I 8 AIR DRYING WATERBORNE, RF,SIN COMPOSITION ABSTRACT: .A-N AIR DRYING WATERBOME RESIN COMPOSITION IS DISCLOSED. SAID RESIN COMPOSITION COMPRISES IT LEAST ONE AMPHIPHILIC AIR DR-YING DENDRITIC POLVMER, AT LEAST ONE NON-AMPHIPHILIC AIR DRYING ALK-YD 5 RESIN, AT LEAST ONE DRIER INITIATING AND/OR PIORNOLING AULOXIDANOTI, AND WAIER. AND OPTIONALLY AT LEAST ONE ANIONIC AND/OI NOMORUC SURFACTANI, ARLD/OR AT LEAST ORLE COALESCENT AGENT. SAID AT LEAST ONE AMPHIPHILIC AIR DR@ING DENDRITIC POINQNER IS BUILT UP FROM A POLYHYDRIC DENDMIC CORE POLVINER HAVIN' TERMINAL HYDROXYL GROUPS AND AT LEAST ONE UNSATURATED CARBOXV1IC ACID ARID AT LEAST ONE ADDUCT, OBTAINABLE BY ADDITION OF A MONOALK-VLAIED POLVETHYLENE GLYCOL TO A I 0 DICARBOXYLIC ACID OR ANHYDRIDE AND/OR A DIISOCYANAIE, EACH BORIDED TO AT LEAST ORLE TERRINNAL HYDROXYL GROUP IN SAID POLYLLYDRIC DENDRITIC CORE POLYNIET.