Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김동렬filedCritical김동렬
Priority to KR1019890009479ApriorityCriticalpatent/KR910002574A/en
Publication of KR910002574ApublicationCriticalpatent/KR910002574A/en
Casting Or Compression Moulding Of Plastics Or The Like
(AREA)
Abstract
내용 없음No content
Description
합성인조목의 제조방법.Method for manufacturing synthetic artificial wood.
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
Claims (1)
불포화포리에스텔수지 25-30%에 스테아린산아연 5-10%, 고무첨가제 4-6%, 안료 8-14%, 열경화촉매제 1%를 혼합한 상태에 분말활석 10-15%, 유리중공구 30-35%, 셀룰로오즈섬유 10-15%를 첨가하여 100℃정도의 금형틀속에 투입하여 35㎏/㎠정도의 압력으로 10-15분 동안 가압성형함을 특징으로한 인조목의 제조방법.Powder talcum 10-15%, glass hollow tool 30 with 25-30% unsaturated polyester resin mixed with 5-10% zinc stearate, 4-6% rubber additive, 8-14% pigment, and 1% thermosetting catalyst -35%, 10-15% of cellulose fiber is added to the mold mold of about 100 ℃ and press molding for about 15 to 15 minutes at a pressure of about 35 ㎏ / ㎠.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019890009479A1989-07-041989-07-04
Manufacturing method of synthetic artificial wood
KR910002574A
(en)
POLYMER PARTICLE COMPOSITION, METHOD FOR THE PRODUCTION OF POLYMER PARTICLE AND LIGHT-DISTRIBUTING THERMOPLASTIC POLYMER COMPOSITION WITH THESE POLYMER PARTICLE.