KR20030015558A - manufacturing process for a file for a nail grinder - Google Patents

manufacturing process for a file for a nail grinder Download PDF

Info

Publication number
KR20030015558A
KR20030015558A KR1020010049344A KR20010049344A KR20030015558A KR 20030015558 A KR20030015558 A KR 20030015558A KR 1020010049344 A KR1020010049344 A KR 1020010049344A KR 20010049344 A KR20010049344 A KR 20010049344A KR 20030015558 A KR20030015558 A KR 20030015558A
Authority
KR
South Korea
Prior art keywords
plate
board
nail
file
beauty
Prior art date
Application number
KR1020010049344A
Other languages
Korean (ko)
Inventor
김상석
Original Assignee
김상석
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김상석 filed Critical 김상석
Priority to KR1020010049344A priority Critical patent/KR20030015558A/en
Publication of KR20030015558A publication Critical patent/KR20030015558A/en

Abstract

PURPOSE: A method for manufacturing nail polishing file is provided, which maintains the polishing function despite carelessly handling of a file and makes more flexible and sustainable beauty file. CONSTITUTION: The method for manufacturing nail polishing file comprises four manufacturing processes. An attaching process is putting a plate(6) on a board(4) by roller with pressure. An etching process is etching the plate(6) with chemicals. The next process is spreading a polishing compound(10) over the plate(6) by an injection device. The final process is a molding process for completed product of beauty file plate(2).

Description

손톱연마용 줄 제조방법{manufacturing process for a file for a nail grinder}Manufacturing process for a file for a nail grinder

본 발명은 손톱연마용 줄 제조공정에 관한 것으로서, 특히 미용줄판을 에폭시수지 또는 폐놀수지와 금속판등의 재질로 된 미용줄판을 구성하므로써, 부주의로 미용줄판을 취급하더라도 연마기능이 항시 유지될 수 있게 하고, 또한 미용줄판이 플렉시블한 기능을 갖도록 한 제조방법을 실현하므로써 생산성과 품질이 보다 향상될 수 있게 하는데에 있으며, 이와 함께 손톱등에 작용력이 완만하게 전달되게 하므로써 균형적인 연마가 이루어지도록 하여 숙련성 없이도 편리하게 사용할 수 있게 한 손톱연마용 줄 제조방법에 관한 것이다.The present invention relates to a nail polishing file manufacturing process, and in particular, by configuring a beauty lineboard made of a material such as epoxy resin or waste paper and metal plate, careless care can be maintained at all times even if handled careless line In addition, it is possible to improve the productivity and quality by realizing the manufacturing method to make the beauty line has a flexible function, and also to smoothly transfer the action force to the nails, etc. The present invention relates to a method for manufacturing a nail polishing line that can be conveniently used.

일반적으로 신체의 일부를 구성하는 손톱은 시간이 지남에 따라서 점차적으로 자라나서 길어지게 되는데, 이와 같이 길어지는 손톱은 미용을 위해서 손톱깍이등을 이용하여 적절한 크기로 절단한 후, 청결을 유지하기 위하여 미용줄판을 이용하였다.In general, the nails that make up a part of the body gradually grow over time and lengthen, and the longer nails are cut to an appropriate size using a nail clipper for beauty, and then maintained for beauty. The board was used.

이와같이 이용되는 미용줄판은 사용하는 과정에서 부주의로 쉽게 파손되거나 부분적으로 손상을 입게 되어 폐기해야 되는 결점을 지니고 있는데, 이러한 결점을 해소하기 위해 새로운 제품을 만들기 위한 제조방법이 요구되는 추세이다.The beauty stripe used in this way has a drawback that must be discarded because it is easily inadvertently broken or partially damaged in the process of use, and a manufacturing method for making a new product is required to solve such a drawback.

종래의 기술을 구성하는 제 1 실시예는 도 4 에 도시된 바와 같이 샌드페이퍼(102)가 구성되는데, 상기 샌드페이퍼(102)는 베이스를 이루는 페이퍼(104)가 주로 직물로 이루어져 구성되고, 상기 페이퍼(104) 전면에는 연마제(106)가접착제(108)로 정착되면서 전면에 걸쳐 도포된다.The first embodiment constituting the prior art is composed of a sand paper 102, as shown in Figure 4, wherein the sand paper 102 is composed of a base paper 104 is mainly made of a fabric, the paper ( 104) The abrasive 106 is applied over the entire surface while the abrasive 106 is fixed to the adhesive 108.

상기와 같이 구성되는 샌드페이퍼(102)를 사용하게 되면, 연마제(106)가 손톱 끝단부분을 연마하면서 일정한 모양으로 만들어주게 된다.When the sandpaper 102 configured as described above is used, the abrasive 106 is made into a predetermined shape while polishing the end of the nail.

상기 연마제(106)가 일정기간 사용되면 점차적으로 마모 되거나 페이퍼(104)로부터 분리되어 떨어지게 된다.When the abrasive 106 is used for a certain period of time, it gradually wears away or separates from the paper 104.

상기와는 달리 사용자가 부주의로 물 등에 빠뜨리게 되면, 상기 페이퍼(104)가 직물로 이루어진 특성으로 인하여 페이퍼(104)로 흡수되는데, 이로 인하여 상기 페이퍼(104) 전면에 위치한 접착제(108)는 접착력이 저하되어 연마제(106)의 정착 정도를 불안정하게 만든다.Unlike the above, when the user inadvertently falls into water or the like, the paper 104 is absorbed into the paper 104 due to the characteristics of the fabric, which causes the adhesive 108 located on the front surface of the paper 104 to have an adhesive force. This lowers, making the fixing degree of the abrasive 106 unstable.

또한 상기한 페이퍼(104)가 직물로 이루어져 있어 잘 구겨지게 됨에 따라, 접혀지는 샌드페이퍼(102) 부분은 사용하기에 곤란한 문제점을 지니게 된다.In addition, as the paper 104 is made of a woven fabric that is wrinkled well, the folded portion of the sand paper 102 has a problem that is difficult to use.

한편 종래의 기술을 구성하는 제 2 실시예로는 선출된 공개특허번호 제 99-73159호(손톱미용 줄판의 제조방법)에서 살펴보면 다음과 같다.On the other hand, as a second embodiment of the prior art, look at the selected Patent Publication No. 99-73159 (manufacture method of nail file) as follows.

먼저 종전에 사용하던 방법으로는 요철무늬패턴을 도안하여 필름화한 뒤, 스테인레스 등의 금속판에 감광하여 현상하고 이를 고온에서 가열한 뒤 염화제이철로 금속표면을 부식시켜 표면에 요철로 형성된 손톱미용줄판을 제조하고, 이 줄판을 원하는 형상으로 절단하여 제품화하였다.First of all, the method used in the past is to make a film by patterning the uneven pattern, and then develop it by exposing it to a metal plate such as stainless, and heating it at a high temperature, and then corroding the metal surface with ferric chloride to form the uneven nail plate on the surface. Was prepared, and this file board was cut into a desired shape to produce a product.

이러한 방법은 제조공정이 증가하여 생산성이 떨어지는 결점을 지니고 있는데, 이러한 결점을 해소하기 위해 종래의 제 2 실시예에서는 다음과 같은 방법을 실시하였다.This method has a drawback in that the productivity increases due to the increase in the manufacturing process, in order to solve this drawback in the second embodiment of the prior art was carried out as follows.

먼저 손톱미용줄판의 제조방법에 있어서, 증류수 1ℓ에 설파민산니켈 300-600g을 첨가하여 전해질 용액을 조성하고, 상기 전해질 용액의 온도를 40-60℃로 유지하는 단계: 상기 원판에 부(-) 전압을 인가하고 상기 니켈판에 정(+)전압을 소정 시간 인가하여 니켈 이온을 상기 원판의 요철면 표면에 소정 두께로 석출한 뒤 이를 상기 원판에서 분리하여 니켈 기판을 제조하는 단계: 상기 기판과 니켈판을 일정 간격을 두고 상기 전해질 용액에 담근 뒤, 상기 기판에 부(-) 전압을 인가하고 상기 니켈판에 정(+)전압을 소정 시간 인가하여 상기 기판의 요철면 표면에 니켈 이온을 소정 두께로 석출한 뒤 이를 상기 기판에서 분리함으로써, 표면에 요철이 형성된 니켈도금판을 제조하는 단계를 포함하고, 상기 니켈도금판 제조 단계를 반복함으로써 니켈로 구성된 손톱미용줄판을 반복 생산하는 것을 특징으로 한다.First, in the method for producing a nail beauty board, to prepare a electrolyte solution by adding 300-600 g of nickel sulfamate to 1 liter of distilled water, and maintaining the temperature of the electrolyte solution at 40-60 ℃: negative (-) to the disc Manufacturing a nickel substrate by applying a voltage and applying a positive voltage to the nickel plate for a predetermined time to deposit nickel ions at a predetermined thickness on the surface of the uneven surface of the disc, and then separating them from the disc to produce a nickel substrate: After the nickel plate is immersed in the electrolyte solution at a predetermined interval, a negative voltage is applied to the substrate and a positive voltage is applied to the nickel plate for a predetermined time so that nickel ions are defined on the uneven surface of the substrate. By depositing a thickness and separating it from the substrate, thereby producing a nickel plated plate having an uneven surface formed thereon, and repeating the nickel plated plate manufacturing step, the hand composed of nickel It characterized by repeatedly producing beauty julpan.

상기한 종래의 제 2 실시예에 의해 만들어진 손톱미용줄판은 전체가 경도가 큰 니켈로 구성됨으로써 플렉시블하게 사용되기에는 어려움이 있게 되는데, 이로 인해 사용자가 손톱미용줄판에 작용력을 가하게 되면 일방적으로 손톱등에 전달된다.Nail beauty bar made by the second embodiment of the prior art is difficult to be used flexibly because the whole is made of a nickel with a high hardness, because of this, when the user applies the action force to the nail beauty board unilaterally Delivered.

따라서 손톱을 전체적으로 균형적인 연마가 이루어지도록 하기 위해서는, 손톱미용줄판에 가하여지는 작용력이 항상 일정하게 되도록 하여야 하는데, 이러한 수단은 숙련성이 요구되어 사용상 불편함이 제기된다.Therefore, in order to achieve a balanced polishing of the nail as a whole, the force applied to the nail beauty board should always be constant, which means that the use of skill requires inconvenience.

이에 본 발명은 미용줄판을 에폭시수지 또는 폐놀수지와 금속판등의 재질로 된 미용줄판을 구성하므로써, 부주의로 미용줄판을 취급하더라도 연마기능을 소원하게 유지할 수 있게 하는데에 그 목적이 있다.Accordingly, the present invention has a purpose to be able to maintain the polishing function wishes carelessly handling the beauty stripe by configuring the beauty stripe made of a material such as epoxy resin or waste paper and metal plate.

다른 목적으로는 미용줄판이 플렉시블한 기능을 갖도록 하므로써, 작용력이 손톱에 완만하게 전달되게 하여 안정적인 연마가 이루어질 수 있게 하는데에 있다.Another purpose is to allow the beauty line to have a flexible function, so that the action force is gently transmitted to the nail to enable a stable polishing.

이를 실현하기 위한 본 발명은, 보오드상에 플레이트를 위치 시킨 후 고주파가열하면서 가압로울러로 가압하여 일체화시키는 부착단계와, 상기 부착단계 이후로 플레이트 표면에 약물로 부식시켜 무늬를 형성시키는 에칭단계와, 상기 에칭단계 이후로 연마제를 플레이트상에 분사장치로 분사하여 정착시키는 도포단계와, 상기 도포단계 이후로 완제품인 미용줄판을 만드는 성형단계로 이루어진다.The present invention for realizing this is, after placing the plate on the board and the high frequency heating while pressing the pressure roller and the integration to integrate, and the etching step to form a pattern by corrosion on the surface of the plate after the attachment step, After the etching step is composed of a coating step of spraying the abrasive on the plate by the injection device and fixing, and a molding step of making the finished cosmetic line after the coating step.

도 1 는 본 발명의 실시예를 나타낸 미용줄판의 사시도.1 is a perspective view of a cosmetic strip showing an embodiment of the present invention.

도 2 는 본 발명의 실시예인 미용줄판의 측단면도.Figure 2 is a side cross-sectional view of the cosmetic strip that is an embodiment of the present invention.

도 3 (a)(b)(c)(d)(e)는 본 발명인 미용줄판의 제조공정도.Figure 3 (a) (b) (c) (d) (e) is a manufacturing process diagram of the present invention beauty line.

도 4 는 종래의 제 1 실시예를 나타낸 부분 상세도.4 is a partial detailed view showing a conventional first embodiment.

<도면의 주요 부분에 대한 부호의 설명><Explanation of symbols for the main parts of the drawings>

2:미용줄판 4:보오드 6:플레이트2: beauty line 4: board 6: plate

8:무늬 10:연마제 12,16:가이드롤러8: Pattern 10: Polishing 12, 16: Guide Roller

18:가압롤러 20:고주파가열장치 22:약물18: pressure roller 20: high frequency heating device 22: chemicals

24:분사장치 26:프레스24: spraying device 26: press

본 발명은 도 1, 2 에 도시된 바와 같이 미용줄판(2)이 구성되는데, 상기 미용줄판(2)에는 소정의 두께를 지니고 있는 보오드(4)가 구성된다.In the present invention, as shown in Figs. 1 and 2, the cosmetic strip 2 is configured, and the cosmetic strip 2 has a board 4 having a predetermined thickness.

이때 상기 보오드(4)는 자유로이 구부릴 수 있도록 에폭시수지 또는 폐놀수지 재질로 이루는데, 이중 어느 하나를 선택하여 적용할 수 있다.At this time, the board 4 is made of an epoxy resin or waste-knot resin material so that it can be bent freely, any one of them may be selected and applied.

그리고 상기 보오드(4) 전면에는 고주파가열에 의해 고정설치되는 플레이트(6)가 금속으로 이루어지면서 위치하는데, 상기 플레이트(6)는 플렉시블하게 유동할 수 있도록 상기 보오드(4) 보다는 매우 얇은 두께로 이루어진다.In addition, the front surface of the board 4 is positioned while the plate 6 fixed by high frequency heating is made of metal, the plate 6 is made of a very thin thickness than the board 4 so as to be able to flow flexibly .

또한 상기 플레이트(6) 전면에는 사용자의 손톱을 용이하게 연마할 수 있도록 그루브 타입의 무늬(8)를 형성할 수 있는데, 이러한 무늬(8)는 모양에 구애받지 않고 다양하게 형성시킬 수 있다.In addition, the front surface of the plate 6 may be formed with a groove-type pattern 8 so that the user's fingernails can be easily polished, and the pattern 8 may be variously formed regardless of the shape.

이와 함께 상기 플레이트(6) 전면에는 손톱을 연마하는 연마제(10)가 접착제등으로 정착되어 위치한다.Along with the plate 6, an abrasive 10 for polishing nails is fixed and fixed with an adhesive or the like.

미 설명부호는 : 12,16:가이드롤러 14:가압장치 18:가압롤러Unexplained code: 12, 16: guide roller 14: pressurizing device 18: press roller

20:고주파가열장치 22:약물 24:분사장치 26:프레스20: high frequency heating device 22: chemicals 24: injection device 26: press

상기와 같이 구성되는 본 발명의 작용을 설명하면 다음과 같다.Referring to the operation of the present invention configured as described above are as follows.

먼저 사용자는 일정 길이로 자란 손톱을 별도록 구비하고 있는 손톱깍이로 소정 길이만큼 절단하고, 마무리를 하기 위하여 상기 미용줄판(2)을 이용하게 되는데 그 작용은 다음과 같다.First, the user cuts a predetermined length with a nail clipper provided to separate the nails grown to a predetermined length, and uses the beauty strip 2 to finish the operation.

최초 사용자는 미용줄판(2) 후미를 손으로 붙잡고 선단부의 플레이트(6)는 연마하고자 하는 손톱에 밀착시킨다.The first user grasps the tail of the cosmetic line 2 by hand, and the plate 6 of the tip is brought into close contact with the nail to be polished.

그리고 상기 미용줄판(2) 중간 또는 후미에 적정한 가압력을 가하면서 밀거나 당기면, 상기 플레이트(6) 전면에 정착된 연마제(10)가 손톱을 연마하게 되어 길이가 조금씩 줄어들게 한다.And when pushing or pulling while applying the appropriate pressing force to the middle or rear of the beauty line 2, the abrasive 10 fixed to the front surface of the plate 6 to polish the nails to reduce the length slightly.

이때 상기 보오드(4)가 에폭시수지 또는 폐놀수지 재질로 되어 있는 관계로, 상기 미용줄판(2)은 탄력적으로 휘어지면서 전달되어 오는 가압력을 흡수하여 상쇄하므로써, 연마제(10)가 손톱을 다른쪽 보다 깊이 연마하는 것을 방지하게 된다.At this time, since the board 4 is made of epoxy resin or waste resin, the beauty strip 2 absorbs and offsets the pressure force transmitted while being elastically bent, so that the abrasive 10 is more effective than the other nail. Deep grinding is prevented.

상기와 같이 손톱을 연마하는 작업을 종료한 후에 미용줄판(2)에 가한 외력을 제거하면, 휘어진 미용줄판(2)은 탄력적으로 본래 위치로 복귀하여 최초 형태를 유지하게 된다.If the external force applied to the beauty file board 2 is removed after finishing the polishing of the nail as described above, the curved beauty file board 2 is elastically returned to its original position to maintain the initial shape.

상기와 같이 사용되는 미용줄판(2)의 제조공정을 도 3 에서 설명하면 다음과 같다.The manufacturing process of the cosmetic strip 2 used as described above is described in Figure 3 as follows.

먼저 제조공정은 크게 부착단계 → 에칭단계 → 도포단계 → 성형단계로 이루어진다.First, the manufacturing process is largely composed of an attachment step → an etching step → an application step → a molding step.

상기 부착단계는 (a)에 도시된 바와 같이 소정 크기로 절단된 보오드(4)를 가이드롤러(12)를 통하여 이동시켜 가압장치(14)에 도달시키면, 상기 가압장치(14)를 구성하는 가압롤러(18)는 미도시된 공급롤러로로부터 보내어지는 플레이트(6)를 당겨 상기 보오드(4) 전면에 밀착시키게 되고, 동시에 가압롤러(18)는 열프레스기의 고주파가열장치(20)로부터 제공되는 열을 전달하게 된다.In the attaching step, when the board 4 cut to a predetermined size is moved through the guide roller 12 to reach the pressurizing device 14 as shown in (a), the pressurizing device 14 is pressurized. The roller 18 pulls the plate 6 sent from the feed roller not shown to closely contact the front surface of the board 4, and at the same time, the pressure roller 18 is provided from the high frequency heating device 20 of the heat press. Heat transfer.

따라서 상기 플레이트(6)는 가압롤러(18)에 의해 가압되면서 보오드(4) 전면에 밀착하게 되는데, 이때 상기 고주파가열장치(20)로부터 절달되는 열에 의해 상기 플레이트(6)는 보오드(4) 전면에 밀착된다.Therefore, the plate 6 is pressed by the pressure roller 18 to be in close contact with the front surface of the board 4, wherein the plate 6 by the heat delivered from the high-frequency heating device 20 is the front of the board 4 Close to

상기와 같이 가압단계가 종료되면 2-3시간 정도 냉각시킨 후 미 도시된 절단장치가 상기 보오드(4)의 길이에 맞게 플레이트(6)를 절단하므로써, 상기 보오드(4)와 플레이트(6)의 크기가 상호 동일하게 한다.When the pressurization step is completed as described above, after cooling for 2-3 hours, the cutting device not shown cuts the plate 6 in accordance with the length of the board 4 so that the board 4 and the plate 6 may be cut. Make the size the same.

계속하여 상기 부착단계 이후로 (b)에 도시된 에칭단계에 도달하면, 상기 플레이트(6) 전면에 약물(22)을 처리하여 도안하고자 하는 무늬(8)를 형성시킨다.Subsequently, when the etching step shown in (b) is reached after the attaching step, the drug 22 is processed on the entire surface of the plate 6 to form a pattern 8 to be designed.

상기 에칭단계 이후로 (c)에 도시된 도포단계에 도달하면 별도로 구비된 분사장치(24)를 통하여 연마제(10)를 니켈과 함께 플레이트(6) 전면에 걸쳐 분사시키게 되는데, 이때 에칭작업에 의해 형성된 무늬(8)로 상기 연마제(10) 일부가 유입되고, 일부는 상기 플레이트(6) 전면에 골고루 도포된다.After the etching step, when the coating step shown in (c) is reached, the abrasive 10 is sprayed over the entire surface of the plate 6 together with nickel through an injection device 24 provided separately. A part of the abrasive 10 is introduced into the formed pattern 8, and a part of the abrasive 10 is evenly applied to the entire surface of the plate 6.

상기와 같이 도포작업이 완료되면 연마제(10)의 접착력을 강화하기 위해 2차로 니켈 또는 크롬등으로 도금을 실시한다.When the coating operation is completed as described above, in order to reinforce the adhesive strength of the abrasive 10, the plating is performed with nickel or chromium.

상기 도포단계 이후로 (d)에 도시된 성형단계에 도달하게 되면, 별도로 구비된 프레스(26)가 작동하면서 플레이트(6)와 보오드(4)를 절단하므로써 (e)에 도시된 바와 같이 일정한 형태를 유지하고 있는 미용줄판(2)을 완성하게 된다.When the forming step shown in (d) is reached after the coating step, the plate 26 and the board 4 are cut while the press 26 provided separately operates to form a certain shape as shown in (e). Will complete the beauty line 2 holding.

본 발명은 미용줄판을 에폭시수지 또는 폐놀수지와 금속판등의 재질로 된 미용줄판을 구성하므로써, 부주의로 미용줄판을 취급하더라도 연마기능을 소원하게 유지할 수 있는 효과가 있다.The present invention has the effect of maintaining the polishing function can be desired even if the careless careless careless careless careless careless careless careless careless careless careless careless careless careless care about the beauty care boards by constructing a beauty care board made of a material such as epoxy resin or waste paper and metal plate.

다른 효과로는 미용줄판이 플렉시블한 기능을 가지므로, 작용력이 손톱에 완만하게 전달되어 안정적인 연마를 실현할 수 있는 장점이 있다.As another effect, since the beauty line has a flexible function, the action force is gently transmitted to the nail, thereby providing a stable polishing.

Claims (6)

보오드(4)상에 플레이트(6)를 위치 시킨 후 가압로울러(18)로 가압하여 일체화시키는 부착단계와,An attachment step of positioning the plate 6 on the board 4 and then integrating the plate 6 by pressing with a pressure roller 18; 상기 부착단계 이후로 플레이트(6) 표면에 약물(22)로 부식시켜 무늬(8)를 형성시키는 에칭단계와,An etching step of forming a pattern 8 by etching the drug 22 on the surface of the plate 6 after the attaching step; 상기 에칭단계 이후로 연마제(10)를 플레이트(6)상에 분사장치(24)로 분사하여 정착시키는 도포단계와,An application step of spraying and fixing the abrasive 10 on the plate 6 by the injection device 24 after the etching step; 상기 도포단계 이후로 완제품인 미용줄판(2)을 만드는 성형단계로 이루어짐을 특징으로 한 손톱연마용 줄 제조방법.Nail polishing line manufacturing method characterized in that it consists of a molding step to make a finished cosmetic line 2 after the coating step. 제 1 항에 있어서,The method of claim 1, 상기 보오드(4)상에 부착되는 플레이트(6)는 고주파가열에 의해 고정됨을 특징으로 한 손톱연마용 줄 제조방법.Plate (6) attached to the board (4) is a method for manufacturing a nail polishing line, characterized in that fixed by high frequency heating. 제 2 항에 있어서,The method of claim 2, 상기 미용줄판(2)은 보오드(4)와, 상기 보오드(4) 전면에 부착되어 고정되는 플레이트(6)와, 상기 플레이트(6) 전면에 도포되는 연마제(10)로 구성됨을 특징으로 한 손톱연마용 줄 제조방법.The beauty stripe board 2 comprises a board 4, a plate 6 attached to and fixed to the front surface of the board 4, and a nail 10, characterized in that the abrasive 10 is applied to the front surface of the plate 6. How to make a file for polishing. 제 3 항에 있어서,The method of claim 3, wherein 상기 플레이트(6) 전면에 무늬(8)가 그루브 타입으로 형성됨을 특징으로 한 손톱연마용 줄 제조방법.Method for producing a nail polishing line, characterized in that the pattern (8) is formed in the groove type on the front of the plate (6). 제 1 항 내지 제 4 항 중 어느 한 항에 있어서,The method according to any one of claims 1 to 4, 상기 보오드(4)는 에폭시수지 또는 폐놀수지 중 어느 하나로 이루어짐을 특징으로 한 손톱연마용 줄 제조방법.The board (4) is a method for producing a nail polishing line, characterized in that made of any one of an epoxy resin or a waste glow resin. 제 1 항 내지 제 4 항 중 어느 한 항에 있어서,The method according to any one of claims 1 to 4, 상기 플레이트(6)는 금속으로 이루어짐을 특징으로 한 손톱연마용 줄 제조방법.The plate (6) is a method for manufacturing a nail file, characterized in that made of metal.
KR1020010049344A 2001-08-16 2001-08-16 manufacturing process for a file for a nail grinder KR20030015558A (en)