مولد البخار مع مكواة مُشكَّل من خزانين (1)، (1 '') مدرج أسفل طرفي المولِّد. يخرج البخار في الجزء العلوي من خلال الأنابيب (7)، (8)، ويأتي لينتشر في المكان من خلال منفذ وبشكل مباشر إلى المكواة.The steam generator with an iron formed from two reservoirs (1) and (1) is listed below the generator ends. The steam comes out at the top through pipes (7), (8) and comes to spread in place through the outlet and directly to the iron.
Process to make a natural nano-reinforcement, from natural silicate of volcanic origin of the sodium montmorillonite type with a size under 2 µm that includes fractionation and wet treatment, incorporating only a deflocculant-flocculant at room temperature; nano-reinforcement and its use to produce nanocomposites.