정전기 처리 배합수를 사용한 고강도 콘크리트의 제조방법Manufacturing Method of High Strength Concrete Using Electrostatic Treatment Compounding Water
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
Claims (1)
콘크리트의 제조시 사용되는 배합수를 정전기 처리하여 사용함으로써, 콘크리트중의 시멘트의 수화 및 응결 작용을 촉진하여, 콘크리트의 강도를 13(%)-27(%)증대시키는 것을 특징으로 하는 고강도 콘크리트의 제조방법By using electrostatic treatment of the blended water used in the production of concrete, it promotes the hydration and condensation of cement in concrete, and increases the strength of concrete by 13 (%)-27 (%). Manufacturing method※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.