KR20040069370A - Flat CRT - Google Patents

Flat CRT Download PDF

Info

Publication number
KR20040069370A
KR20040069370A KR1020030005694A KR20030005694A KR20040069370A KR 20040069370 A KR20040069370 A KR 20040069370A KR 1020030005694 A KR1020030005694 A KR 1020030005694A KR 20030005694 A KR20030005694 A KR 20030005694A KR 20040069370 A KR20040069370 A KR 20040069370A
Authority
KR
South Korea
Prior art keywords
panel
funnel
effective screen
cathode ray
ray tube
Prior art date
Application number
KR1020030005694A
Other languages
Korean (ko)
Inventor
이구화
김지순
임경률
Original Assignee
엘지.필립스디스플레이(주)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 엘지.필립스디스플레이(주) filed Critical 엘지.필립스디스플레이(주)
Priority to KR1020030005694A priority Critical patent/KR20040069370A/en
Publication of KR20040069370A publication Critical patent/KR20040069370A/en

Abstract

PURPOSE: A flat cathode ray tube is provided to improve a productivity and to reduce a cost in results of removing a resin for uniting an anti-explosion glass and the anti-explosion glass by reinforcing an edge side of a panel concentrated to a stress. CONSTITUTION: A flat cathode ray tube comprises a panel(10) having a fluorescent film(11) at an inside surface and a non-effective screen part at an edge portion; a funnel(20) fused at a rear side of the panel, a mask supporter(30) arranged to an outside edge of the fluorescent film at an inside of the panel; a shadow mask(40) fixed to the mask supporter and having a dot or a slot shape hole; an electron gun mounted at an edge part of a rear side of the funnel and emitting an electron beam; a deflection yoke formed at a slim neck part of the funnel and forming a uniform magnetic field about an electron beam emitted from the electron gun; a reinforcing band(60) covered at an edge of a front part of the panel; and a reinforcing part formed more thick than an effective screen part by at least a first difference of a thickness(13) at the non-effective screen part of the panel.

Description

평면 음극선관{Flat CRT}Flat Cathode Ray Tubes {Flat CRT}

본 발명은 평면 음극선관에 관한 것으로, 더욱 상세하게는 패널의 비 유효화면 부의 구조를 개선함으로써 방폭유리의 삭제가 가능하고, 또 패널과 펀넬을 프릿 글라스에 의해 융착한 후 내부를 진공상태로 유지하기 위한 배기공정을 할 때 패널과 펀넬이 접합된 부분으로 집중되는 응력을 감쇠시키는 평면 음극선관에 관한 것이다.The present invention relates to a planar cathode ray tube, and more particularly, it is possible to eliminate the explosion-proof glass by improving the structure of the non-effective screen portion of the panel, and to keep the interior in a vacuum state after fusing the panel and the funnel with the frit glass. The present invention relates to a planar cathode ray tube which attenuates the stress concentrated at the jointed portion of the panel and the funnel during the exhaust process.

도 1에는 일반적인 평면 음극선관의 내부 구성을 보인 단면도가 도시되어 있다.Figure 1 is a cross-sectional view showing the internal configuration of a typical flat cathode ray tube.

이에 도시된 바와 같이, 평면 음극선관의 패널(10)은 그 내측 면에 도면표현을 생략한 형광체(11)가 도포되어 있고 그 외측 면에는 방폭유리(12)가 부착되어 있다.As shown in the figure, the panel 10 of the planar cathode ray tube is coated with phosphor 11, which is omitted from the drawing, on the inner side thereof, and explosion-proof glass 12 is attached to the outer side thereof.

상기 방폭유리(12)는 패널(10)을 외부의 충격으로부터 보호하는 기능을 하며 광경화성 접착제인 레진에 의해 패널(10)과 일체로 접착된다.The explosion-proof glass 12 functions to protect the panel 10 from external impact and is integrally bonded to the panel 10 by a resin, which is a photocurable adhesive.

한편, 상기 패널(10)의 후방에는 벌브(Bulb) 형상의 펀넬(20)이 프릿 글라스에 의해 패널(10)에 대해 일체로 융착되며 튜브(T)(또는 진공용기)를 형성하고 있다.On the other hand, a bulb-shaped funnel 20 behind the panel 10 is integrally fused to the panel 10 by frit glass to form a tube T (or a vacuum vessel).

또 상기 패널(10)의 내측에는 장, 단축으로 분리 구성된 것이 부착되며 사각 틀의 형상을 갖는 마스크 지지체(30)가 접합되어 있다.In addition, a mask support 30 having a rectangular frame shape is attached to the inside of the panel 10.

상기 마스크 지지체(30)에는 슬릿 또는 공극 형상의 미세한 홀(41)이 형성된 새도우마스크(40)가 상기 마스크 지지체(30)에 대해 인장된 상태로 고정되어 있다.A shadow mask 40 having a slit or pore-shaped fine hole 41 is fixed to the mask supporter 30 in a tensioned state with respect to the mask supporter 30.

또한, 상기 펀넬(20)의 후방에 구비된 네크부(21)에는 R,G,B 의 영상신호에 따라 도면 표현상 가시화 된 전자빔을 방출하는 전자총(23)이 장착되어 있으며, 상기 펀넬(20)의 외측에는 수직/수평 방향으로 균일한 자계를 형성하여 전자빔(22)을 굴절시키는 편향요크(50)가 설치되어 있다.In addition, the neck 21 provided at the rear of the funnel 20 is equipped with an electron gun 23 for emitting an electron beam visualized in the drawing representation according to image signals of R, G, and B, and the funnel 20. The deflection yoke 50 is provided on the outer side of the deflection yoke, which forms a uniform magnetic field in the vertical / horizontal direction and refracts the electron beam 22.

한편, 상기 패널(10)의 외측 테두리에는 패널(10)을 보강하기 위한 보강밴드(60)가 에워싸여지며, 보강밴드(60)의 각 코너 부위에는 음극선관을 후술하는 모니터 또는 텔레비전의 외관을 형성하는 케이스에 장착하기 위한 러그(61)가 배치된다.On the other hand, the outer edge of the panel 10 is surrounded by a reinforcing band 60 for reinforcing the panel 10, and each corner portion of the reinforcing band 60 shows the appearance of a monitor or television which will describe the cathode ray tube described later. The lug 61 for attaching to the case to form is arrange | positioned.

도면중 미 설명부호 70은 자계쉴드이다.In the drawings, reference numeral 70 denotes a magnetic field shield.

따라서, 상기 전자총(23)의 도시되지 않은 음극에 3원색의 영상신호가 인가됨에 따라 그 전자빔(22)이 상기 패널(10)의 내면측에 도포된 상기 형광체(11)를 향해 방출된다.Accordingly, when an image signal of three primary colors is applied to a cathode (not shown) of the electron gun 23, the electron beam 22 is emitted toward the phosphor 11 applied to the inner surface side of the panel 10.

상기와 같이 방출된 전자빔(22)은 그 방출되는 경로상에 위치한 새도우마스크(40)에 의해 불필요한 전자빔(22)(약 80%)은 차단되고, 화상재현에 필요한 전자빔(약 20%)은 상기 새도우 마스크(40)에 형성된 미세한 홀(41)을 통해 R,G,B 의 형광체(11)와 충돌하며 칼라 화상이 재현된다.The electron beam 22 emitted as described above is blocked by the shadow mask 40 positioned on the emission path so that unnecessary electron beam 22 (about 80%) is blocked, and the electron beam (about 20%) necessary for image reproduction is It collides with the phosphor 11 of R, G, and B through the fine hole 41 formed in the shadow mask 40, and a color image is reproduced.

한편, 상기와 같은 구성의 일반적인 평면 음극선관에서 특히 패널과 펀넬을 융착시키는 일련의 공정중에는 다음과 같은 문제점들이 발생되었다.On the other hand, in the general planar cathode ray tube of the above-described configuration, in particular during the series of processes for fusing the panel and funnel, the following problems occurred.

즉, 패널(10)과 펀넬(20)을 프릿 글라스에 의해 융착시킨 상태에서 튜브(T)의 내부압력을 10-7∼10-8torr 정도의 고진공으로 형성하는 배기공정을 하게되면 음극선관의 외부는 760 torr의 대기압 상태이지만 그 내부는 10-7∼10-8torr 정도이므로 음극선관의 내·외부 사이의 기압차에 의한 1.01325×100000 N/m²의 압력을 받게되고, 이에 따라 패널(10)과 펀넬(20)은 도 2에 표현(이해를 돕기 위해 약간 표현을 과장함.)된 바와 같이 원래의 모습으로부터 그 형상이 변형되고, 동시에 패널(10)과 펀넬(20)의 각 부위는 응력이 작용하게 된다.In other words, when the panel 10 and the funnel 20 are fused by frit glass, the exhaust tube is formed with a high vacuum of about 10 −7 to 10 −8 torr in the internal pressure of the tube T. The outside is at atmospheric pressure of 760 torr, but the inside is about 10 -7 to 10 -8 torr, so the pressure is 1.01325 × 100000 N / m² due to the pressure difference between the inside and the outside of the cathode ray tube. ) And the funnel 20 is deformed from its original shape as shown in FIG. 2 (a slightly exaggerated representation for clarity), and at the same time each part of the panel 10 and the funnel 20 The stress acts.

이와 같은 요인에 의해 발생되는 응력은 패널(10)과 펀넬(20)은 그 주성분이 인장 응력에 취약한 유리성분으로 제작된 관계로 도면상 K로 표현된 부분인 패널과 펀넬의 접합부분에 집중되고, 그에 따라 K 부분에서 크랙이 발생될 수 있으며, 또한 그와 같이 불안정한 상태에서는 외부에서 가해지는 충격에 의해 폭죽이 발생될 우려도 발생된다.The stress generated by such a factor is concentrated in the panel-funnel junction, which is a part represented by K in the drawing, because the panel 10 and the funnel 20 are made of a glass component whose main component is vulnerable to tensile stress. Therefore, cracks may be generated in the K part, and in such an unstable state, there is a fear that firecrackers may be generated by an external impact.

상기와 같은 우려를 방지하기 위해 패널(10)의 전면에는 방폭유리(12)를 광경화성 수지인 레진에 의해 부착 사용함으로써 패널(10)을 보강 사용하였다.In order to prevent such a concern, the panel 10 was reinforced and used by attaching the explosion-proof glass 12 to the front surface of the panel 10 with a resin of photocurable resin.

그러나, 상기와 같이 광경화성 수지인 레진을 패널(10)의 전면에 도포한 후 그 전방에 다시 방폭유리(12)를 부착하는 라미네이션 공정을 진행하는 동안에 레진에 이물질 등이 함유하게되면 기포가 발생하게되었고, 그와 같은 요인에 의해 발생되는 기포는 음극선관의 불량요인으로 지적되었을 뿐만 아니라 고도로 청정한 분위기를 요구하는 작업공간에서 방폭유리 부착공정이 이루어져야 하므로 방폭유리를부착하기에 최적의 조건인 별도의 작업공간을 확보해야 하는 또 다른 문제점이 있었다.However, when the resin, which is a photocurable resin, is applied to the entire surface of the panel 10 as described above, and foreign matter is contained in the resin during the lamination process of attaching the explosion-proof glass 12 to the front thereof, bubbles are generated. Bubbles generated by such factors were not only pointed out as a bad factor of cathode ray tube, but also the explosion-proof glass attaching process should be performed in a work space requiring a highly clean atmosphere. There was another problem to secure the workspace of.

따라서, 본 발명이 해결하고자 하는 기술적 과제, 즉, 본 발명의 목적은 상술한 평면 음극선관을 제조하는 공정 중에 발생되는 문제점을 해결하기 위한 것으로, 패널과 펀넬을 프릿 글라스에 의해 융착한 후 내부를 진공상태로 유지하기 위한 배기공정을 할 때 발생되는 응력에 대한 문제점을 해결하기 위한 것으로, 응력이 집중되는 패널의 가장자리 측을 보강함으로써 방폭유리와 그 방폭유리를 접합시키기 위한 레진을 삭제함으로써 원가를 절감하고 생산성을 향상할 수 있는 평면 음극선관을 제공하는데 있다.Therefore, the technical problem to be solved by the present invention, that is, the object of the present invention is to solve the problems occurring during the above-described manufacturing process of the planar cathode ray tube, the panel and the funnel by fusing the glass after fusing the inside It is to solve the problem of the stress generated during the exhaust process to maintain the vacuum state, and by reinforcing the edge side of the panel where the stress is concentrated, the cost is eliminated by eliminating the resin for bonding the explosion-proof glass and the explosion-proof glass. It is to provide a flat cathode ray tube that can save and improve productivity.

본 발명의 다른 목적은, 패널의 전면에 부착되었던 방폭유리의 삭제가 가능함으로써 방폭유리를 부착하기 위한 별도의 작업공간을 줄일 수 있어 제조코스트를 낮출 수 있는 평면 음극선관을 제공하는데 있다.Another object of the present invention is to provide a flat cathode ray tube which can reduce the manufacturing cost by reducing the separate work space for attaching the explosion-proof glass by being able to delete the explosion-proof glass attached to the front of the panel.

도 1은 일반적인 평면 음극선관의 단면도1 is a cross-sectional view of a typical flat cathode ray tube

도 2는 종래 평면 음극선관에서 배기공정시 음극선관에 응력이 발생되는 상태를 보인 예시도Figure 2 is an exemplary view showing a state in which a stress is generated in the cathode ray tube during the exhaust process in the conventional flat cathode ray tube

도 3은 본 발명이 적용된 평면 음극선관의 단면도Figure 3 is a cross-sectional view of a flat cathode ray tube to which the present invention is applied

도 4는 본 발명에서 적용된 패널의 배면도Figure 4 is a rear view of the panel applied in the present invention

도 5의 a는 본 발명의 주요부를 보인 평단면도Figure 5a is a cross-sectional plan view showing the main part of the present invention.

도 5의 b는 본 발명의 다른 실시 예를 보인 평단면도Figure 5b is a cross-sectional view showing another embodiment of the present invention

***도면의 주요 부분에 대한 부호의 설명****** Description of the symbols for the main parts of the drawings ***

10:패널 12;보강부10: panel 12; reinforcing part

13;제1 단차 14;제2 단차13; first step 14; second step

20;펀넬 22;전자빔20; funnel 22; electron beam

23;전자총 30;마스크 지지체23; electron gun 30; mask support

40;새도우마스크 50;편향요크40; shadow mask 50; deflection yoke

60;보강밴드 "T";튜브60; reinforcing band "T"; Tube

상기한 목적을 달성하기 위하여 본 발명의 바람직한 제1 실시 예는, 유효화면인 내측 면에 형광막이 도포되며 가장자리 테두리에 비 유효화면부가 형성된 패널; 상기 패널의 후방에 융착되는 벌브 형상의 펀넬; 상기 패널의 내측면에 상기 형광막의 외측 가장자리로 접착 배열된 마스크 지지체; 상기 마스크 지지체에 대해인장된 상태로 고정되며 도트 또는 슬롯 형상의 홀이 형성된 새도우마스크; 상기 펀넬의 후방 끝단부에 봉입 설치되며 전자빔을 방사하는 전자총; 상기 펀넬의 잘록한 네크부에 형성되며 상기 전자총에 의해 방사되는 전자빔에 대해 균일한 자계를 형성하는 편향요크; 상기 패널의 전면부 테두리에 에워싸여지는 보강밴드를 포함하는 평면 음극선관에 있어서, 상기 패널의 비 유효화면 부에는 적어도 한 개의 제1 단차에 의해 유효화면 부의 두께보다 두껍게 형성된 보강부가 구비된 것을 포함하는 평면 음극선관을 제공한다.In order to achieve the above object, a first embodiment of the present invention includes a panel in which a fluorescent film is applied to an inner surface of an effective screen and an ineffective screen portion is formed at an edge of the panel; A bulb-shaped funnel fused to the rear of the panel; A mask supporter adhesively arranged to an outer edge of the fluorescent film on an inner surface of the panel; A shadow mask fixed in a tensioned state with respect to the mask support and having a dot or slot-shaped hole formed therein; An electron gun encapsulated in the rear end of the funnel and emitting an electron beam; A deflection yoke formed in the narrow neck portion of the funnel and forming a uniform magnetic field with respect to the electron beam emitted by the electron gun; A flat cathode ray tube including a reinforcing band surrounded by a front edge of the panel, wherein the non-effective screen portion of the panel includes a reinforcement portion formed thicker than the thickness of the effective screen portion by at least one first step. It provides a flat cathode ray tube.

바람직한 제2 실시 예로는, 상기 보강부에 형성된 적어도 한 개의 제1 단차 내측에는 상기 마스크 지지체가 장착되고, 외측에는 상기 펀넬이 융착되는 것이 바람직하다.In a second preferred embodiment, the mask supporter is mounted inside the at least one first step formed in the reinforcement part, and the funnel is fused to the outside.

바람직한 제3 실시 예로는, 상기 보강부는 상기 패널의 비 유효화면 부에 제1,2 단차가 단계적으로 배치되고, 상기 제1 단차에는 상기 마스크 지지체가 부착되며 상기 제2 단차에는 펀넬이 부착된 것이 바람직하다.In a third preferred embodiment, the reinforcement part has first and second steps disposed on the non-effective screen part of the panel in stages, the mask support is attached to the first step, and a funnel is attached to the second step. desirable.

바람직한 제4 실시 예로는, 유효화면 부의 두께를 A, 비 유효화면 부의 두께를 B, 최대 비 유효화면 부의 두께를 C, 유효화면 부의 두께+패널 내측면에서 새도우마스크 까지의 거리를 D,라 할 때 하기의 식을 만족하는 것이 바람직하다.In the fourth preferred embodiment, the thickness of the effective screen portion A, the thickness of the non-effective screen portion B, the thickness of the maximum non-effective screen portion C, the thickness of the effective screen portion + the distance from the inner surface of the panel to the shadow mask are D, When the following formula is satisfied.

A+2㎜ < B < D,A + 2 mm <B <D,

B = C < B+30㎜B = C <B + 30 mm

바람직한 제5 실시 예로는, 비 유효화면 부의 폭을 E라 할 때, C와 B의 영역을 갖는 비 유효화면 부 B와 C의 경계는 유효화면 부와 비 유효화면 부가 만나는경계선상에서 E의 1/3E∼2/3E 위치에 존재하는 것이 바람직하다.In the fifth preferred embodiment, when the width of the non-effective screen portion is E, the boundary between the non-effective screen portions B and C having the areas of C and B is 1 / E of E on the boundary line where the effective screen portion and the non-effective screen portion meet. It is preferable to exist in 3E-2 / 3E position.

바람직한 제6 실시 예로는, 비 유효화면 부가 구비된 상기 패널의 외측 둘레에는 보강밴드가 더 장착되는 것이 바람직하다.In a sixth preferred embodiment, it is preferable that a reinforcing band is further mounted on an outer circumference of the panel provided with an ineffective screen portion.

이하에서는 상기의 목적을 달성하는 본 발명의 바람직한 실시예를 첨부된 도면을 참조하여 보다 상세히 설명한다.Hereinafter, with reference to the accompanying drawings, preferred embodiments of the present invention for achieving the above object will be described in more detail.

설명의 편의를 위해 종래와 동일한 부분, 부재에 대해서는 동일 부호를 부여하여 설명한다.For convenience of explanation, the same parts and members as in the prior art will be described with the same reference numerals.

도 3에는 본 발명이 적용된 평면 음극선관의 측단면도가 도시되어 있고, 도 4 내지 도 5의 a,b에는 본 발명의 주요부를 보인 확대 단면도가 도시되어 있다.3 is a side cross-sectional view of a planar cathode ray tube to which the present invention is applied, and an enlarged cross-sectional view showing main parts of the present invention is shown in FIGS. 4 to 5 a and b.

이에 도시된 바와 같이, 또 상기 패널(10)의 후방에는 벌브(Bulb) 형상의 펀넬(20)이 프릿 글라스(Frit Glass)에 의해 패널(10)에 대해 일체로 융착되어 내부 진공압 약 10-7을 유지한 상태를 가지는 튜브(T)(또는 진공용기)를 형성하고 있다.Thus as shown, yet binary inside the funnel 20 in the rear, the bulb (Bulb) of the panel (10) shape is welded integrally to the panel 10 by the frit glass (Frit Glass) air pressure of about 10 - A tube T (or vacuum vessel) having a state of 7 is formed.

또한, 상기 패널(10)의 내측에는 장, 단축으로 분리 구성된 것이 부착되며 사각 틀의 형상을 갖는 마스크 지지체(30)가 접합되어 있다.In addition, a mask support 30 having a rectangular frame shape is attached to the inside of the panel 10.

상기 마스크 지지체(30)에는 슬릿 또는 공극 형상의 미세한 홀(41)이 형성된 새도우마스크(40)가 상기 마스크 지지체(30)에 대해 인장된 상태로 고정되어 있다.A shadow mask 40 having a slit or pore-shaped fine hole 41 is fixed to the mask supporter 30 in a tensioned state with respect to the mask supporter 30.

또한, 상기 펀넬(20)의 후방에 구비된 네크부(21)에는 R,G,B 의 영상신호에 따라 도면 표현상 가시화 된 전자빔을 방출하는 전자총(23)이 장착되어 있으며, 상기 펀넬(20)의 외측에는 수직/수평 방향으로 균일한 자계를 형성하여 전자빔(22)을굴절시키는 편향요크(50)가 설치되어 있는데 이들 구성은 종래의 기술에서 상술한 일반적인 평면 음극선관의 구성과 대동소이하다.In addition, the neck 21 provided at the rear of the funnel 20 is equipped with an electron gun 23 for emitting an electron beam visualized in the drawing representation according to image signals of R, G, and B, and the funnel 20. The deflection yoke 50 is formed on the outside of the deflection yoke 50 to form a uniform magnetic field in the vertical / horizontal direction to deflect the electron beam 22. These configurations are similar to those of the general planar cathode ray tube described above in the related art.

다만, 본 발명에서의 지배적인 특징부는, 비 유효화면 부분인 가장자리 테두리에 보강부(12)가 일체로 형성된다.However, the dominant feature of the present invention is that the reinforcing portion 12 is integrally formed at the edge of the non-effective screen portion.

상기 보강부(12)는 상기 패널(10)의 비 유효화면 부에 구비되며 적어도 한 개의 제1 단차(13)에 의해 유효화면 부의 두께보다 두껍게 구비된다.The reinforcement part 12 is provided in the non-effective screen part of the panel 10 and is provided thicker than the thickness of the effective screen part by at least one first step 13.

상기 보강부(12)에는 적어도 한 개의 제1 단차(13)가 형성되고, 그 내측에는 상기 마스크 지지체(30)가 장착되고, 외측에는 상기 펀넬(20)이 융착되는 것이 바람직하다.At least one first step 13 is formed in the reinforcement part 12, the mask supporter 30 is mounted on the inside thereof, and the funnel 20 is fused on the outside thereof.

또한, 바람직하게는, 상기 보강부(12)는 상기 패널(10)의 비 유효화면 부에 제1,2 단차(13)(14)가 단계적으로 배치되고, 상기 제1 단차(13)에는 상기 마스크 지지체(30)가 부착되며 상기 제2 단차(14)에는 펀넬(20)이 각각 양분된 상태에서 부착된 것이 바람직하다.In addition, preferably, the reinforcement part 12 includes first and second steps 13 and 14 disposed step by step on an ineffective screen part of the panel 10, and the first step 13 in the reinforcement part 12. The mask supporter 30 is attached, and the funnel 20 is preferably attached to the second step 14 in a bisected state.

또한, 바람직하게는, 패널의 유효화면 부의 두께를 A, 비 유효화면 부의 두께를 B, 최대 비 유효화면 부의 두께를 C, 유효화면 부의 두께+패널 내측면에서 새도우마스크 까지의 거리를 D,라 할 때 하기의 식을 만족하는 것이 바람직하다.Preferably, the thickness of the effective screen portion of the panel A, the thickness of the non-effective screen portion B, the thickness of the maximum non-effective screen portion C, the thickness of the effective screen portion + the distance from the inner surface of the panel to the shadow mask D, It is preferable to satisfy the following formula when doing so.

A+2㎜ < B < D,A + 2 mm <B <D,

B = C < B+30㎜B = C <B + 30 mm

상기와 같이 유효화면 부의 두께 C가 B+30㎜ 이상일 경우에는 보강효과의 상승은 없으면서 패널의 무게만을 상승시키게되는 문제가 있다.As described above, when the thickness C of the effective screen portion is B + 30 mm or more, there is a problem that only the weight of the panel is increased without increasing the reinforcing effect.

또한, 바람직한 제6 실시 예로는, 비 유효화면 부의 폭을 E라 할 때, C와 B의 영역을 갖는 비 유효화면 부 B와 C의 경계는 유효화면 부와 비 유효화면 부가 만나는 경계선상에서 E의 1/3E∼2/3E 위치에 존재하는 것이 바람직하다.Also, in the sixth preferred embodiment, when the width of the non-effective screen portion is E, the boundary between the non-effective screen portions B and C having the areas of C and B is defined by E on the boundary line where the effective screen portion and the non-effective screen portion meet. It is preferable to exist in the 1 / 3E-2 / 3E position.

한편, 본 발명에서 적용되는 유효화면 부가 구비된 상기 패널(10)의 외측 둘레에는 보강밴드(60)가 더 구비되는 것이 바람직하다.On the other hand, it is preferable that the reinforcing band 60 is further provided on the outer periphery of the panel 10 provided with the effective screen portion applied in the present invention.

물론, 본 발명에 따른 보강부는 패널을 제조할 때 일체로 제조할 수 있지만, 각 제1,2 단차부를 별도로 제작한 후 프릿 글라스에 의해 융착시켜 고정할 수도 있지만 상기와 같이 할 경우 본 발명의 목적인 공정시간 단축 그리고 생산성 향상의 측면에서 볼 때 바람직하지 못하다.Of course, the reinforcement portion according to the present invention can be manufactured integrally when manufacturing the panel, but after manufacturing the first and second stepped portions separately may be fused and fixed by frit glass, but the above is the object of the present invention It is not desirable from the standpoint of shortening process time and improving productivity.

상기와 같이 구성된 본 발명의 동작에 대해 설명한다.The operation of the present invention configured as described above will be described.

즉, 본 발명은 종래와 같이 패널(10)과 펀넬(20)을 프릿 글라스에 의해 융착시킨 상태에서 튜브(T)를 형성하며, 그 일련의 동작은 종래의 기술에서 설명한 바와 같이 일반적인 평면 음극선관과 동일하므로 이에 대한 별도의 부연 설명은 생략한다.That is, the present invention forms a tube (T) in a state in which the panel 10 and the funnel 20 are fused by frit glass as in the prior art, and the series of operations are performed in the general flat cathode ray tube as described in the related art. Since the description is the same as that of the additional description will be omitted.

다만, 본 발명에서의 지배적인 특징부는 패널의 전면에 부착되는 방폭유리를 삭제한 반면, 패널(10)의 비 유효화면 부인 가장자리의 두께를 두껍게 형성한 구조에 의해 패널(10)과 펀넬(20)이 접착되는 부분의 강도를 증가시켜 패널(10)과 펀넬(20)을 융착한 후 배기공정을 진행하더라도 그 접착부위에서 크게 발생되었던 응력에 대한 대응 응력이 발생되어 패널(10)과 펀넬(20)의 접착부위에서 발생되는 내부 응력을 감쇠시키게 된다.However, the dominant feature in the present invention is to eliminate the explosion-proof glass attached to the front of the panel, while the panel 10 and the funnel 20 by a thick structure of the edge of the non-effective screen denier of the panel 10 ) Is bonded to the panel 10 and the funnel 20 by increasing the strength of the bonded portion, even if the exhaust process proceeds to the stress corresponding to the stress generated largely in the bonding portion generated panel 10 and funnel (20) This attenuates the internal stresses generated at the bonding part of

또한, 본 발명에서의 다른 특징부는 보강부(12)에 의해 비 유효화면 부인 패널(10)의 가장자리 측이 두꺼워졌으므로 결국 보강밴드(60)를 패널(10)의 가장자리에 장착할 때에는 보강밴드(60)와의 접촉면적이 넓어져 외부로부터 부여되는 충격에 대응하는 응력 완화동작을 충분하게 할 수 있다.In addition, another feature of the present invention is that the edge side of the non-effective screen denying panel 10 is thickened by the reinforcing portion 12, so that when the reinforcing band 60 is attached to the edge of the panel 10, the reinforcing band ( The contact area with (60) becomes wider, and the stress relaxation operation corresponding to the impact applied from the outside can be made sufficient.

이상에서 상세히 설명한 바와 같이 본 발명에 의하면, 패널의 비 유효화면 부의 구조를 개선하여 패널과 펀넬을 프릿 글라스에 의해 융착한 후 내부를 진공상태로 유지하기 위한 배기공정을 할 때 패널과 펀넬이 접합된 부분으로 집중되는 응력을 감쇠시키는 효과가 있다.As described in detail above, according to the present invention, the panel and the funnel are bonded when the structure of the non-effective screen portion of the panel is improved and the panel and the funnel are fused by frit glass to perform the exhaust process for maintaining the interior in a vacuum state. There is an effect of damping the stress concentrated in the portion.

또 본 발명은 패널의 전면에 부착되었던 방폭유리와 광경화성 레진의 삭제가 가능함으로써 방폭유리를 부착하기 위한 별도의 작업공간을 줄일 수 있음은 물론, 방폭유리를 부착하기 위한 별도의 작업공간을 요하지 않으므로 제조코스트를 낮출 수 있는 효과도 있다.In addition, the present invention can reduce the separate work space for attaching the explosion-proof glass by eliminating the explosion-proof glass and photo-curable resin that was attached to the front of the panel, and does not require a separate work space for attaching the explosion-proof glass. Therefore, the manufacturing cost can be lowered.

지금까지는 본 발명의 바람직한 실시 예에 대하여 상세히 설명하고 또 도시하였지만 이에 한정하지 않고 당 분야에서 통상의 지식을 가진 자에 의해 다양하게 변경 사용이 가능하다.So far, the preferred embodiments of the present invention have been described and illustrated in detail, but are not limited thereto and can be variously changed and used by those skilled in the art.

그러나, 그와 같은 단순한 변경은 특허청구의 범위에 기재된 본 발명의 권리범위에 속함이 명백하다.However, it is apparent that such simple modifications fall within the scope of the present invention described in the claims.

Claims (6)

유효화면인 내측 면에 형광막이 도포되며 가장자리 테두리에 비 유효화면부가 형성된 패널; 상기 패널의 후방에 융착되는 벌브 형상의 펀넬; 상기 패널의 내측면에 상기 형광막의 외측 가장자리로 접착 배열된 마스크 지지체; 상기 마스크 지지체에 대해 인장된 상태로 고정되며 도트 또는 슬롯 형상의 홀이 형성된 새도우마스크; 상기 펀넬의 후방 끝단부에 봉입 설치되며 전자빔을 방사하는 전자총; 상기 펀넬의 잘록한 네크부에 형성되며 상기 전자총에 의해 방사되는 전자빔에 대해 균일한 자계를 형성하는 편향요크; 상기 패널의 전면부 테두리에 에워싸여지는 보강밴드를 포함하는 평면 음극선관에 있어서,A panel having a fluorescent film coated on an inner surface of the effective screen and having an ineffective screen portion formed at an edge of the panel; A bulb-shaped funnel fused to the rear of the panel; A mask supporter adhesively arranged to an outer edge of the fluorescent film on an inner surface of the panel; A shadow mask fixed in a tension state with respect to the mask supporter and having a dot or slot-shaped hole formed therein; An electron gun encapsulated in the rear end of the funnel and emitting an electron beam; A deflection yoke formed in the narrow neck portion of the funnel and forming a uniform magnetic field with respect to the electron beam emitted by the electron gun; In the flat cathode ray tube comprising a reinforcing band surrounded by the front edge of the panel, 상기 패널의 비 유효화면 부에는 적어도 한 개의 제1 단차에 의해 유효화면 부의 두께보다 두껍게 형성된 보강부가 구비된 것을 포함하는 평면 음극선관.And a reinforcing part formed thicker than the thickness of the effective screen part by at least one first step in the non-effective screen part of the panel. 제 1 항에 있어서,The method of claim 1, 상기 보강부에 형성된 적어도 한 개의 제1 단차 내측에는 상기 마스크 지지체가 장착되고, 외측에는 상기 펀넬이 융착되는 것을 포함하는 평면 음극선관At least one first step formed in the reinforcement portion is a planar cathode ray tube comprising a mask support is mounted on the inside, the outer side of the funnel fusion welded 제 1 항에 있어서,The method of claim 1, 상기 보강부는 상기 패널의 비 유효화면 부에 제1,2 단차가 단계적으로 배치되고, 상기 제1 단차에는 상기 마스크 지지체가 부착되며 상기 제2 단차에는 펀넬이 부착된 것을 포함하는 평면 음극선관.The reinforcing part of the flat cathode ray tube of claim 1, wherein the first step and the second step is disposed on the non-effective screen portion of the panel, the mask support is attached to the first step and the funnel is attached to the second step. 제 1 항에 있어서,The method of claim 1, 유효화면 부의 두께를 A, 비 유효화면 부의 두께를 B, 최대 비 유효화면 부의 두께를 C, 유효화면 부의 두께+패널 내측면에서 새도우마스크 까지의 거리를 D,라 할 때 하기의 식을 만족하는 것을 포함하는 평면 음극선관.When the thickness of the effective screen portion A, the thickness of the non-effective screen portion B, the thickness of the maximum non-effective screen portion C, and the thickness of the effective screen portion + the distance from the inner surface of the panel to the shadow mask D, the following equations are satisfied. Flat cathode ray tube comprising the. A+2㎜ < B < D,A + 2 mm <B <D, B = C < B+30㎜B = C <B + 30 mm 제 1 항 또는 제 4 항에 있어서,The method according to claim 1 or 4, 비 유효화면 부의 폭을 E라 할 때,When the width of the ineffective screen portion is E, C와 B의 영역을 갖는 비 유효화면 부 B와 C의 경계는 유효화면 부와 비 유효화면 부가 만나는 경계선상에서 E의 1/3E∼2/3E 위치에 존재하는 것을 포함하는 평면 음극선관.And the boundary between the non-effective picture portion B and C having the areas of C and B is present at positions 1 / 3E to 2 / 3E of E on the boundary line where the effective picture portion and the non-effective picture portion meet. 제 1 항에 있어서,The method of claim 1, 비 유효화면 부가 구비된 상기 패널의 외측 둘레에는 보강밴드가 더 장착된 것을 포함하는 평면 음극선관.Flat cathode ray tube comprising a reinforcing band is further mounted on the outer periphery of the panel provided with an ineffective screen portion.
KR1020030005694A 2003-01-29 2003-01-29 Flat CRT KR20040069370A (en)