Claims (2)
콘크리트를 양생함에 있어서, 배합설계상의 배합수양만큼의 90-100℃ 고온수를 시멘트나 골재에 주가하거나 또는 블록콘크리트에 주가하여 배합 콘크리트 온도가 60-80℃가 되게 함을 특징으로 하는 콘크리트를 양생하는 방법.In curing the concrete, curing the concrete characterized in that the mixture concrete temperature of 90-100 ℃ hot water to the cement or aggregate, or block concrete to be 60-80 ℃ as the mixing quantity in the mixing design How to.제1항에 있어서, 콘크리트 배합시에 팽창제를 혼가하는 양생방법.The curing method according to claim 1, wherein the expansion agent is mixed when concrete is blended.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019810004377A1981-11-131981-11-13
How to cure concrete