KR970024361A - SOLID ELECTROLYTE FUEL CELL WITH AN IRREGULARITY SURFACE - Google Patents

SOLID ELECTROLYTE FUEL CELL WITH AN IRREGULARITY SURFACE Download PDF

Info

Publication number
KR970024361A
KR970024361A KR1019950035032A KR19950035032A KR970024361A KR 970024361 A KR970024361 A KR 970024361A KR 1019950035032 A KR1019950035032 A KR 1019950035032A KR 19950035032 A KR19950035032 A KR 19950035032A KR 970024361 A KR970024361 A KR 970024361A
Authority
KR
South Korea
Prior art keywords
fuel cell
solid electrolyte
electrolyte fuel
electrolyte
present
Prior art date
Application number
KR1019950035032A
Other languages
Korean (ko)
Other versions
KR0153307B1 (en
Inventor
한영희
서일영
한이섭
윤종민
Original Assignee
우덕창
쌍용양회공업 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 우덕창, 쌍용양회공업 주식회사 filed Critical 우덕창
Priority to KR1019950035032A priority Critical patent/KR0153307B1/en
Publication of KR970024361A publication Critical patent/KR970024361A/en
Application granted granted Critical
Publication of KR0153307B1 publication Critical patent/KR0153307B1/en

Abstract

본 발명은 산소 이온화 반응이 주로 일어나는 삼상 계면의 면적을 늘리기 위하여 전해질 분말의 도포 등의 방법으로 전해질 표면에 요철을 주고 공기극 전극을 입히는 방법으로 고체 전해질 연료 전지의 분극 현상을 개선하여 전지 성능을 향상시킬 수 있는 표면 요철을 갖는 고체 전해질 연료 전지를 제공하기 위한 것이다.The present invention improves the cell performance by improving the polarization phenomenon of the solid electrolyte fuel cell by applying unevenness to the surface of the electrolyte and coating the cathode electrode in order to increase the area of the three-phase interface in which the oxygen ionization reaction mainly occurs. It is to provide a solid electrolyte fuel cell having surface irregularities.

본 발명의 표면 요철을 갖는 고체 전해질 연료 전지는 전해질 표면에 1㎛ 이상의 직경을 갖는 전해질 분말을 20㎛ 이하의 두께로 스프레이법 또는 스크린 인쇄법에 의해 도포하고 여기에 공기극 물질을 입혀서 된 것임을 특징으로 한다.The solid electrolyte fuel cell having the surface irregularities of the present invention is characterized by applying an electrolyte powder having a diameter of 1 μm or more to the surface of the electrolyte by a spray method or a screen printing method with a thickness of 20 μm or less, and coating the cathode material thereon. do.

본 발명의 장점은 공기극의 분극 저항을 획기적으로 감소시켜 연료 전지의 성능을 종래 보다 15% 이상 증가 시킴에 따라 상용시 막대한 연료의 절감 효과를 나타낼 수 있다.An advantage of the present invention is to dramatically reduce the polarization resistance of the air electrode to increase the performance of the fuel cell by 15% or more than the conventional can exhibit a significant fuel savings in commercial use.

Description

표면 요철을 갖는 고체 전해질 연료 전지(SOLID ELECTROLYTE FUEL CELL WITH AN IRREGULARITY SURFACE)SOLID ELECTROLYTE FUEL CELL WITH AN IRREGULARITY SURFACE

본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음As this is a public information case, the full text was not included.

제 1도는 표면 요철을 갖는 고체 전해질 연료 전지의 전극과 전해질의 계면 모식도,1 is a schematic diagram of an interface between an electrode and an electrolyte of a solid electrolyte fuel cell having surface irregularities,

제 2도는 종래 고체 전해질 연료 전지의 전극과 전해질 계면의 모식도,2 is a schematic diagram of an electrode and an electrolyte interface of a conventional solid electrolyte fuel cell,

제 3도는 본 발명에 따라 제조된 단위 전지의 성능 및 비교예를 나타낸 그래프이다.3 is a graph showing the performance and comparative examples of the unit cell manufactured according to the present invention.

Claims (2)

고체 전해질 연료 전지에 있어서, 전해질 표면에 1㎛ 이상의 직경을 갖는 전해질 분말을 20㎛ 이하의 두께로 스프레이법 또는 스크린 인쇄법에 의해 도포하고 여기에 공기극 물질을 입혀서 된 것임을 특징으로 하는 표면 요철을 갖는 고체 전해질 연료 전지.In the solid electrolyte fuel cell, an electrolyte powder having a diameter of 1 μm or more is applied to the surface of the electrolyte by a spray method or a screen printing method with a thickness of 20 μm or less and coated with a cathode material thereon. Solid electrolyte fuel cell. 제 1항에 있어서, 상기 전해질 분말의 크기는 공기극 물질의 직경보다 2배 이상의 크기를 갖는 것임을 특징으로 하는 표면 요철을 갖는 고체 전해질 연료 전지.The solid electrolyte fuel cell having surface irregularities as claimed in claim 1, wherein the electrolyte powder has a size larger than twice the diameter of the cathode material. ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019950035032A 1995-10-12 1995-10-12 Solid electrolyte fuel cell with an irregular surface KR0153307B1 (en)