KR930018773A - Manufacturing method of cylindrical spiral winding battery - Google Patents
Manufacturing method of cylindrical spiral winding battery Download PDFInfo
- Publication number
- KR930018773A KR930018773A KR1019930001319A KR930001319A KR930018773A KR 930018773 A KR930018773 A KR 930018773A KR 1019930001319 A KR1019930001319 A KR 1019930001319A KR 930001319 A KR930001319 A KR 930001319A KR 930018773 A KR930018773 A KR 930018773A
- Authority
- KR
- South Korea
- Prior art keywords
- separator
- winding
- cylindrical spiral
- battery
- halpin
- Prior art date
Abstract
원통형 와권식 전지를 제조하는데 있어서, 전지의 특성에 악영향을 미치지 않고, 할(割)핀을 중심으로 하여 권회한 와권식 전극구조체를 할핀으로부터 용이하게 발리(拔離)할 수 있도록 한다.In the manufacture of a cylindrical spiral wound battery, the spiral wound electrode structure wound around the split pin can be easily removed from the split pin without adversely affecting the characteristics of the battery.
미다공성(微多功性) 고분자 필름으로 이루어지는 세퍼레이터를 전극권취용의 할핀의 할흠에 끼워 넣어 감기 시작하고, 또한 띠형의 정극(正極)과 부극(負極)과를 상호 접촉하지 않도록 이 세퍼레이터를 개재시키면서 권회함으로서 원통형 와권식 전지를 제조하는 경우에, 세퍼레이터를 할핀의 할흠에 끼워 넣어 감기 시작하기 전에, 세퍼레이터의 할핀에 접하는 부분의 최소한 일부를 미리 그 연화점 이상, 융점 미만의 온도로 열처리하여 둔다.The separator made of a microporous polymer film is sandwiched between the pins of the halpin for winding the electrode, and the separator is interposed so as not to contact the strip-shaped positive electrode and the negative electrode. In the case of manufacturing a cylindrical spiral wound battery by winding while winding, at least a part of the separator contacting the halpin of the separator is heat-treated at a temperature above its softening point and below the melting point before the separator is inserted into the halting of the halpin.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
제1도는 세퍼레이터의 가열처리 부분을 나타낸 도면.1 is a view showing a heat treatment portion of a separator.
제2도는 실시예에 있어서 전극과 세퍼레이터와의 관계를 설명하는 도면.2 is a diagram illustrating a relationship between an electrode and a separator in an embodiment.
제3도는 와권식 전극구조체의 제조방법을 설명하는 도면.3 is a view for explaining a method of manufacturing a spiral wound electrode structure.
Claims (1)