KR100886760B1 - Screw strengthening coil manufacture device - Google Patents

Screw strengthening coil manufacture device Download PDF

Info

Publication number
KR100886760B1
KR100886760B1 KR1020070046197A KR20070046197A KR100886760B1 KR 100886760 B1 KR100886760 B1 KR 100886760B1 KR 1020070046197 A KR1020070046197 A KR 1020070046197A KR 20070046197 A KR20070046197 A KR 20070046197A KR 100886760 B1 KR100886760 B1 KR 100886760B1
Authority
KR
South Korea
Prior art keywords
winding shaft
screw
reinforcing coil
coil
female thread
Prior art date
Application number
KR1020070046197A
Other languages
Korean (ko)
Other versions
KR20080100081A (en
Inventor
이재익
Original Assignee
이재익
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 이재익 filed Critical 이재익
Priority to KR1020070046197A priority Critical patent/KR100886760B1/en
Publication of KR20080100081A publication Critical patent/KR20080100081A/en
Application granted granted Critical
Publication of KR100886760B1 publication Critical patent/KR100886760B1/en

Abstract

본 발명은 나사구멍이 형성되는 모재가 수나사에 비하여 무른 재질일 경우에, 수나사를 체결하기에 앞서 나사구멍에 먼저 체결한 다음 수나사를 체결토록 함으로써 나사구멍이 보강되도록 하는 암나사 강화코일 제조장치에 관한 것이다.The present invention relates to a female screw reinforcing coil manufacturing apparatus for reinforcing a screw hole by fastening the screw hole first and then tightening the male screw before the male screw is formed of a softer material than the male screw. will be.

상하의 롤러(11)(11')에 의해 소재(2)를 압송하는 공급부(10)와, 본체(1)의 중앙에 설치되고 외면에는 제조할 암나사 강화코일(3)과 같은 피치를 갖는 나사홈(21)을 형성하며, 선단부 끝단면 중앙에는 소재(2)의 끝을 걸어 회전시키도록 걸림홈(22)이 형성하되 걸림홈(22)은 회전방향을 기준으로 일측방향으로는 완만한 경사면(22')을 형성하고, 반대 방향으로는 회전시 소재(2)가 걸려 회전할 수 있도록 '∧'형 및 '∨'형의 걸림부(22")를 형성한 권회축(20)과, 권회축(20)을 중심으로 소재(2)가 진입하는 쪽의 반대쪽에 구성되어 권회축(20)에 밀착되었다가 이격되는 동작을 하는 스톱퍼(30)와, 권회축(20)의 상부에 구성되어 블럭(41)이 하강하여 암나사 강화코일(3)을 눌러주는 압박부(40)와, 권회축(20)에 근접하여 전후진 하는 절단날(60)로 구성됨을 특징으로 한다. A feed groove 10 for pressurizing the raw material 2 by the upper and lower rollers 11 and 11 ', and a screw groove provided at the center of the main body 1 and having the same pitch on the outer surface as the female thread reinforcing coil 3 to be manufactured. (21) is formed, the locking groove 22 is formed so as to rotate the end of the material (2) in the center of the tip end surface, the locking groove 22 is a gentle inclined surface in one direction relative to the rotation direction ( 22 '), and the winding shaft 20, which forms the locking portion 22 " of the' ∧ 'type and the' ∨ 'type so that the material 2 can be caught and rotated in the opposite direction. The stopper 30 and the upper part of the winding shaft 20 are configured on the opposite side of the rotational shaft 20 on the opposite side to the entry of the raw material 20 to be in close contact with the winding shaft 20 and spaced apart from each other. The block 41 is lowered, characterized in that it is composed of a pressing portion 40 for pressing the female thread reinforcing coil (3), and a cutting blade (60) to move forward and backward close to the winding shaft (20).

스크링코일, 암나사 보강, 강화코일, 스프링, 권회축 Spring coil, internal thread reinforcement, reinforcing coil, spring, winding shaft

Description

암나사 강화코일 제조장치{screw strengthening coil manufacture device}Female tightening coil manufacture device

도 1은 본 발명에 의한 제조장치의 전체 구성 정면도1 is an overall configuration front view of a manufacturing apparatus according to the present invention

도 2는 본 발명에 의한 제조장치의 요부 작용상태 상세도Figure 2 is a detailed view of the main action state of the manufacturing apparatus according to the present invention

도 3은 본 발명에 의한 권회축 및 암나사 강화코일의 사시도 3 is a perspective view of a winding shaft and a female thread reinforcing coil according to the present invention.

도 4는 본 발명에 의한 권회축의 측면도4 is a side view of the winding shaft according to the present invention;

도 5는 도 1의 권회축 부분을 도시한 평단면도
도 6은 본 발명에 의한 절단홈 가공부의 작용 상태도
5 is a plan sectional view showing the winding shaft portion of FIG.
6 is an operation state diagram of the cutting groove processing unit according to the present invention

***도면의 주요 부분에 대한 부호의 설명****** Description of the symbols for the main parts of the drawings ***

1: 본체 2: 소재1: body 2: material

3: 암나사 강화코일 3': 절단홈3: Female thread reinforcing coil 3 ': Cutting groove

4: 절곡부4: bend

10: 공급부 11, 11': 롤러10: supply part 11, 11 ': roller

20: 권회축 21: 나사홈20: winding shaft 21: screw groove

22: 걸림홈 22': 경사면22: engaging groove 22 ': slope

22": 걸림부 23: 요부22 ": Hanging part 23: main part

30: 스톱퍼30: stopper

40: 압박부 41: 블럭40: pressure part 41: block

50: 절단홈 가공부 51: 지지관체50: cutting groove processing part 51: support tube

52: 회전날52: rotary blade

60; 절단날60; Cutting blade

본 발명은 나사구멍이 형성되는 모재가 수나사(또는 볼트)에 비하여 무른 재질일 경우에, 수나사를 체결하기에 앞서 나사구멍에 먼저 체결한 다음 수나사를 체결토록 함으로써 나사구멍이 보강되도록 하는 암나사 강화코일 제조장치에 관한 것이다.According to the present invention, when the base material on which the screw hole is formed is a softer material than the male screw (or bolt), the female screw reinforcing coil for reinforcing the screw hole by tightening the male screw first and then tightening the male screw prior to tightening the male screw. It relates to a manufacturing apparatus.

주지된 바와 같이 수나사가 체결되도록 나사구멍이 형성되는 모재가 경합금, 다이케스터, 주철, 플라스틱, 목재 등과 같이 수나사에 비하여 무른 재질로 구성되는 경우에, 수나사의 강한 토크(Torque)에 잘 견디지 못하였던 것이며, 이러한 문제로 인하여 나사구멍이 마모되거나 헐거워지고 따라서 많은 기계적 고장의 원인이 되었던 것이다. As is well known, when the base material in which the screw hole is formed to fasten the male screw is made of a material that is softer than the male screw such as light alloy, die caster, cast iron, plastic, wood, etc., it did not endure the strong torque of the male screw well. This problem causes the screw holes to wear out or loosen, thus causing many mechanical failures.

이러한 문제점을 해결하기 위하여 최근에는 나사구멍을 수나사의 크기보다 더 크게 형성하고, 여기에 먼저 나사구멍에 체결되도록 나사형이면서 마름모꼴 단면을 가진 암나사 강화코일(나사부쉬의 한 종류로서 일명 '스크링코일'이라고 함)을 체결한 후, 다시 수나사를 체결하는 방식이 사용되고 있다. In order to solve this problem, in recent years, a screw hole is formed larger than the size of a male screw, and a female thread reinforcing coil having a rhombic cross-section and a threaded shape to be fastened to the screw hole first (a type of screw bush, also known as a screw coil). And then tighten the male screw again.

이와 같은 암나사 강화코일은 종래 일반적인 코일스프링을 제조하는 장치를 이용하여 제조하였던 바, 암나사 강화코일은 소재의 단면이 마름모꼴이라는 것과 나사구멍에 체결하기 위해 끝단부에 중심을 가로지르는 절곡부를 구성하여야 한다는 것 등의 구조적인 특징을 감안하여 제조하지 못하였으므로 생산능률이 저조하고 효율적이지 못하여 생산비용이 불필요하게 상승되는 문제가 있었다. Such female thread reinforcing coils have been manufactured using a conventional coil spring manufacturing apparatus. Female thread reinforcing coils have a rhombic cross section of a material, and a bent portion that crosses the center of the end portion to be fastened to the screw hole should be formed. In consideration of the structural features such as the thing did not manufacture because there is a problem that the production cost is unnecessarily increased because the production efficiency is low.

본 발명은 상기한 문제점을 감안하여 안출한 것으로서, 일측에서 진입하는 소재를 걸어 절곡부를 형성함과 동시에 스프링 형으로 감아주는 장치와, 이와 연동하면서 절곡부 제거를 위한 홈을 형성하는 장치 및 완전한 권회가 이루어진 후 절단하는 장치 등으로 구성되어 매우 효율적이고 능률적으로 암나사 강화코일을 제조할 수 있는 장치의 제공을 목적으로 하는 것이다. The present invention has been made in view of the above-mentioned problems, the device to form a bent portion by hooking the material entering from one side, and at the same time, the device to form a groove for removing the bent portion while interlocking with the device and the complete winding It is intended to provide a device capable of manufacturing a female thread reinforcing coil very efficiently and efficiently consists of a device for cutting after the made.

본 발명의 제조장치는 소재를 적절한 타이밍 간격으로 밀어주는 공급부와, 절곡부를 형성함과 동시에 스프링 형으로 권회하는 권회축과, 절곡부에 절단홈을 형성하는 장치와 절단 및 완료 후 분리를 위한 압박부 및 절단날로 이루어짐을 특징으로 하는바, 이하 첨부된 도면에 의거 본 발명의 바람직한 구성 실시 예를 상세히 살펴보면 다음과 같다.The manufacturing apparatus of the present invention, the supply unit for pushing the material at appropriate timing intervals, the winding shaft to form a bent portion and at the same time the spring-shaped winding, the apparatus for forming a cutting groove in the bent portion and the pressing for separation after cutting and completion Bar and cutting blade is characterized in that, according to the accompanying drawings, a preferred embodiment of the present invention in detail as follows.

도 1은 본 발명에 의한 제조장치의 전체 구성 정면도, 1 is an overall configuration front view of a manufacturing apparatus according to the present invention;

도 2는 본 발명에 의한 제조장치의 요부 작용상태 상세도, Figure 2 is a detailed view of the main action state of the manufacturing apparatus according to the present invention,

도 3은 본 발명에 의한 권회축 및 암나사 강화코일의 사시도, 3 is a perspective view of a winding shaft and a female thread reinforcing coil according to the present invention;

도 4는 본 발명에 의한 권회축의 측면도,4 is a side view of the winding shaft according to the present invention;

도 5는 도 1의 권회축 부분을 도시한 평단면도이다.FIG. 5 is a plan sectional view showing the winding shaft portion of FIG. 1. FIG.

본 발명의 제조장치는 먼저 일측에서 상하의 롤러(11)(11')에 의해 소재(2)를 압송하는 공급부(10)가 구성된다. In the manufacturing apparatus of the present invention, first, the supply unit 10 for feeding the material 2 by the upper and lower rollers 11 and 11 'is configured on one side.

본체(1)의 중앙에 권회축(20)의 선단이 돌출되도록 설치되는데, 권회축(20)의 외면에는 제조할 암나사 강화코일(3)과 같은 피치를 갖는 나사홈(21)을 형성하였으며, 선단부 끝단면 중앙에는 소재(2)의 끝을 걸어 회전시키도록 걸림홈(22)이 형성되는데, 상기 걸림홈(22)은 회전방향을 기준으로 일측방향으로는 완만한 경사면(22')을 형성하고 반대 방향으로는 회전시 소재(2)가 걸려 회전할 수 있도록 '∧'형 및 '∨'형의 걸림부(22")를 형성한 것이다. The front end of the winding shaft 20 is installed to protrude in the center of the main body 1, the outer surface of the winding shaft 20 was formed with a screw groove 21 having the same pitch as the female thread reinforcing coil (3) to be manufactured, A locking groove 22 is formed at the center of the tip end surface to rotate the end of the material 2, and the locking groove 22 forms a gentle inclined surface 22 'in one direction based on the rotation direction. And in the opposite direction to form the '22' and '∨' type locking portion 22 "so that the material (2) is rotated when rotating.

또 상기 걸림부의(22") 중간 일측에는 절단홈(3')을 형성시 장애를 받지 않도록 하는 요부(23)를 갖는다.In addition, the middle portion of the engaging portion 22 "has a recess 23 to prevent the obstacle when forming the cutting groove (3 ').

상기 권회축(20)은 정회전을 하면서 외면의 피치 간격만큼 서서히 전진을 하고, 역회전시에는 후진하도록 구성하였다.The winding shaft 20 was configured to slowly move forward by the pitch interval of the outer surface while performing the forward rotation, and to reverse in the reverse rotation.

그리고 권회축(20)을 중심으로 소재(2)가 진입하는 쪽의 반대쪽에는 전후진을 반복하면서 권회축(20)에 밀착되었다가 이격되는 동작을 하는 스톱퍼(30)를 구성하였는데, 소재(2)가 진입할 때 스톱퍼(30)가 전진하여 권회축(20)에 밀착한 상태를 유지하므로 소재(2)의 과도한 진입을 제한하여 정지시키는 역할을 하고 그러한 기능이 완료되면 후진하여 다음의 진입을 기다리는 것이다.And on the opposite side of the winding shaft 20 to enter the material (2) on the opposite side while repeating the forward and backward while the close contact with the winding shaft (20) constituted a stopper (30) to operate the spaced apart, When the stop enters the stopper 30 advances and maintains the state in close contact with the winding shaft 20 serves to limit the excessive entry of the material (2) to stop, and when such a function is completed, the reverse to the next entry I'm waiting.

권회축(20)의 상부에는 압박부(40)가 구성되는데, 필요한 만큼 감기가 이루어진 다음 블럭(41)이 하강하여 권회된 암나사 강화코일(3)을 누른 상태에서 권회 가 끝나는 부분을 절단하게 되는 것이며, 또한 절단이 완료된 후, 블럭(41)이 암나사 강화코일(3)을 눌러 회전하지 않도록 한 상태에서 권회축(20)을 역회전시키면 권회축(20)이 후진을 하면서 암나사 강화코일(3)과 분리 되도록 한다. The upper portion of the winding shaft 20 is configured with a pressing portion 40, the winding is made as necessary, then the block 41 is lowered to cut the end portion of the winding while pressing the wound female thread reinforcing coil (3) Also, after cutting is completed, if the block 41 reversely rotates the winding shaft 20 in a state in which the block 41 does not rotate by pressing the female thread reinforcing coil 3, the winding shaft 20 moves backward while the female thread reinforcing coil 3 Separate from).

그리고 본체(1)의 일측에는 절단홈 가공부(50)가 구성되는데, 회동하는 지지관체(51)의 끝단에 회전날(52)을 형성하여 도 6과 같이 지지관체(51)가 권회축(20)의 중심 방향으로 회동하면 회전날(52)이 암나사 강화코일(3)에 절단홈(3')을 형성하는 것이다.And one side of the main body 1 is formed with a cutting groove processing unit 50, by forming a rotary blade 52 at the end of the rotating support pipe 51, as shown in Figure 6 the support pipe 51 is the winding shaft ( When rotating in the direction of the center of 20, the rotary blade 52 is to form a cutting groove (3 ') in the female thread reinforcing coil (3).

또한 권회축(20)에 근접하여 전후진 하는 절단날(60)를 구성하는데 권회축(20)이 권회를 완료한 상태에서 절단날(60)이 전진하여 권회가 완료된 암나사 강화코일(3)의 끝부분을 절단하는 것이다.In addition, to form a cutting blade 60 to move forward and backward close to the winding shaft (20) of the female thread reinforcing coil (3) of the winding is completed by the cutting blade 60 is advanced in the state that the winding shaft (20) completed the winding. To cut the tip.

도면 중 미설명된 부호 5는 배출가이드, 6은 실린더, 7은 캠장치이다.In the drawings, reference numeral 5 denotes a discharge guide, 6 a cylinder, and 7 a cam device.

이러한 구성으로 된 본 발명의 작용을 순서에 따라 상세히 살펴보면 다음과 같다. Looking at the operation of the present invention having such a configuration in detail as follows.

먼저 공급부(10)의 롤러(11)(11') 의해 소재가 공급되는데, 권회축(20)의 걸림홈(22)까지 진입이 이루어지면서 스톱퍼(30)에 닿게 되면 공급이 중단되고 권회축(20)이 한바퀴 회전하면서 절곡부(4)를 형성하는데, 권회축(20)의 걸림홈(22)에 소재(2)가 삽입된 상태에서 회전을 하면 걸림홈(22)의 걸림부(22")에 소재()가 걸려 회전하므로 절곡부(4)가 형성되는 것이다.First, the material is supplied by the rollers 11 and 11 ′ of the supply unit 10. When the material reaches the stopper 30 while entering the locking groove 22 of the winding shaft 20, the supply is stopped and the winding shaft ( 20 rotates one turn to form the bent portion 4, and when the material 2 is rotated in the state of being inserted into the locking groove 22 of the winding shaft 20, the locking portion 22 "of the locking groove 22 is rotated. The material () is caught and rotated so that the bent portion 4 is formed.

권회축(20)이 한바퀴를 회전한 후에 스톱퍼(30)가 후진하여 원위치로 복귀하고, 공급부(10)는 소재(2)를 자유상태로 놓아주는 것이며, 이후 권회축(20)은 2-3 바퀴를 더 회전한 다음에 일단 정지하게 된다. After the winding shaft 20 rotates one turn, the stopper 30 retracts and returns to its original position, the supply unit 10 releases the material 2 in a free state, and the winding shaft 20 then rotates 2-3. After turning the wheel further, it stops once.

이때 절단홈 가공부(50)가 작용하는데, 도 6과 같이 지지관체(51)가 권회축(20) 방향으로 일정각도 회동하면, 회전날(52)이 암나사 강화코일(3)의 절곡부(4)가 형성된 좀 뒤 원형으로 권회가 시작되는 부분에 절단홈(3')을 형성하는 것이며, 계속하여 권회축(20)은 필요한 만큼 회전하여 암나사 강화코일(3)의 권회를 완성하게 되는 것이다.At this time, the cutting groove processing unit 50 acts, as shown in Figure 6, when the support tube 51 is rotated at a predetermined angle in the direction of the winding axis 20, the rotary blade 52 is the bent portion of the female screw reinforcing coil ( 4) is formed to form a cutting groove (3 ') at the beginning of the winding in a circular shape a little later, the winding shaft 20 is rotated as necessary to complete the winding of the female screw reinforcing coil (3). .

완성 후에는 압박부(40)가 하강하여 감겨진 암나사 강화코일(3)의 외면을 눌러준 상태에서 절단날(60)이 전진하여 소재(2)의 감기지 아니한 부분을 절단하여 완성한다.After completion, the cutting unit 60 is advanced by pressing the outer surface of the female thread reinforcing coil (3) wound down by the pressing unit 40 is completed by cutting the unwinding portion of the material (2).

절단 완료 후에는 압박부(40)가 누르고 있는 상태에서 권회축(20)이 역회전하여 완성된 암나사 강화코일(3)과 분리되는 것이고, 분리된 암나사 강화코일(3)은 아래로 낙하하여 수거된다. After the cutting is completed, the winding shaft 20 is reversely rotated and separated from the completed female thread reinforcing coil 3 while the pressing part 40 is pressed, and the separated female thread reinforcing coil 3 falls down and is collected. do.

이상 설명한 바와 같은 본 발명에 의하면, 전체적으로 자동화가 이루어지므로 암나사 강화코일을 효율적으로 생산할 수 있게 되는 것이며, 특히 암나사 강화코일의 절곡부까지 한 번의 공정으로 형성할 수 있게 되는 것으로, 암나사 강화코일의 생산능률을 크게 향상시키고 균일한 품질과 저렴한 가격으로 암나사 강화코일을 제공할 수 있게 해주는 유용한 발명인 것이다. According to the present invention as described above, it is possible to produce the female screw reinforcement coil efficiently because the automation is performed as a whole, in particular, to be able to form the bent portion of the female screw reinforcement coil, production of the female screw reinforcement coil It is a useful invention that can significantly improve efficiency and provide female thread reinforcing coils with uniform quality and low price.

Claims (1)

상하의 롤러(11)(11')에 의해 소재(2)를 압송하는 공급부(10)와;A supply section 10 for feeding the raw material 2 by the upper and lower rollers 11 and 11 '; 본체(1)의 중앙에 설치되고 외면에는 제조할 암나사 강화코일(3)과 같은 피치를 갖는 나사홈(21)을 형성하며, 선단부 끝단면 중앙에는 소재(2)의 끝을 걸어 회전시키도록 걸림홈(22)이 형성하되 걸림홈(22)은 회전방향을 기준으로 일측방향으로는 완만한 경사면(22')을 형성하고, 반대 방향으로는 회전시 소재(2)가 걸려 회전할 수 있도록 '∧'형 및 '∨'형의 걸림부(22")를 형성한 권회축(20)과;It is installed at the center of the main body 1 and forms a screw groove 21 having the same pitch as the female thread reinforcing coil 3 to be manufactured on the outer surface, and is hooked to rotate by walking the end of the material 2 in the center of the distal end surface. The groove 22 is formed, but the locking groove 22 forms a gentle inclined surface 22 'in one direction based on the rotation direction, and in the opposite direction, the material 2 can be caught and rotated in the opposite direction. A winding shaft 20 having a locking portion 22 " 권회축(20)을 중심으로 소재(2)가 진입하는 쪽의 반대쪽에 구성되어 권회축(20)에 밀착되었다가 이격되는 동작을 하는 스톱퍼(30)와;A stopper 30 configured to be opposite to the side on which the material 2 enters around the winding shaft 20 to be in close contact with the winding shaft 20 and spaced apart from each other; 권회축(20)의 상부에 구성되어 블럭(41)이 하강하여 암나사 강화코일(3)을 눌러주는 압박부(40)와; Compression portion 40 is configured on the winding shaft 20, the block 41 is lowered to press the female screw reinforcing coil (3); 권회축(20)에 근접하여 전후진 하는 절단날(60);A cutting blade 60 moving forward and backward close to the winding shaft 20; 로 구성됨을 특징으로 하는 암나사 강화코일 제조장치.Female thread reinforcing coil manufacturing apparatus, characterized in that consisting of.
KR1020070046197A 2007-05-11 2007-05-11 Screw strengthening coil manufacture device KR100886760B1 (en)