KR200373391Y1 - Rub weld device for bundle-band of packing machine - Google Patents
Rub weld device for bundle-band of packing machine Download PDFInfo
- Publication number
- KR200373391Y1 KR200373391Y1 KR20-2004-0030038U KR20040030038U KR200373391Y1 KR 200373391 Y1 KR200373391 Y1 KR 200373391Y1 KR 20040030038 U KR20040030038 U KR 20040030038U KR 200373391 Y1 KR200373391 Y1 KR 200373391Y1
- Authority
- KR
- South Korea
- Prior art keywords
- band
- electric
- friction
- substrate
- base
- Prior art date
Abstract
본고안은 포장기의 묶음밴드를 전기용접방식으로 이룩한 기계적마찰방식으로 용해접합하는 장치를 제공하는 것을 그 목적으로 하고 있다.The purpose of this paper is to provide a device for melt bonding a bundle band of a packaging machine by a mechanical friction method achieved by electric welding.
포장기의 본체의 적당한 장소에 묶음밴드의 중합부(重合部)를 위로부터 누르는 상밴드 기판과, 밑으로부터 눌러서 밴드를 끼워 하밴드 기판의 하방으로 연결하여, 하밴드의 기판을 상방으로 밀어올리는 가압구를 가지며, 또한 밴드 기판을 전후로 왕복시켜 이동시키는 마찰발생구를 부설하여, 상하밴드기판의 사이에 끼워진 밴드의 중합부(重合部)에 마찰을 가하여 고온을 발생시켜 용해시키고, 그것으로 밴드를 접합할수 있도록 구성되어 있는 포장기의 묶음밴드 마찰용접장치The upper band substrate which presses the polymerization part of a bundle band from the top in the suitable place of the main body of a packing machine, and presses from below and presses a band, connects it to the lower side of the lower band board | substrate, and presses the board of a lower band upwards A friction generating port having a sphere and a reciprocating band substrate is moved back and forth, and friction is applied to the polymerized portion of the band sandwiched between the upper and lower band substrates to generate a high temperature to dissolve the band. Bundle band friction welding device of packing machine configured to join
Description
본고안은 포장기의 묶음밴드를 마찰에 의해 고온을 발생시켜 용해연결하는 장치에 관한 것이다.The present invention relates to a device for melting and connecting a bundle band of a packaging machine by generating a high temperature by friction.
종래의 일반적인 포장기는 공작대의 위에 밴드를 묶는 물품을 놓아, 밴드묶음장치로서 밴드를 물품의 주위에 감아붙여서 단단하게 묶고나서, 밴드용접장치로서 밴드가 중합(重合)하는 장소에 열을 가하여 용해시켜 접합시킨 후 절단한다. 전통적인 포장기의 용접장치는 대부분 전기용접의 방식을 사용하여 밴드의 중합부분을 전열히터의 가운데 끼워서 그 부분을 용해한 후, 전열히터를 제거하고 용해된 접합부분을 냉각시켜서 접합한다.Conventional general packaging machines place articles to bind the band on the workbench, wrap the band around the article as a band bundling device to bind it tightly, and then heat and dissolve the band as a band welding device where the band is polymerized. After bonding, cut. In the conventional packaging machine welding apparatus, most of the welding machines use an electric welding method to insert the polymerized part of the band in the center of the electric heater to dissolve the part, and then remove the electric heater and cool the melted joint.
그러나 종래의 전통적인 전기용접에 의한 밴드의 접합방법은 포장기가 작동한 후의 조작진행중에는 전열히터가 계속하여 고온상태로 유지되고 있기 때문에, 온도가 지나치게 높아, 파손되기 쉽고 또한 이를 위한 열의 부족이 발생하여 유효하게 열용접의 목적을 달성할 수 없고, 그래서 그 사용수명을 단축시키고, 또한 고열로 인하여 일어나는 의외의 접촉에 의한 위험성이 있었다.However, in the conventional method of joining the band by conventional electric welding, since the electric heater is kept at a high temperature continuously during the operation after the packaging machine is operated, the temperature is too high, it is easy to be damaged, and there is a lack of heat for this. Effectively, the purpose of heat welding could not be achieved, so that the service life was shortened, and there was a danger of unexpected contact caused by high heat.
본 고안은 상기한 종래의 문제점을 해결하기 위하여 안출된 것으로서,The present invention is devised to solve the above-mentioned conventional problems,
종래의 전열용접에 의한 포장기의 묶음밴드의 방법을 일종의 기계식 마찰에 의한 용접으로 변경하여 이러한 결점을 제거함에 그 목적이 있다.The purpose of this method is to eliminate this defect by changing the conventional method of the bundle band of the packaging machine by electrothermal welding to a kind of mechanical friction welding.
도1은 본고안 포장기의 국부단면도이고,1 is a local cross-sectional view of the packaging machine of the present invention,
도2는 상(上)접착 밴드의 기판과, 마찰구와 가압안내구의 상대관계를 나타내는 측면도이고,Fig. 2 is a side view showing the relative relationship between the substrate of the upper bonding band, the friction sphere and the pressing guide;
도3은 본고안의 마찰구를 다른 각도에서 본 상면도이고,Figure 3 is a top view of the friction sphere in this view seen from another angle,
도4는 본고안의 마찰용접의 동작을 나타내는 측면도이다4 is a side view showing the operation of friction welding in the present article;
<도면의 주요부분에 대한 부호의 설명><Description of the symbols for the main parts of the drawings>
1 : 포장기본체 2 : 마찰용접장치1: packaging body 2: friction welding device
3 : 묶음밴드 10 : 상밴드기판3: bundled band 10: upper band substrate
11 : 밴드잡이 고정면 20 : 가압구11: band holder fixing surface 20: pressure port
21 : 좌대 22 : 로울러21: left arm 22: roller
30 : 마찰동작구 31 : 기대30: friction action 31: expectation
311 : 저판(底板)311: bottom plate
상기한 목적을 달성하기 위한 기술적인 구성으로서, 본 고안의 묶음밴드 마찰용접장치는 상밴드 기판과 하밴드 기판을 포장기의 본체의 적당한 장소에 부설하여 묶음밴드의 중합부를 단단하게 죌 수 있도록 한다. 상밴드기판을 고정하여 움직이지 않고, 하밴드기판은 상하로 움직이도록 그 밑에 가압구를 연결하여 그 가압구가 하밴드기판을 상하로 움직이도록 한다. 또한 하밴드기판이 밴드의 중합부를 끼운 후, 하밴드기판을 전후로 신속하게 왕복으로 움직이게 하는 마찰발생구를 설치한다. 이 마찰발생구는 모우터와 2개의 벨트차(車)와, 편심(偏心)샤프트와 추봉(推棒)과 연결괴(連結塊)를 조합하여, 그로서 모우터가 회전하면, 추봉(推棒)의 선단에 맞추어 설치된 연결괴(連結塊)는 편심(偏心)샤프트의 작용에 의하여 하 밴드기판을 신속하게 전후로 왕복하여 이동시켜, 그로서 하밴드기판은 밴드의 중합부에 마찰작용을 가하여, 고온을 발생하여 용해시켜, 그로서 냉각하면 단단하게 접합할 수 있게된다.As a technical configuration for achieving the above object, the bundled band friction welding apparatus of the present invention is to install the upper band substrate and the lower band substrate in a suitable place of the main body of the packaging machine to firmly hold the polymerized portion of the bundle band. The upper band substrate is fixed and does not move, and the lower band substrate is connected to the pressurization hole underneath so as to move up and down so that the pressing hole moves the lower band substrate up and down. In addition, the lower band substrate is provided with a friction generating port for moving the lower band substrate back and forth quickly back and forth after inserting the polymerized portion of the band. This friction generating port combines a motor, two belt cars, an eccentric shaft, a weight bar, and a connecting rod, and when the motor rotates, the weight bar Joints installed at the tip of the head) move the lower band substrate back and forth quickly by the action of the eccentric shaft, so that the lower band substrate applies friction to the polymerized part of the band. The high temperature is generated, dissolved, and cooled, whereby it can be bonded firmly.
본고안의 포장기의 묶음밴드의 마찰용해장치는 그 상밴드기판과 하밴드기판의 사이에 끼워져있는 밴드의 하밴드기판의 전후로 신속하게 왕복하여 이동하는 것에 의해 밴드에 마찰작용을 가하여, 그로서 밴드에 고온이 발생하여 용해되므로 이를 냉각시키면 그 중합부가 단단하게 접합된다.The friction dissolution device of the bundle band of the packing machine in this paper applies friction to the band by rapidly reciprocating back and forth between the upper band substrate and the lower band substrate of the band sandwiched between the upper band substrate and the lower band substrate. Since high temperature is generated and dissolved, the polymerized part is firmly bonded when cooled.
<실시례><Example>
본고안 포장기의 묶음밴드 마찰용접장치의 비교적 양호한 실시례는, 도1과 도2에 나타난 바와 같이 포장기본체(1)의 적당한 장소에 상밴드기판(10)과 가압구(20)와 마찰동작구(30)를 설치하여 구성된다.A comparatively preferred embodiment of the bundled band friction welding device of the present packaging machine includes the upper band substrate 10, the pressurizing opening 20, and the friction operation mechanism (see Fig. 1 and Fig. 2) at a suitable place of the packaging main body (1). 30) is configured by installing.
그 중 상밴드기판(10)은 포장기본체(1)의 묶음밴드가 중합부를 용접하는 장소의 가까이에 고정설치되어 그 말단면에 울퉁불둥하고 조잡한 상밴드포착고정면(11)을 설치하여 둔다.Among them, the upper band substrate 10 is fixed near the place where the bundle band of the packaging base body 1 welds the polymerization part, and the bumpy and coarse upper band trapping fixing surface 11 is provided on the end surface thereof.
그 중의 가압구(20)는 좌대(21)을 하부에 가지며, 상방에는 로울러(22)를 지축(支軸)으로 설치하여, 좌대(21)와 함께 상밴드기판(10)의 방향으로 이동하게 된다.좌대(21)는 탄성고무(도면에 도시되어 있지 않음)의 작동으로 움직이지만, 이 탄성고무의 작동방식은 잘 알려진 기술이므로 그 상세한 설명은 생략한다.Among them, the pressure port 20 has a pedestal 21 at the lower portion thereof, and a roller 22 is installed on the upper portion of the upper portion of the pressurizing member 20 so as to move in the direction of the upper band substrate 10 together with the pedestal 21. The seat 21 is moved by the operation of the elastic rubber (not shown in the figure), but the operation of the elastic rubber is a well-known technique and its detailed description is omitted.
그 중의 마찰동작구(30)는 도2가 나타내는 바와 같이 포장기본체(1)를 가지고 포장기본체(1)는 저판(311)을 가지며, 이 저판(311)은 포장기본체(1)의 적당한 장소에 고정설치되어, 저판(311)의 말단은 U형모우터 고정판(312)과 베어링좌(313)를 고정설치하고, 이 모우터고정판(312)의 위에는 모우터(32)가 고정된다.As shown in Fig. 2, the friction operation tool 30 has a packaging body 1, and the packaging body 1 has a bottom plate 311, which is fixed to a suitable place of the packaging body 1. The end of the bottom plate 311 is fixed to the U-shaped motor fixing plate 312 and the bearing seat 313, and the motor 32 is fixed on the motor fixing plate 312.
이 모우터(32)는 출력샤프트(321)를 가진다. 이 출력샤프트(321)는 직각으로 모우터고정판(312)에 축설 연결된다.This motor 32 has an output shaft 321. The output shaft 321 is axially connected to the motor fixing plate 312 at a right angle.
또 도3에 나타내는 바와 같이 베어링좌(313)는 편심샤프트(33)와 축설로 연결되어, 이 편심샤프트(33)는 거의 그 중단(中段)에 편심부(331)를 형성하여, 이 편심부(331)는 추봉(34)의 말단과 편심 연결되어 고정위치한다. 이 추봉(推棒)(34)의 다른 말단은 연결괴(35)를 연결하고 , 이 연결괴(35)는 U자형구(溝)(351)를 가지며, 이 U자형구(溝)(351)는 가압구(20)의 로울러(22)의 외주면에 가동적(可動的)으로 끼워지고, 다시 연결괴(35)에 하밴드기판(36)을 단단하게 옥죈다. 또 도2 및도4에 나타내는 바와 같이 이 하밴드기판(36)의 말단은 울퉁불퉁하고 조잡한 하밴드포착 고정면(361)을 형성하여, 상밴드기판(10)의 상밴드포착 고정면(11)과 대향하게 한다. 또한 모우터(32)의 출력샤프트(321)와 편신샤프트(33)의 적당한 장소에 각별하게 제1벨트차(車)(37)와 제2벨트차(38)를 고정설치하여, 벨트(39)를 이 양벨트차의 주위에 걸어서 연결하여 그로서 모우터(32)의 출력이 편심샤프트(33)에 전동(傳動)되게한다.As shown in Fig. 3, the bearing seat 313 is connected to the eccentric shaft 33 in a concentric manner, and the eccentric shaft 33 almost forms an eccentric portion 331 at the middle thereof. 331 is eccentrically connected to the distal end of the weight bar (34) is fixed. The other end of the weight rod 34 connects the connecting rod 35, and the connecting rod 35 has a U-shaped sphere 351, and this U-shaped sphere 351 ) Is movable on the outer circumferential surface of the roller 22 of the pressure port 20, and the lower band substrate 36 is firmly squeezed to the connecting ingot 35 again. 2 and 4, the lower end of the lower band substrate 36 forms an uneven and coarse lower band trapping fixing surface 361, and the upper band trapping fixing surface 11 of the upper band substrate 10 is formed. To face. Further, the first belt car 37 and the second belt car 38 are fixedly installed at appropriate positions of the output shaft 321 and the single-shaft shaft 33 of the motor 32, and the belt 39 ) Is hooked around these two belt cars so that the output of the motor 32 is transmitted to the eccentric shaft 33.
다음에 본고안의 사용방법과 그 작용을 설명한다.The following describes how to use this paper and its operation.
우선 도2, 3과 4를 참고로 한다.First, reference is made to FIGS. 2, 3 and 4.
포장기의 위에 놓여진 물품이 밴드(3)으로 감아붙여져서 묶여진 때에는 밴드(3)는 포장기본체(1)의 적당한 장소에 중합(重合)한다. 그리고 마찰용접장치When the article placed on the packaging machine is wound by the band 3 and bundled, the band 3 polymerizes in a suitable place of the packaging base body 1. And friction welding device
(2)가 스타트되어, 가압구(20)의 좌대(21)가 상밴드기판(10)쪽으로 이동되어 압력을 가한다.(2) is started, and the base 21 of the pressure port 20 is moved to the upper band substrate 10 to apply pressure.
이와 동시에 마찰동작구(30)의 연결괴(35)와 하밴드기판(36)을 움직여서, 하밴드기판(36)의 하밴드 포착 고정면(361)은 밴드(3)의 중합부를 상밴드기판(10)의 상밴드포착고정면(11)에 눌러붙인다. 이때 마찰구(30)의 모우터(32)가 처음으로 스타트되어 회전하면, 출력은 순서대로 출력샤프트(321)을 경유하여, 제1벨트차(37)와 벨트(39)와 제2벨트차(38)가 회전과 이동을 하여, 편심샤프트(33)이 회전된다. 그래서 편심샤프트(33)의 편심부(331)의 위에 있는 추봉(推棒)(34)이 바이어스(bias)작동을 발생시켜 그 말단에 있는 연결괴(35)를 전후로 왕복하여 밀어내어 로울러(22)의 외주면에서 신속히 전후로 미끄어져 움직이고, 그로서 연결괴(35)로 연결되어 있는 하밴드기판(36)도 밴드(3)의 중합부의 밑에서 신속히 전후로 왕복이동하여 밴드(3)에 대하여 마찰작용을 가한다. 밴드(3)의 중합부는 그 상하가 각상하밴드기판(10)과 (36)으로 적당한 압력으로 끼워져 있어, 이 양기판은 상하밴드포착고정면(11)과(361)로서 밴드(3)를 붙잡고 또한 움직이지 않도록 고정하고있기 때문에, 모우터(32)가 스타트되면, 이 밴드(3)의 중합부는 극히 단시간에의 마찰작용으로 고열을 발생하여 녹은상태로 되고, 냉각시키면 그 중합부가 단단하게 접합되어 작업을 마친다.At the same time, the connection band 35 and the lower band substrate 36 of the friction operation tool 30 are moved, so that the lower band capturing fixing surface 361 of the lower band substrate 36 has a polymerized portion of the band 3 formed on the upper band substrate ( It is pressed against the upper band catching fixed surface 11 of 10). At this time, when the motor 32 of the friction ball 30 is first started and rotated, the output is sequentially passed through the output shaft 321, and the first belt car 37, the belt 39, and the second belt car. 38 rotates and moves, and the eccentric shaft 33 is rotated. Thus, the rod 34 on the eccentric portion 331 of the eccentric shaft 33 generates a biasing operation to reciprocate the connecting rod 35 at its end back and forth to push the roller 22. The lower band substrate 36, which slides back and forth on the outer circumferential surface of the circumferential surface) and is thus connected to the connecting rod 35, also reciprocates back and forth quickly under the polymerization portion of the band 3 to perform friction action against the band 3. Add. The polymerized portion of the band 3 is inserted into the upper and lower band substrates 10 and 36 at an appropriate pressure, and the two substrates have the band 3 as the upper and lower band trapping fixing surfaces 11 and 361. Since the motor 32 is started when the motor 32 is started, the polymerized portion of the band 3 is melted due to frictional action in a very short time and becomes molten. Joined to finish the work.
상술한 구성으로 이루어진 본 고안은 다음과 같은 효과를 갖는다.The present invention made of the above-described configuration has the following effects.
본고안의 상하기판(10)(36)이 기계식의 신속한 마찰작용으로 그 사이에 끼워진 밴드의 중합부가 고온을 발생하여, 용접된 후 냉각하여 단단하게 용접되는 것에 의하고, 전통식의 전열가열에 의한 용접이 아니므로 여기에 수반하는 고열접촉으로 일어나는 위험성이 없다. 또 이 전통식의 전열가열에 의한 과열로부터 발생하는 기구의 파손이나 작업인원에 대한 신체상해의 위험도 없다. 그외 온도부족의 현상도 생기지 않고, 사용수명이 비교적 길고 그 용접의 품질도 안정되어있다The upper and lower substrates 10 and 36 of the present invention are formed by the high-speed polymerization of the bands sandwiched between them by rapid mechanical action, which is welded and cooled and welded firmly. Therefore, there is no risk of high temperature contact accompanying them. In addition, there is no risk of damage to the equipment or physical injury to the workforce resulting from overheating caused by this conventional electric heating. In addition, there is no phenomenon of lack of temperature, the service life is relatively long, and the welding quality is stable.
Claims (2)