고분자 복합재료 충진재의 표면처리방법과 그 장치Surface treatment method of polymer composite filler and its device
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음As this is a public information case, the full text was not included.
제1도는 본 발명의 표면처리장치의 구성도.1 is a block diagram of a surface treatment apparatus of the present invention.
Claims (2)
무기충진재를 반응용기에 투입하고 물(유기결합제에 대한 4.5-30중량비)과 알코올을 넣어 교반 분산시킨 후 다시 알코올과 시란족 유기결합제(무기충진재에 대한 0.3-3중량비)를 투입하여 무기충진재를 코팅한 다음 진공펌프를 가동시켜 감압된 응축기에서 알코올을 회수하고 다시 감압시켜 물을 회수하게함으로서 반응용기 내에는 유기 결합제에 코팅된 건조된 무기충진제를 얻게함을 특징으로 하는 고분자 복합재료충진재의 표면처리 방법.Inorganic filler is added to the reaction vessel, water (4.5-30 weight ratio of organic binder) and alcohol are added and dispersed, and then alcohol and sirane organic binder (0.3-3 weight ratio of inorganic filler) are added again. Coating and then operating a vacuum pump to recover alcohol from the depressurized condenser and to decompress water again to obtain dried inorganic filler coated with an organic binder in the reaction container. Surface treatment method.반응용기(2)를 항온수조(4)가 연결된 초음파 분산기(3) 내에 설치하고 반응용기(2)는 응축기(8)에 연결하여 응축기(8)에는 냉각수관(7)과 용매회수용기(8b)를 설치하며 진공펌프(9)를 배관으로 연결시킨 것을 특징으로 하는 고분자복합재료 충진재의 표면처리장치.The reaction vessel (2) is installed in the ultrasonic disperser (3) to which the constant temperature water tank (4) is connected, and the reaction vessel (2) is connected to the condenser (8). The condenser (8) has a cooling water pipe (7) and a solvent recovery vessel (8b). ) And the surface treatment apparatus of the polymer composite material filler, characterized in that the vacuum pump (9) is connected by a pipe.※참고사항:최초출원 내용에 의하여 공개하는 것임.※ Note: This is to be disclosed based on the first application.