KR100604950B1 - Method for manufacturing non-woven fabric bag - Google Patents

Method for manufacturing non-woven fabric bag Download PDF

Info

Publication number
KR100604950B1
KR100604950B1 KR1020050002139A KR20050002139A KR100604950B1 KR 100604950 B1 KR100604950 B1 KR 100604950B1 KR 1020050002139 A KR1020050002139 A KR 1020050002139A KR 20050002139 A KR20050002139 A KR 20050002139A KR 100604950 B1 KR100604950 B1 KR 100604950B1
Authority
KR
South Korea
Prior art keywords
nonwoven fabric
buffer roller
instantaneous heating
heating heater
heater wire
Prior art date
Application number
KR1020050002139A
Other languages
Korean (ko)
Other versions
KR20060081748A (en
Inventor
금용수
Original Assignee
금용수
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 금용수 filed Critical 금용수
Priority to KR1020050002139A priority Critical patent/KR100604950B1/en
Publication of KR20060081748A publication Critical patent/KR20060081748A/en
Application granted granted Critical
Publication of KR100604950B1 publication Critical patent/KR100604950B1/en

Abstract

본 발명의 부직포는 섬유조직을 갖고 있기 때문에 완성된 제품은 공기의 통풍성이 높아 세계적으로 문제화 되고 있는 아이들의 장난으로 뒤집어 쓰므로 질식사할 수 있는 사례를 발생시키지 않아 위험하지 않은 부직포 봉투의 제조방법으로, 부직포(10)를 반접기 한후에 연속적으로 송출롤러(12a),(12b)를 통해 이동시키는 단계와, 길이방향으로 순간가열히터선(22)이 절연판(21)에 고정된 압착부(20) 및 압착부(20)의 하부측에 일정간격을 두고 형성된 완충롤러(30)에 반접기된 부직포(10)를 정지시키는 단계와,완충롤러(30)상에 반접기된 부직포(10)가 얹혀지게 이동된 후, 부직포의 끝단은 이송롤러(36a),(36b)에 물려 고정되고 완충롤러(30)를 상부측에 형성된 압착부(20)측으로 상승시키는 단계와, 압착부(20)의 순간가열히터선(22)이 하강되면서 400℃∼800℃까지 순간 가열 압착시킴과 동시에 부직포(10)가 공급되는 수평선상까지 완충롤러(30)를 하강시켜 부직포(10)를 절단,융착시키는 단계와, 압착부(20)의 순간가열히터선(22)에 의해 절단된 부직포(10)의 융착 부위가 완전하게 부착되도록 자연냉각되는 단계로 구성된 특징이 있다.Since the nonwoven fabric of the present invention has a fibrous structure, the finished product is used in children's pranks, which are highly problematic in the world because of high air ventilation, so that it does not cause cases of suffocation, and thus is a method for producing a non-woven fabric that is not dangerous. After the non-woven fabric 10 is folded, the step of continuously moving the feed rollers 12a and 12b and the crimping unit 20 in which the instantaneous heating heater wire 22 is fixed to the insulating plate 21 in the longitudinal direction. And stopping the nonwoven fabric 10 folded on the buffer roller 30 formed at a predetermined interval on the lower side of the crimping portion 20, and the nonwoven fabric 10 folded on the buffer roller 30 is placed thereon. After the fork is moved, the end of the nonwoven fabric is bitten by the feed rollers 36a and 36b, and the buffer roller 30 is raised to the side of the crimping portion 20 formed on the upper side. Instantly from 400 ° C to 800 ° C as the heating heater wire 22 descends Pressing and simultaneously cutting the nonwoven fabric 10 by lowering the buffer roller 30 to the horizontal line on which the nonwoven fabric 10 is supplied, and by the instantaneous heating heater wire 22 of the crimping unit 20. It is characterized in that the step of natural cooling so that the fusion site of the cut nonwoven fabric 10 is completely attached.

부직포, 완충롤러.Nonwovens, buffer rollers.

Description

부직포 봉투의 제조방법{METHOD FOR MANUFACTURING NON-WOVEN FABRIC BAG}Manufacturing method of nonwoven bag {METHOD FOR MANUFACTURING NON-WOVEN FABRIC BAG}

도 1 (a)∼(g)는 본 발명의 부직포 봉투의 제조방법의 공정단계를 나타내는 도면.1 (a) to (g) are diagrams showing the process steps of the method for producing a nonwoven fabric bag of the present invention.

-도면의 주요부분에 대한 설명-                 Description of the main parts of the drawing

10: 부직포 12a,12b: 송출롤러          10: nonwoven fabric 12a, 12b: feeding roller

20: 압착부 21: 절연판          20: crimping portion 21: insulating plate

22: 순간가열히터선 30: 완충롤러          22: instantaneous heating heater wire 30: buffer roller

본 발명은 부직포 봉투의 제조방법에 관한 것으로, 더욱 상세하게는 부직포는 섬유조직을 갖고 있기 때문에 완성된 제품은 공기의 통풍성이 높아 세계적으로 문제화되고 있는 아이들의 장난으로 뒤집어 쓰므로 질식사할 수 있는 사례를 발생시키지 않을 뿐만 아니라, 제조시에 접착제가 필요 없이 자동으로 접착시키면서 봉투를 만들 수 있는 부직포 봉투의 제조방법에 관한 것이다.The present invention relates to a method for manufacturing a nonwoven fabric bag, and more particularly, since the nonwoven fabric has a fibrous structure, the finished product has a high air permeability and is used as a joke of children, which is becoming a problem worldwide. Not only does not generate, but also relates to a method for producing a nonwoven bag that can be made while automatically bonding the bag without the need for adhesive during manufacture.

최근에 와서는 구매한 물건을 담을 수 있는 봉투로 종이 봉투, 비닐 봉투, 부직포 봉투 등을 사용해 오고 있으나 그중에 종이 봉투는 잘찢어지고 가격이 높은 문제점한 있에 최근에는 제조가 쉽고 가격이 저렴한 비닐 봉투 등을 많이 사용하고 있다.Recently, paper bags, plastic bags, and non-woven bags have been used as bags to store purchased items. Among them, paper bags are easily torn and expensive. I use a lot.

그러나, 봉투를 만들기 위해 테두리 부분을 서로 붙일시 초음파가열기에 의해 부착시키기 때문에 비닐이 서로 녹아 붙을시 유해물질이 배출되 환경오염을 발생시킬 뿐만 아니라, 특히 비닐 봉투는 얇고 잘찢어지는 문제점이 있다.However, when the edges are attached to each other to make an envelope by ultrasonic heaters, when the vinyl is melted together, harmful substances are discharged and environmental pollution is generated. In particular, plastic bags have a problem of being thin and easily torn. .

또한, 비닐 봉투는 소각시에 환경오염을 발생시킬 수 있어 환경오염차원에서 규제되가고 있는 실정이다.In addition, plastic bags can generate environmental pollution during incineration, which is regulated in terms of environmental pollution.

또한 최근에 사용되는 것으로 부직포 봉투는, 잘찢어지지 않는 특성과 공기의 통과성이 좋아 많이 최근에 많이 사용하고 있다.In addition, recently used nonwoven fabric bags have been frequently used in recent years because of their poor tearing properties and good air permeability.

부직포를 이용한 봉투는, 제조시에 테두리 부분을 실 등을 이용해 박음질처리를 하거나 초음파가열에 의해 부착시키고 있다.Envelopes made of nonwoven fabrics are stitched together using a thread or the like during the manufacture of the bag or attached by ultrasonic heating.

부직포를 실등으로 박음질해서 봉투를 만들시에는 인건비에 의한 제조단가 상승되므로 최근에는 가열부착에 의한 방법으로 초음파가열기를 이용하고 있다.When manufacturing a bag by stitching a nonwoven fabric into a thread and so on, the manufacturing cost is increased due to labor costs. Recently, ultrasonic heaters have been used as a method of heating and attaching.

상기 초음파가열기를 이용한 가열 부착방식은 지속적으로 열이 가해지는 이유때문에 부직포 면의 부착면에 가열기가 맞닿음될시에 지속되는 가열로 인해 부직포의 부착면이 쉽게 녹아 버리기 때문에 그 형태를 유지하기가 어렵다.The heating attachment method using the ultrasonic heater maintains its shape because the attachment surface of the nonwoven fabric is easily melted due to the heating that is continued when the heater is brought into contact with the attachment surface of the nonwoven fabric because of the continuous heating. Is difficult.

또한,초음파가열기는 많은 불량품을 양산하며 여러단계의 작업공정을 거쳐야 하기때문 때문에 제조단가가 상승하는 문제점을 안고 있다.In addition, the ultrasonic heater has a problem that the production cost increases because it is required to go through several stages of work process and mass production of many defective products.

따라서, 본 발명은 상기와 같은 종래의 문제점은 감안하여 창출된 것으로, 그 목적으로 부직포는 섬유조직을 갖고 있기 때문에 완성된 제품은 공기의 통풍성이 높아 세계적으로 문제화되고 있는 아이들이 장난으로 뒤집어 쓰므로 질식사할 수 있는 사례를 발생시키지 않을 뿐만 아니라, 제조시에 접착제가 필요 없어 자동으로 접착시킬 수 있는 부직포 봉투의 제조방법을 제공함에 있다.Therefore, the present invention has been created in view of the above-described conventional problems, and for this purpose, since the nonwoven fabric has a fibrous structure, the finished product has high air permeability, so that the children who are being troubled around the world use it as a mischief. Not only does not cause the case of suffocation, but also provides a method of manufacturing a non-woven bag that can be automatically glued because no adhesive is required at the time of manufacture.

상기와 같은 본 발명의 목적을 달성하기 위하여, 부직포 봉투의 제조방법은, 부직포를 반접기 한후에 연속적으로 공급시켜 주는 송출롤러를 통해 이동시키는 단계와, 길이방향으로 순간가열히터선이 절연판에 고정된 압착부 및 압착부의 하부측에 일정간격을 두고 형성된 완충롤러에 반접기된 부직포를 정지시키는 단계와, 완충롤러상에 반접기된 부직포가 얹혀지게 이동된 후, 부직포의 끝단은 이송롤러에 물려 고정되면 완충롤러를 상부측에 형성된 압착부측으로 상승시키는 단계와, 압착부의 순간가열히터선이 하강되면서 400℃∼800℃까지 순간 가열 압착시킴과 동시에 부직포가 공급되는 수평선상까지 완충롤러를 하강시켜 부직포를 절단,융착시키는 단계와, 압착부의 순간가열히터선에 의해 절단된 부직포의 융착 부위가 완전하게 부착되도록 자연냉각되는 단계로 구성된다.In order to achieve the object of the present invention as described above, the manufacturing method of the nonwoven fabric bag, the step of moving through the feed roller that is continuously supplied after the non-woven fabric folded, and the instantaneous heating heater wire in the longitudinal direction is fixed to the insulating plate Stopping the non-woven fabric folded on the cushioning roller formed at a predetermined distance on the lower side of the pressing portion and the pressing portion, and after the non-woven fabric folded on the buffer roller is placed on the buffer roller, the end of the nonwoven fabric is bitten by a feed roller. When the buffer roller is raised to the crimping part formed on the upper side, the instantaneous heating heater line of the crimping part is lowered, and instantaneous heat compression is performed at 400 ° C to 800 ° C, and the buffer roller is lowered to the horizontal line where the nonwoven fabric is supplied. Cutting and fusion, and the fusion site of the nonwoven fabric cut by the instantaneous heating heater wire of the crimping portion is completely attached. It consists of a cooling step that is open.

상기와 같이 구성된 본 발명의 부직포 봉투의 제조방법을 첨부된 도면을 참조하여 아래와 같이 구체적으로 설명한다.With reference to the accompanying drawings, a method for manufacturing a nonwoven bag of the present invention configured as described above will be described in detail as follows.

도 1 (a)∼(g)는, 본 발명의 부직포 봉투의 제조방법의 공정단계를 나타내는 도면이다.Fig.1 (a)-(g) is a figure which shows the process step of the manufacturing method of the nonwoven fabric bag of this invention.

본 발명은 도 1 (a)와 같이 연속으로 공급되는 부직포(10)를 부착하기 위해 점선으로 표시된 부분을 중심으로 도 1 (b)와 같이 반접기한다.In the present invention, to attach the nonwoven fabric 10 continuously supplied as shown in FIG.

상기와 같이 반접기된 부직포(10)는 서로 반접기된 면이 들뜨게 되어 있기 때문에 이를 방지하기 위해 밀착된 상태로 이동시키도록 도 1 (c)의 압착 이동롤러(12a),(12b)를 통해 압착하면서 이동시킨다.Since the semi-folded nonwoven fabric 10 is lifted up as described above, the rolled non-woven fabric 10 is moved through the pressing movement rollers 12a and 12b of FIG. Squeeze and move.

도 1 (c)의 이동롤러(12a),(12b)를 통해 이동되는 부직포(10)는 이동롤러(12a),(12b)의 회전에 의해 이동되어 도 1 (d)에 위치되어 있는 완충롤러(30)의 상부측에 얹혀지게 이동된후 정지된다.The nonwoven fabric 10 that is moved through the moving rollers 12a and 12b of FIG. 1 (c) is moved by the rotation of the moving rollers 12a and 12b and positioned in FIG. 1 (d). It is moved to rest on the upper side of 30 and then stopped.

완충롤러(30)상에 부직포(10)가 이동되어 정지되면, 완충롤러(30)상에 위치되어 있는 압축부(20)가 도 1 (e)와 같이 하강됨과 동시에 하부측의 완충롤러(30) 또한 약간 상승된다. 즉, 상기 압축부(20)의 순간가열히터선(22)이 하강하면서 겹쳐져 있는 부직포(10)를 가압할시 완충롤러(30)를 약간 상승시키므로 눌릴시 겹쳐져 있는 상하의 부직포(10)면이 서로 어긋나는 것을 방지할 수 있다.When the nonwoven fabric 10 is moved and stopped on the buffer roller 30, the compression unit 20 located on the buffer roller 30 is lowered as shown in FIG. 1 (e) and at the same time the buffer roller 30 on the lower side. ) Is also slightly elevated. That is, when the instantaneous heating heater wire 22 of the compression unit 20 is lowered, the buffer roller 30 is slightly raised when pressing the overlapping nonwoven fabric 10, so that the upper and lower surfaces of the nonwoven fabric 10 overlapped when pressed. The shift can be prevented.

이동롤러(12a),(12b)에 의해 이동된 부직포(10)의 끝단은 완충롤러(30)를 지나 이송롤러(36a),(36b)에 물린 상태로 정지되고, 이후에 접착,절단작업이 종료된후 부직포(10)를 이송시키도록 이송롤러(36a),(36b)를 회전된다.The end of the nonwoven fabric 10 moved by the moving rollers 12a and 12b is stopped while being bitten by the transfer rollers 36a and 36b after passing through the buffer roller 30, and then the bonding and cutting operations are performed. After the end, the feed rollers 36a and 36b are rotated to feed the nonwoven fabric 10.

이와같이 부직포(10)가 압축부(20)에 의해 완충롤러(30)측으로 하강되면서 눌려지면, 도 1 (f)와 같은 상태가 되도록 순간가열히터선(22)에 순간적으로 전압을 가했다 끊어주면 그 순간 융착열이 발생된다.When the nonwoven fabric 10 is pressed while being lowered to the buffer roller 30 by the compression unit 20 in this way, when the voltage is momentarily applied to the instantaneous heating heater line 22 so as to be in a state as shown in FIG. Instantaneous fusion heat is generated.

이때에 순간가열히터선(22)과 압축부(20)와의 사이에는 절연판(21)이 형성되어 있기 때문에 압축부(20)측으로 발생된 열이 전달되지 않고, 순간가열히터선(22) 에만 약 0.2∼0.4초동안 약 400∼800℃까지 순간적으로 열이 발생된다.At this time, since the insulating plate 21 is formed between the instantaneous heating heater wire 22 and the compression part 20, heat generated to the compression part 20 side is not transferred, and only the instantaneous heating wire 22 is weak. Heat is instantaneously generated to about 400 to 800 ° C. for 0.2 to 0.4 seconds.

압축부(20)의 하단측에 장착된 순간가열히터선(22)에 의해 부직포(10)는 완충롤러(30)측으로 눌려지면서 그 부위의 면이 도 1 (f)와 같이 잘려지면서 실링되면서 부착된다.The nonwoven fabric 10 is pressed to the buffer roller 30 by the instantaneous heating heater line 22 mounted on the lower end side of the compression unit 20 while the surface of the part is cut while being sealed as shown in FIG. 1 (f). do.

상기와 같이 본 발명의 온도범위내에서 정해진 시간내에 순간가열히터선(22)에 온도를 가해주었을 경우에는 원활하게 절단되면서 실링되는 반면에, 온도는 낮게 한경우에는 연속적으로 인입되는 부직포(10)가 제대로 끊어지지 않고 연이어져 나오게 되며, 온도범위를 주워진 온도 보다 높게 형성했을 경우에는 순간가열히터선(22)에 닿는 부직포(10)의 많은 면적의 부위가 녹아버리는 경우가 발생하기때문에 정해진 범위내에서 실시하는 것이 좋다.When the temperature is applied to the instantaneous heating heater wire 22 within a predetermined time within the temperature range of the present invention as described above is smoothly cut and sealed, while the temperature is low, the nonwoven fabric 10 is continuously drawn in. Is not broken properly, and if the temperature range is formed higher than the picked-up temperature, a large area of the nonwoven fabric 10 that contacts the instantaneous heating heater line 22 may melt, so that a predetermined range It is good to carry out within.

특히, 본 발명의 순간가열히터선(22)에 의해 눌려지면서 가열 절단되는 부직포(10)는 완충롤러(30)의 상단 정점 부위가 눌려짐과 동시에 부직포(10)의 잘려지는 양면이 융착되면서 실링되는 특징이 있다.In particular, the nonwoven fabric 10 that is pressed by the instantaneous heating heater wire 22 of the present invention is heat-cut and sealed while the upper end portion of the buffer roller 30 is pressed and the both sides of the nonwoven fabric 10 are fused. There is a characteristic.

압축부(20)의 순간가열히터선(22)에 가해진 전압은 눌려지면서 0.3초 공급후 순간 공급/차단되기때문에 부직포(10)는 녹아떨어진다.Since the voltage applied to the instantaneous heating heater wire 22 of the compression unit 20 is pressed and then instantaneously supplied / blocked after 0.3 seconds supply, the nonwoven fabric 10 melts.

이는 순간가열히터선(22)의 온도가 800℃까지 상승후 300℃까지 순간 높아졌다 떨어지기 때문에 부직포(10)의 융착되는 상하 면은 순간가열되면서 녹아 붙은 상태에서 높은 열은 지속적으로 발생되지 않고 0.5초동안 식으면서 굳어지기 때문에 쉽게 떨어지지 않는다. 즉, 순간가열히터선(22)에 의해 순간 고열이 발생되지만 전압을 가했다 바로 차단시켜주면 순간 발생된 온도가 빠르게 떨어지므로 부직포의 융착된 모서리부분은 계속해서 융착되지 않고 바로 굳어버리게 된다.This is because the temperature of the instantaneous heating heater wire 22 rises to 800 ° C and then rises to 300 ° C. Then, the fused upper and lower surfaces of the nonwoven fabric 10 are instantaneously heated, and the high heat is not generated continuously. It hardens as it cools for seconds, so it does not fall easily. That is, instantaneous high heat is generated by the instantaneous heating heater wire 22, but if the voltage is applied and then immediately blocked, the instantaneously generated temperature drops quickly, and thus the fused edge portion of the nonwoven fabric is immediately hardened without being fused.

따라서, 부직포(10)는 압축부(20)의 순간가열히터선(22)에 의해 완충롤러(30)로 눌려지기 때문에 부직포(10)의 눌려진 면은 순간적으로 녹아떨어지면서 상하 잘려진 부직포(10)의 모서리면이 서로 융착되면서 붙게 되므로 그 면이 일직선지면서 실링되는 특징이 있다.Therefore, since the nonwoven fabric 10 is pressed by the buffer roller 30 by the instantaneous heating heater wire 22 of the compression unit 20, the pressed surface of the nonwoven fabric 10 is melted down instantaneously, and the nonwoven fabric 10 is cut up and down. Since the edges of the surfaces are fused with each other, the surfaces are straight and sealed.

반대로, 순간가열히터선(22)에 순간적인 전압을 가하지 않고 지속적으로 전압을 가해 열을 지속적으로 발생시킬시에는 지속되는 열로 인해 맞닿음되는 부직포(10)의 맞닿는면을 더욱 많이 녹여버리기 때문에 일직선지게 융착되지 않은 상태로 녹아버리는 문제점으로 인해 잘 붙지 않고, 부착부위가 일직선지게 형성되지 않아 되도록이면 순간가열히터선(22)이 순간적으로 열이 가해졌다가 식게하는 것이 바람직하다.On the contrary, when continuously applying voltage to the instantaneous heating heater wire 22 without generating instantaneous voltage and continuously generating heat, the contact surface of the nonwoven fabric 10 which is brought into contact with each other due to the continuous heat melts more in a straight line. Due to the problem of melting in a non-fused state, it is preferable that the instantaneous heating heater line 22 is instantaneously heated and cooled, so that it does not stick well and the attachment part is not formed in a straight line.

순간가열히터선(22)에 의해 잘려지면서 융착된 부직포 봉투는 도 1 (g)와 같이 이송롤러(36a),(36b)를 통해 이동되어 롤러(33)를 따라 이동시켜 처리된다.The nonwoven bag cut and fused by the instantaneous heating heater line 22 is moved through the conveying rollers 36a and 36b as shown in FIG. 1 (g) and processed along the roller 33.

특히, 본 발명의 완충롤러(30)는 상부측에서 압축부(20)가 눌려질시에 완충될 뿐만 아니라, 열에 강할뿐만 아니라 완충성이 좋은 실리콘으로 형성되어 있어 상부측에서 압축부(20)의 순간가열히터선(22)이 완충롤러(30)상에서 눌려질시 눌려짐과 동시에 부직포만이 녹으면서 절단된다.In particular, the buffer roller 30 of the present invention is not only buffered when the compression unit 20 is pressed on the upper side, but also formed of silicon that is not only resistant to heat but also has good buffering properties. When the instantaneous heating heater wire 22 is pressed on the buffer roller 30, the instantaneous heating heater wire 22 is pressed while being cut while melting only the nonwoven fabric.

따라서, 상기와 같이 부직포 봉투의 제조방법에 의해 부직포를 자동으로 절단시키면 밀봉시킬 수 있어 공정의 단순화와 더불어 대량생산을 할 수 있는 효과가 있다.Therefore, if the nonwoven fabric is automatically cut by the manufacturing method of the nonwoven bag as described above, it can be sealed, thereby simplifying the process and producing mass production.

또한, 부직포는 섬유조직을 갖고 있기 때문에 완성된 제품은 무거운 제품을 넣어도 찢어지지 않을 뿐만 아니라, 공기의 통풍성이 높아 세계적으로 문제화되고 있는 아이들이 장난으로 뒤집어 써도 위험하지 않은 특징이 있다.In addition, since the nonwoven fabric has a fibrous structure, the finished product is not torn even when a heavy product is put into it, and there is a feature that is not dangerous even if children around the world have high air ventilation and use it as a prank.

본 발명의 부직포 봉투는 질기며 결방향이 없으로 다른 원단과 합성하지 않고도 제조가 가능하므로 순수하게 재생,재활용해서 사용할 수 있고 또한 경고문구의 인쇄가 필요없어 친환경적인 효과가 있다.
Since the nonwoven bag of the present invention is tough and has no grain direction, it can be manufactured without synthesis with other fabrics, so that it can be used purely recycled and recycled, and it does not require printing of warning phrases, thereby having an environmentally friendly effect.

Claims (3)

부직포 봉투의 제조방법에 있어서,In the manufacturing method of the nonwoven bag, 부직포(10)를 반접기 한후에 연속적으로 공급시켜 주는 송출롤러(12a),(12b)를 통해 이동시키는 단계와,Moving the nonwoven fabric 10 through the feeding rollers 12a and 12b which continuously supply the nonwoven fabric 10 after being folded, 길이방향으로 순간가열히터선(22)이 절연판(21)에 고정된 압착부(20) 및 압착부(20)의 하부측에 일정간격을 두고 형성된 완충롤러(30)에 반접기된 부직포(10)를 정지시키는 단계와,The non-woven fabric 10 folded by the instantaneous heating heater wire 22 fixed to the insulating plate 21 in the longitudinal direction and the buffer roller 30 formed at a predetermined interval on the lower side of the crimping portion 20. )), 완충롤러(30)상에 반접기된 부직포(10)가 얹혀지게 이동된 후, 부직포의 끝단은 이송롤러(36a),(36b)에 물려 고정되면 완충롤러(30)를 상부측에 형성된 압착부(20)측으로 상승시키는 단계와,After the semi-folded nonwoven fabric 10 is moved onto the buffer roller 30, the end of the nonwoven fabric is bitten by the feed rollers 36a and 36b to fix the buffer roller 30 to the upper side. Raising to the (20) side, 압착부(20)의 순간가열히터선(22)이 하강되면서 400℃∼800℃까지 순간 가열 압착시킴과 동시에 부직포(10)가 공급되는 수평선상까지 완충롤러(30)를 하강시켜 부직포(10)를 절단,융착시키는 단계와,While the instantaneous heating heater wire 22 of the crimping unit 20 is lowered, the instantaneous heating and compression of 400 ° C to 800 ° C is simultaneously performed, and the buffer roller 30 is lowered to the horizontal line on which the nonwoven fabric 10 is supplied. Cutting and fusion step; 압착부(20)의 순간가열히터선(22)에 의해 절단된 부직포(10)의 융착 부위가 완전하게 부착되도록 자연냉각되는 단계로 이루어지는 것을 특징으로 하는 부직포 봉투의 제조방법.Method of producing a nonwoven fabric bag characterized in that the step of natural cooling so that the fusion site of the nonwoven fabric (10) cut by the instantaneous heating heater wire (22) of the crimping portion 20 is completely attached. 제 1 항에 있어서, 상기 완충롤러(20)는 실리콘인 것을 특징으로 하는 부직포 봉투의 제조방법.The method according to claim 1, wherein the buffer roller (20) is silicon. 제 1 항에 있어서, 순간가열히터선(22)의 순간 가열시간은 0.2∼0.4초인 것을 특징으로 하는 부직포 봉투의 제조방법.The method for producing a nonwoven fabric bag according to claim 1, wherein the instantaneous heating time of the instantaneous heating heater wire (22) is 0.2 to 0.4 seconds.
KR1020050002139A 2005-01-10 2005-01-10 Method for manufacturing non-woven fabric bag KR100604950B1 (en)