent. . 4. Werkwijze volgens conclusie 3, met het kenmerk, dat het ontzuringsmiddel in gas- of dampvorm wordt afgegeven door een laag van een poreus materiaal, dat geïmpregneerd is met het ontzuringsmiddel.A method according to claim 3, characterized in that the deacidification agent in gaseous or vapor form is released through a layer of a porous material impregnated with the deacidification agent. 5. Werkwijze volgens één der conclusies 1-4, met het kenmerk, dat de archivalia voor gebruik daarvan voor een gewenst doel eerst ontgast worden.A method according to any one of claims 1-4, characterized in that the archives are first degassed for use for a desired purpose. 6. Werkwijze volgens conclusie 5, met het kenmerk, dat ontgassing plaats vindt aan de lucht.Method according to claim 5, characterized in that degassing takes place in the air. 7. Werkwijze volgens conclusie 5, met het kenmerk, dat ontgassing plaats vindt in een geforceerde luchtstroom.Method according to claim 5, characterized in that degassing takes place in a forced air flow. 8. Inrichting voor het uitvoeren van de werkwijze volgens één der conclusies 1-7, omvattende een gasdichte houder, een reservoir voor ontzuringsmiddel en een gasdoor-latende afscheiding tussen het reservoir en de te conserveren van de archivalia.Apparatus for carrying out the method according to any one of claims 1-7, comprising a gastight container, a deacidification agent reservoir and a gas-permeable partition between the reservoir and the archives to be preserved. 9. Inrichting volgens conclusie 8, met het kenmerk, dat de houder een gasdichte kartonnen archiefdoos is.Device according to claim 8, characterized in that the container is a gastight cardboard archive box. 10. Inrichting volgens conclusie 8 of 9 met het kenmerk, dat het reservoir voor ontzuringsmiddel een laag poreus materiaal is.Device according to claim 8 or 9, characterized in that the deacidification agent reservoir is a layer of porous material. 11. Inrichting volgens conclusie 10, met het kenmerk, dat het poreuze materiaal schuimrubber is.Device according to claim 10, characterized in that the porous material is foam rubber. 12. Inrichting volgens één der conclusies 8-11, met het kenmerk, dat de gasdoorlatende afscheiding wordt gevormd door een rooster van inert materiaal.Device according to any one of claims 8-11, characterized in that the gas-permeable partition is formed by a grid of inert material. 13. Inrichting volgens conclusie 12, met het kenmerk, dat het inerte materiaal een inert metaal is.Device according to claim 12, characterized in that the inert material is an inert metal. 14. Inrichting volgens één der conclusies 8-13, met het kenmerk, dat de inrichting is voorzien van een pH-indicator .Device according to any one of claims 8-13, characterized in that the device is provided with a pH indicator.
NL9201387A 1992-07-01 1992-07-31 Method and device for preserving paper documents and books NL9201387A (en)