KR920002226A - 철섬아연광의 선광방법 - Google Patents
철섬아연광의 선광방법 Download PDFInfo
- Publication number
- KR920002226A KR920002226A KR1019900010774A KR900010774A KR920002226A KR 920002226 A KR920002226 A KR 920002226A KR 1019900010774 A KR1019900010774 A KR 1019900010774A KR 900010774 A KR900010774 A KR 900010774A KR 920002226 A KR920002226 A KR 920002226A
- Authority
- KR
- South Korea
- Prior art keywords
- iron
- beneficiation
- fine zinc
- iron fine
- arsenic
- Prior art date
Abstract
내용 없음
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
Claims (1)
- 본문에 상술한 바와같이 비소, 철분이 함유된 철섬아연광의 선광에 있어 포트랜트 시멘트를 유비철, 황철광 및 자류철광등의 불순물의 억제제로 사용하므로서 철섬아연광을 부유시키고 비소, 철분의 함유광물을 억제 제거시킴을 특징으로 하는 철섬아연광의 선광방법.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.