KR200448759Y1 - JIG FOR ANODIZING Mg ALLOYS GOODS - Google Patents

JIG FOR ANODIZING Mg ALLOYS GOODS Download PDF

Info

Publication number
KR200448759Y1
KR200448759Y1 KR2020070019806U KR20070019806U KR200448759Y1 KR 200448759 Y1 KR200448759 Y1 KR 200448759Y1 KR 2020070019806 U KR2020070019806 U KR 2020070019806U KR 20070019806 U KR20070019806 U KR 20070019806U KR 200448759 Y1 KR200448759 Y1 KR 200448759Y1
Authority
KR
South Korea
Prior art keywords
tab
jig
product
magnesium alloy
close contact
Prior art date
Application number
KR2020070019806U
Other languages
Korean (ko)
Other versions
KR20090005805U (en
Inventor
김재근
박창훈
김진희
유재용
한병하
김기홍
유재인
Original Assignee
경운대학교 산학협력단
(주) 태양기전
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 경운대학교 산학협력단, (주) 태양기전 filed Critical 경운대학교 산학협력단
Priority to KR2020070019806U priority Critical patent/KR200448759Y1/en
Publication of KR20090005805U publication Critical patent/KR20090005805U/en
Application granted granted Critical
Publication of KR200448759Y1 publication Critical patent/KR200448759Y1/en

Abstract

본 고안에 의한 마그네슘합금 제품의 아노다이징용 지그는 프레임에 다수개 설치되어 마그네슘합금 제품의 안쪽으로 작용하는 탄성력으로 마그네슘합금의 제품을 탄성 고정하는 마그네슘합금 제품의 아노다이징용 지그에 있어서, 프레임에 고정되는 고정체의 선단부에 제1탭이 밀착되어 나사에 의해 통전 가능하게 고정된 뒤에 제1탭과 밀착되는 부위를 제외한 고정체 전체 표면이 절연체로 피복되고, 상기 고정체와 핀으로 통전 가능하게 X자 형상으로 결합되는 회전체의 선단부에 제2탭이 밀착되어 나사로 통전 가능하게 고정된 뒤에 제2탭과 밀착되는 부위를 제외한 회전체 전체 표면이 절연체로 피복되며, 상기 제1탭과 제2탭을 근접하는 방향으로 탄성력을 작용하는 탄성부재의 양단부가 절연되도록 처리된 뒤, 상기 탄성부재가 상기 고정체와 회전체 사이에 설치되는 것으로 이루어진다.Anodizing jig of magnesium alloy product according to the present invention is a plurality of jig for anodizing of magnesium alloy product to elastically fix the product of magnesium alloy with elastic force acting on the inside of the magnesium alloy product, which is fixed to the frame The first tab is in close contact with the distal end of the fixture, and the entire surface of the fixture is covered with an insulator, except for the portion that comes into close contact with the first tab after the first tab is secured to be energized by a screw. The second tab is in close contact with the distal end of the rotating body which is coupled in shape, and the entire surface of the rotating body is covered with an insulator except for the portion in which the second tab is in close contact with the second tab. After both ends of the elastic member exerting an elastic force in an approaching direction are insulated, the elastic member is rotated with the fixing body. It is made to be provided between the body.

따라서 본 고안은 전체적으로 X 형상으로 형성되어 탄성부재의 탄성력에 의해 두 개의 탭이 제품을 견고하게 밀착 고정하기 때문에 지그의 접촉 부위의 밀착력이 증대되어 전기가 원활하게 흘러서 제품의 표면 처리의 품질을 용이하게 향상하며, 제품과 밀착되는 탭만을 교체하기 때문에 탭이 마모되었을 때에 프레임에 설치된 지그 전체를 사용하지 못하는 것이 아니라 마모된 탭을 신속하게 교체할 수 있어 작은 비용으로 유지 보수할 수 있는 등의 효과를 발휘한다.Therefore, the present invention is formed in an X shape as a whole, and the two tabs firmly fix the product by the elastic force of the elastic member, so that the adhesive force of the contact portion of the jig is increased and electricity flows smoothly, thereby facilitating the quality of the surface treatment of the product. In addition, it replaces only the tab that comes in close contact with the product, so that when the tab is worn out, the entire jig installed in the frame is not used, but the worn tab can be replaced quickly, thereby maintaining a low cost. Exert.

마그네슘합금, 아노다이징, 지그, 아노다이징용 지그 Magnesium alloy, anodizing, jig, anodizing jig

Description

마그네슘합금 제품의 아노다이징용 지그{JIG FOR ANODIZING Mg ALLOYS GOODS}JIG FOR ANODIZING Mg ALLOYS GOODS}

본 고안은 마그네슘합금으로 제조되는 제품을 아노다이징할 때에 제품을 고정하기 위한 지그에 관한 것으로서, 더욱 상세하게는 탄성부재의 탄성력으로 제품을 고정함과 더불어 제품과 밀착되는 부위를 교체하는 구조로 개선함으로써 제품의 표면 처리의 품질을 용이하게 향상하고 지그의 일부만을 교체할 수 있어 작은 비용으로 유지보수할 수 있도록 하는 마그네슘합금 제품의 아노다이징용 지그에 관한 것이다.The present invention relates to a jig for fixing a product when anodizing a product made of magnesium alloy, and more particularly, by fixing the product with an elastic force of an elastic member and improving the structure to replace the close contact with the product. It relates to anodizing jig of magnesium alloy products that can easily improve the quality of the surface treatment of the product and can replace only a part of the jig, so that maintenance can be performed at a low cost.

일반적으로 마그네슘합금는 치수 안정성이 우수하고, 미강도, 전자기파 차폐성, 진동 감쇄 등이 알루미늄 합금과 철강에 비하여 우수하여 자동차와 항공기용 부품, 휴대폰 케이스, 노트북 컴퓨터 케이스, 안경테 등에 많이 사용되고 있으며, 표준 전극 단위가 낮고 내식성이 취약하여 부식 방지를 위하여 표면 처리하게 된다.In general, magnesium alloy has excellent dimensional stability, and excellent strength, electromagnetic shielding, and vibration damping are superior to aluminum alloy and steel, and are widely used in automobile and aircraft parts, mobile phone cases, laptop computer cases, and eyeglass frames. Low corrosion resistance and poor surface treatment to prevent corrosion.

그래서 상기 마그네슘합금을 재질로 하는 제품을 표면 처리하기 위하여, 아노다이징(anodizing)이라고 지칭되는 양극 처리 방법을 사용하게 되는 바, 상기 아 노다이징(anodizing)은 제품의 표면을 청정화하거나 연마 산화 처리를 할 때, 제품을 양극과 연결하여 전해액 속에 넣고 불활성 금속을 음극으로 하여 전류를 통하여 제품의 표면에 산소를 발생시키고 이러한 산소에 의해 제품의 표면에 산화 피막이 형성되도록 하는 처리법이다.Therefore, in order to surface-treat the product made of the magnesium alloy, anodizing method called anodizing is used. The anodizing is used to clean or polish the surface of the product. In this case, the product is connected to the positive electrode, put into the electrolyte, and an inert metal is used as the negative electrode to generate oxygen on the surface of the product through a current, and the oxygen film is formed on the surface of the product by the oxygen.

그래서 상기 마그네슘합금 제품을 아노다이징하면 도장에 대한 우수한 밀착성과 내식성을 구현할 수 있는 것이다.Thus, anodizing the magnesium alloy product can realize excellent adhesion and corrosion resistance for painting.

여기서 상기와 같이 마그네슘합금 제품을 아노다이징할 경우, 양극과 연결된 지그로 제품을 잡아서 전해질에 넣게 되는 바, 종래의 지그는 도 5에 도시한 바와 같이 ㄷ자 형상의 지그(101)의 양단부를 외측으로 절곡 형성한 뒤, 양극과 연결되는 프레임(102)에 지그(101)를 일체로 설치하고, 상기 지그(101)의 양단부를 제외한 나머지 부위와 상기 프레임(102) 전체를 절연체로 피복시키는 구조를 이루고 있다.Here, when anodizing the magnesium alloy product as described above, the product is caught in the jig connected with the positive electrode and put into the electrolyte, the conventional jig is bent outwardly both ends of the c-shaped jig 101 as shown in FIG. After forming, the jig 101 is integrally installed on the frame 102 connected to the anode, and the rest of the jig 101 and the entire frame 102 are covered with an insulator. .

이와 같이 이루어지는 지그(101)를 손으로 잡아서 지그(101)의 양단부의 거리를 축소시킨 뒤, 마그네슘합금 제품의 내부에 지그(101)의 양단부를 배치하여 손을 놓아서 지그(101) 자체의 탄성력에 의해 지그(101)의 양단부가 마그네슘합금 제품의 내부에 밀착되는 것이다.By holding the jig 101 made in this way by reducing the distance between both ends of the jig 101, and placing both ends of the jig 101 inside the magnesium alloy product to release the hand to the elastic force of the jig 101 itself Both ends of the jig 101 are in close contact with the inside of the magnesium alloy product.

물론 상기 프레임(102) 상에는 다수의 지그(101)가 일체로 설치되는 것이며, 다수의 지그(101)를 이용하여 다수의 마그네슘합금 제품을 탄성 고정한 뒤, 다수의 마그네슘합금 제품을 지그와 함께 넣어서 프레임(102)에 전기를 통전시켜서 마그네슘합금 제품의 표면에 산화 피막을 형성하게 된다.Of course, the plurality of jigs 101 are integrally installed on the frame 102, and after the elastic fixing of the plurality of magnesium alloy products using the plurality of jigs 101, the plurality of magnesium alloy products are put together with the jig to make the frame. Electricity is supplied to 102 to form an oxide film on the surface of the magnesium alloy product.

그러나 종래의 지그는 구조가 단순하게 형성되는 장점이 있으나, 지그 자체의 탄성력으로 제품을 고정하기 때문에 지그의 단부와 제품의 접촉 부위의 밀착력이 저하되는 경우가 빈번하여 접촉 부위의 저항이 커지면서 제품의 접촉 부위가 녹아서 제품의 불량을 초래하게 된다는 단점이 있다.However, the conventional jig has the advantage that the structure is simply formed, but since the fixing of the product by the elastic force of the jig itself, the adhesion between the end of the jig and the contact portion of the product is often lowered and the resistance of the contact portion increases. There is a disadvantage that the contact part is melted and causes a defect of the product.

또한 종래의 지그를 오랫동안 사용하여 지그의 선단부가 마모되는 경우, 프레임에 설치된 다수의 지그 중에 마모된 지그만을 신속하게 교체할 수 없기 때문에 아노다이징 공정의 효율성을 위하여 프레임과 다수의 지그 전체를 교체하게 된다는 단점이 있다.In addition, if the tip of the jig is worn by using the conventional jig for a long time, only the worn jig among the many jig installed in the frame cannot be replaced quickly, so that the entire frame and the multiple jig are replaced for the efficiency of the anodizing process. There are disadvantages.

본 고안은 상기와 같은 종래 기술의 문제점을 해결하기 위하여 안출된 것으로서, 본 고안의 목적은 탄성부재의 탄성력으로 제품을 고정함과 더불어 제품과 밀착되는 부위를 교체하는 구조로 개선함으로써, 제품과 지그의 접촉 부위의 밀착력이 증대되면서 전기가 원활하게 흐르게 되어 제품의 표면 처리의 품질을 용이하게 향상하고, 제품과 접촉되는 지그의 일부를 교체할 수 있어 프레임에 설치된 다수의 지그 전체를 교체하지 않아 작은 비용으로 유지보수할 수 있는 마그네슘합금 제품의 아노다이징용 지그를 제공하는 데 있다.The present invention has been devised to solve the problems of the prior art as described above, the object of the present invention is to improve the structure to replace the part in close contact with the product, while fixing the product by the elastic force of the elastic member, jig and product As the adhesion of the contact area increases, electricity flows smoothly, which improves the quality of the surface treatment of the product, and it is possible to replace a part of the jig contacted with the product. To provide an anodizing jig of magnesium alloy products that can be maintained at cost.

상기와 같은 목적을 달성하기 위하여, 본 고안은 프레임에 다수개 설치되어 마그네슘합금 제품의 안쪽으로 작용하는 탄성력으로 마그네슘합금의 제품을 탄성 고정하는 마그네슘합금 제품의 아노다이징용 지그에 있어서, 프레임에 고정되는 고정체의 선단부에 제1탭이 밀착되어 나사에 의해 통전 가능하게 고정된 뒤에 제1탭과 밀착되는 부위를 제외한 고정체 전체 표면이 절연체로 피복되고, 상기 고정체와 핀으로 통전 가능하게 X자 형상으로 결합되는 회전체의 선단부에 제2탭이 밀착되어 나사로 통전 가능하게 고정된 뒤에 제2탭과 밀착되는 부위를 제외한 회전체 전체 표면이 절연체로 피복되며, 상기 제1탭과 제2탭을 근접하는 방향으로 탄성력을 작용하는 탄성부재의 양단부가 절연되도록 처리된 뒤, 상기 탄성부재가 상기 고정체와 회전체 사이에 설치되는 것으로 이루어지는 마그네슘합금 제품의 아노다이징용 지그를 제공한다.In order to achieve the above object, the present invention is installed in a plurality of frames in the jig for anodizing the magnesium alloy product to elastically fix the product of the magnesium alloy with an elastic force acting inwardly of the magnesium alloy product, which is fixed to the frame The first tab is in close contact with the distal end of the fixture, and the entire surface of the fixture is covered with an insulator, except for the portion that comes into close contact with the first tab after the first tab is secured to be energized by a screw. The second tab is in close contact with the distal end of the rotating body which is coupled in shape, and the entire surface of the rotating body is covered with an insulator except for the portion in which the second tab is in close contact with the second tab. After both ends of the elastic member exerting an elastic force in an approaching direction are insulated, the elastic member is disposed between the fixed body and the rotating body. It provides a jig for anodizing a magnesium alloy product consisting of being installed.

상기와 같이 이루어지는 본 고안에 의한 마그네슘합금 제품의 아노다이징용 지그는 전체적으로 X 형상으로 형성되어 탄성부재의 탄성력에 의해 두 개의 탭이 제품을 견고하게 밀착 고정하기 때문에 지그의 접촉 부위의 밀착력이 증대되어 전기가 원활하게 흘러서 제품의 표면 처리의 품질을 용이하게 향상하며, 제품과 밀착되는 탭만을 교체하기 때문에 탭이 마모되었을 때에 프레임에 설치된 지그 전체를 사용하지 못하는 것이 아니라 마모된 탭을 신속하게 교체할 수 있어 작은 비용으로 유지 보수할 수 있다는 이점이 있다.The anodizing jig of the magnesium alloy product according to the present invention made as described above is formed in an X shape as a whole, and the two tabs firmly adhere to the product firmly by the elastic force of the elastic member, thereby increasing the adhesion of the contact portion of the jig, thereby increasing electricity. Flows smoothly and easily improves the quality of the surface treatment of the product, and replaces only the tabs that come in close contact with the product, so that worn tabs can be replaced quickly instead of not using the entire jig installed in the frame when the tabs are worn out. This has the advantage of being low cost maintenance.

이하 본 고안의 바람직한 실시예를 첨부한 도면에 의거하여 더욱 상세하게 설명한다.Hereinafter, preferred embodiments of the present invention will be described in more detail with reference to the accompanying drawings.

도 1과 도 2는 본 고안에 의한 마그네슘합금 제품의 아노다이징용 지그를 나타내는 도면으로서, 상기 지그(1)의 다수개가 프레임(2)에 설치되어 마그네슘합금 제품(10)의 안쪽으로 작용하는 탄성력으로 마그네슘합금의 제품(10)을 탄성 고정하게 된다.1 and 2 are diagrams showing the anodizing jig of the magnesium alloy product according to the present invention, a plurality of the jig (1) is installed on the frame (2) to the elastic force acting inside the magnesium alloy product (10) The product 10 of the magnesium alloy is elastically fixed.

즉 상기 지그(1)는 프레임(2)에 고정되는 고정체(11), 상기 고정체(11)의 선단부에 설치되는 제1탭(12), 상기 고정체(11)와 X자로 결합되는 회전체(13), 상기 회전체(13)의 선단부에 설치되는 제2탭(14), 상기 고정체(11)와 회전체(13) 사이에 설치되는 탄성부재(15)로 이루어지며, 상기 제1,제2탭(12,14)를 제외한 부위가 절연체(16)로 피복된다.That is, the jig 1 includes a fixture 11 fixed to the frame 2, a first tab 12 installed at a tip end of the fixture 11, and a combination of X and the fixture 11. It consists of the whole 13, the second tab 14 provided on the front end of the rotating body 13, the elastic member 15 provided between the fixed body 11 and the rotating body 13, The portions except the first and second tabs 12 and 14 are covered with the insulator 16.

다시 말하면 상기 프레임(2)에 고정되는 고정체(11)의 선단부에는 도 1과 도 3에 도시한 바와 같이 제1탭(12)이 밀착되어 나사(12a)에 의해 통전 가능하게 고정된 뒤, 상기 제1탭(12)과 밀착되는 부위를 제외한 고정체(11) 전체 표면이 절연체(16)로 피복된다.In other words, as shown in FIGS. 1 and 3, the first tab 12 is in close contact with the front end of the fixed body 11 fixed to the frame 2, and is electrically fixed by the screw 12a. The entire surface of the fixture 11 except for the portion in close contact with the first tab 12 is covered with an insulator 16.

또한 상기 회전체(13)은 도 1과 도 3에 도시한 바와 같이 상기 고정체(11)와 핀(17)으로 통전 가능하게 X자 형상으로 결합되며, 이의 선단부에는 제2탭(14)이 밀착되어 나사(14a)로 통전 가능하게 고정된 뒤, 상기 제2탭(14)과 밀착되는 부위를 제외한 회전체(13) 전체 표면이 절연체(16)로 피복된다.In addition, as shown in FIGS. 1 and 3, the rotor 13 is coupled to the fixed body 11 and the pin 17 in an X-shape so as to be energized, and a second tab 14 is formed at the tip thereof. After being in close contact with each other and securely energized by screws 14a, the entire surface of the rotor 13 except for the part in close contact with the second tab 14 is covered with the insulator 16.

더우기 상기 고정체(11)와 회전체(13) 사이에는 탄성부재(15)가 설치되며, 상기 탄성부재(15)의 양단부는 절연되도록 처리되고, 상기 탄성부재(15)는 상기 제1탭(12)과 제2탭(14)을 근접시키는 방향으로 고정체(11)와 회전체(13)에 탄성력을 작용하게 된다.Furthermore, an elastic member 15 is installed between the fixed body 11 and the rotating body 13, and both ends of the elastic member 15 are insulated from each other, and the elastic member 15 has the first tab ( An elastic force is applied to the fixing body 11 and the rotating body 13 in a direction in which 12) and the second tab 14 are close to each other.

한편 상기 제1탭(12)과 제2탭(14)가 제품(10)의 외부면에 밀착 접촉하게 되는 바, 제품(10)의 고정 상태를 견고하게 하기 위하여 상기 제1탭(12)과 제2탭(14)은 도 3과 도 4에 도시한 바와 같이 마그네슘합금 제품(10)의 표면과 밀착되는 부위의 한쪽 면에 V 자 또는 ㄷ자 형상의 홈(12b,14b)을 각각 형성하는 된다.On the other hand, the first tab 12 and the second tab 14 are in close contact with the outer surface of the product 10, the first tab 12 and in order to secure the fixed state of the product 10 As shown in Figs. 3 and 4, the second tab 14 forms V-shaped or c-shaped grooves 12b and 14b on one surface of the portion in close contact with the surface of the magnesium alloy product 10, respectively. .

이와 같이 이루어지는 본 고안에 의한 마그네슘합금 제품의 아노다이징용 지그는 작업자가 회전체(13)의 후단부를 잡고 당기면 제1탭(12)과 제2탭(14) 사이의 거리가 이격되고, 상호 이격된 제1탭(12)과 제2탭(14) 사이에 제품(10)을 놓고 손을 놓으면 도 3과 도 4와 같이 제품(10)이 탄성부재(15)의 탄성력으로 견고하게 고정하게 된다.The anodizing jig of the magnesium alloy product according to the present invention made as described above is a distance between the first tab 12 and the second tab 14 when the operator grabs the rear end of the rotating body 13 and is spaced apart from each other. When the product 10 is placed between the first tab 12 and the second tab 14 and the hands are released, the product 10 is firmly fixed by the elastic force of the elastic member 15 as shown in FIGS. 3 and 4.

상기와 같이 고정된 제품(10)은 제1탭(12)과 제2탭(14)에 밀착되므로 이들의 접촉 부위의 통전성이 향상되는 것이며, 제1탭(12)과 제2탭(14) 사이의 이격 거리의 변화가 크므로 다양한 크기의 제품에도 적용할 수 있는 것이다.Since the product 10 fixed as described above is in close contact with the first tab 12 and the second tab 14, the electrical conduction of the contact portion thereof is improved, and the first tab 12 and the second tab 14 are improved. Since the change of separation distance between them is large, it can be applied to products of various sizes.

더우기 제품(10)과 접촉되는 제1,제2탭(12,14)의 표면에 전기 저항에 의해 마모되기 쉬운 바, 제1,제2탭(12,14)이 마모되더라도 프레임(2)에 설치된 지그(1) 전체를 모두 사용하지 못하는 것이 아니라 마모된 제1,제2탭(12,14)만을 간편하게 교체할 수 있는 것이다.In addition, since the surface of the first and second tabs 12 and 14 in contact with the product 10 are easily worn by electrical resistance, the frame 2 may be worn even if the first and second tabs 12 and 14 are worn. It is not possible to use all of the jig (1) is installed, it is possible to simply replace the worn first, second tabs (12, 14).

도 1은 본 고안에 의한 지그의 다수개가 프레임에 설치된 상태를 나타내는 발췌 사시도,1 is an excerpt perspective view showing a state in which a plurality of jigs according to the present invention are installed in a frame;

도 2는 본 고안에 의한 마그네슘합금 제품의 아노다이징용 지그의 측면도,Figure 2 is a side view of the jig for anodizing the magnesium alloy product according to the present invention,

도 3은 도 2의 A - A선 단면도,3 is a cross-sectional view taken along the line A-A of FIG.

도 4는 본 고안에 의한 지그에 적용되는 제1,제2탭의 다른 예를 나타내는 단면도,4 is a cross-sectional view showing another example of the first and second tabs applied to the jig according to the present invention;

도 5는 종래에 관련하는 마그네슘합금 제품의 아노다이징용 지그의 발췌 사시도이다.5 is an excerpt perspective view of an anodizing jig of a magnesium alloy product according to the related art.

<도면의 주요 부분에 대한 부호의 설명><Explanation of symbols for the main parts of the drawings>

1 : 지그 2 : 프레임1: jig 2: frame

11 : 고정체 12,14 : 제1,제2탭11: fixed body 12, 14: first and second tab

13 : 회전체 15 : 탄성부재13: rotating body 15: elastic member

Claims (2)

프레임에 다수개 설치되어 마그네슘합금 제품의 안쪽으로 작용하는 탄성력으로 마그네슘합금의 제품을 탄성 고정하는 마그네슘합금 제품의 아노다이징용 지그에 있어서,In the anodizing jig of magnesium alloy products, which are installed in a plurality of frames and elastically fix the magnesium alloy products with an elastic force acting inside the magnesium alloy products, 프레임에 고정되는 고정체의 선단부에 제1탭이 밀착되어 나사에 의해 통전 가능하게 고정된 뒤에 제1탭과 밀착되는 부위를 제외한 고정체 전체 표면이 절연체로 피복되고,The entire surface of the fixture is covered with an insulator, except that the first tab is in close contact with the front end of the fixture fixed to the frame and is secured to be energized by screws, and then the part of the fixture is in close contact with the first tab. 상기 고정체와 핀으로 통전 가능하게 X자 형상으로 결합되는 회전체의 선단부에 제2탭이 밀착되어 나사로 통전 가능하게 고정된 뒤에 제2탭과 밀착되는 부위를 제외한 회전체 전체 표면이 절연체로 피복되며,The entire surface of the rotating body is covered with an insulator except for a portion where the second tab is in close contact with the fixing member and the pin is electrically connected to the X-shape so as to be energized by the pin, and the part is in close contact with the second tab. , 상기 제1탭과 제2탭을 근접하는 방향으로 탄성력을 작용하는 탄성부재의 양단부가 절연되도록 처리된 뒤, 상기 탄성부재가 상기 고정체와 회전체 사이에 설치되는 것으로 이루어지는 마그네슘합금 제품의 아노다이징용 지그.For anodizing a magnesium alloy product, wherein both ends of an elastic member exerting an elastic force in a direction proximate the first tab and the second tab are insulated, and then the elastic member is installed between the fixed body and the rotating body. Jig. 제1항에 있어서,The method of claim 1, 상기 제1탭과 제2탭은 마그네슘합금 제품의 표면과 밀착되는 부위의 한쪽 면에 V 자 또는 ㄷ자 형상의 홈을 형성하는 것을 포함하여 이루어지는 마그네슘합금 제품의 아노다이징용 지그.The first tab and the second tab jig for anodizing magnesium alloy product comprising forming a V-shaped or c-shaped groove on one side of the portion in close contact with the surface of the magnesium alloy product.
KR2020070019806U 2007-12-10 2007-12-10 JIG FOR ANODIZING Mg ALLOYS GOODS KR200448759Y1 (en)