산업폐기물을 이용한 고온소결 방법에 의한 건축용 벽돌의 제조방법Manufacturing method of building brick by high temperature sintering method using industrial waste
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
Claims (1)
본문에 상술한 바와 같이 일반 폐기물, 유해화학폐기물등의 산업폐기물 70% 내외에 점토 30% 내외를 혼합하여 압형 및 건조한 후 700℃―1300℃의 소결온도에서 고형화하여 얻어지는 산업폐기물을 이용한 고온소결방법에 의한 건축용 벽돌의 제조방법.As described above, high-temperature sintering method using industrial wastes obtained by solidification at sintering temperature of 700 ℃ -1300 ℃ by molding and drying after mixing about 30% of clay and 70% of industrial waste such as general waste, hazardous chemical waste, etc. Method for manufacturing building bricks by※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019810004138A1981-10-271981-10-27
Manufacturing method of building brick by high temperature sintering method using industrial waste
KR830007457A
(en)
INDUSTRIAL UTILIZATION OF OIL-BEARING SCHIST OF PINDAMONHANGABA REGION OF SAO PAULO STATE, WITH THE AIM OF INDUSTRIAL USE IN THE FABRICATION OF CERAMIC BUILDING MATERIALS