JPS635701A - Footwear and its production - Google Patents
Footwear and its productionInfo
- Publication number
- JPS635701A JPS635701A JP61148163A JP14816386A JPS635701A JP S635701 A JPS635701 A JP S635701A JP 61148163 A JP61148163 A JP 61148163A JP 14816386 A JP14816386 A JP 14816386A JP S635701 A JPS635701 A JP S635701A
- Authority
- JP
- Japan
- Prior art keywords
- plastic
- sheet
- soft
- bottom member
- footwear
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。(57) [Summary] This bulletin contains application data before electronic filing, so abstract data is not recorded.
Description
【発明の詳細な説明】
[発明の目的]
(産業上の利用分野)
この発明は、例えば歩行可能なスリッパ型の足温器とし
て使用する履物およびその製造方法に関する。DETAILED DESCRIPTION OF THE INVENTION [Object of the Invention] (Industrial Application Field) The present invention relates to footwear used as, for example, a walkable slipper-type foot warmer, and a method for manufacturing the same.
(従来の技術)
例えば足温器として使用される履物は、第3図に示すよ
うに、偏平箱形状の底部材1の上面に足台2を取付け、
この足台2の下面側にヒータ3を組込み、また足台2の
上面をクツション材4を介して表布5で覆い、さらにこ
の表布5の先端側のほぼ半部を保温カバー6で覆ってス
リッパ状に構成してなる。そして上記底部材1は、人体
の体重を充分に支え得るように硬質のプラスチックで形
成されている。(Prior Art) For example, footwear used as a foot warmer has a footrest 2 attached to the upper surface of a flat box-shaped sole member 1, as shown in FIG.
A heater 3 is built into the lower surface of the footrest 2, and the upper surface of the footrest 2 is covered with an outer cloth 5 via a cushion material 4, and approximately half of the front end of the outer cloth 5 is covered with a heat insulating cover 6. It has a slipper-like structure. The bottom member 1 is made of hard plastic so as to be able to sufficiently support the weight of a human body.
ところが、このように底部材1が硬質のプラスチックで
あると、その特性上、床面等との摩擦抵抗が小さく、こ
のため歩行中に滑りゃすくなり、そこでこの底部材1の
下面に、大きな摩擦抵抗が生じる発泡ゴムなどの軟質の
滑り止め部材7を接着剤で取付けるようにしている。However, when the bottom member 1 is made of hard plastic, due to its characteristics, the frictional resistance with the floor etc. is small, making it easy to slip while walking. A soft anti-slip member 7 made of foamed rubber or the like that generates frictional resistance is attached with adhesive.
(発明が解決しようとする問題点)
しかしながら上述のように、底部材1の下面に接着剤を
用いて滑り止め部材7を取付ける手段においては、作業
上の能率が低下しやすいとともに、接着剤が無駄にはみ
出して経済的な損失を招きやすく、さらに接着剤に用い
る溶剤で作業環境が悪化し、また公害をひき起す恐れが
生じるという問題があった。この発明はこのような問題
点の解決を目的とするものである。(Problems to be Solved by the Invention) However, as described above, in the method of attaching the anti-slip member 7 to the lower surface of the bottom member 1 using an adhesive, work efficiency tends to decrease, and the adhesive There is a problem that the adhesive tends to overflow and cause economic loss, and that the solvent used in the adhesive worsens the working environment and may cause pollution. This invention aims to solve these problems.
[発明の構成]
この発明はこのような問題点を解決するために、硬質の
プラスチックで成形した底部材の下面に、軟質ないしは
半軟質のプラスチック製の滑り止め部材を、上記底部材
の成形時の熱で融着して一体的に取付けて履物を構成し
、また、金型内に、熱可塑性で軟質ないし半軟質のプラ
スチックのシートを配置し、この状態で金型内に、熱硬
化性で硬質のプラスチックの溶液を射出し、このプラス
チックの熱で上記シートの表面層を溶融させ、この溶融
で上記シートを上記プラスチックに融着して一体化し、
上記プラスチックを底部材として凝固させ、上記シート
をその底部材の下面に配置する滑り止め部材として硬化
させて履物を製造するようにしたものである。[Structure of the Invention] In order to solve these problems, the present invention provides a non-slip member made of soft or semi-soft plastic on the lower surface of the bottom member made of hard plastic. In addition, a soft or semi-soft thermoplastic sheet is placed in the mold, and in this state a thermosetting sheet is placed in the mold. inject a hard plastic solution, the heat of this plastic melts the surface layer of the sheet, and this melting fuses the sheet to the plastic and integrates it,
Footwear is manufactured by solidifying the plastic as a sole member and hardening the sheet as a non-slip member disposed on the lower surface of the sole member.
(作用)
底部材の成形時の熱を利用して、滑り止め部材の素材を
底部材に結合させることにより、接着剤の使用による弊
害を排除する。(Function) By using heat during molding of the bottom member to bond the material of the anti-slip member to the bottom member, the adverse effects caused by the use of adhesives are eliminated.
(実施例)
以下、この発明の一実施例について第1図および第2図
を参照Qて説明する。(Embodiment) An embodiment of the present invention will be described below with reference to FIGS. 1 and 2.
第1図に足温器として構成された履物を示し、11が底
部材、12が足台、13がヒータ、14がクツション材
、15が表布、16が保温カバーである。底部材11は
ポリプロピレン、ポリスチレン、ABS樹脂などの熱硬
化性で硬質のプラスチックにより一体に成形され、下面
には凹部17が形成されている。そしてこの底部材11
の下面に上記凹部17に嵌合するように滑り止め部材1
9が設けられ、この滑り止め部材19の下面に凸部20
・・・が−体に形、成されている。滑り止め部材19は
底部材11の材料よりも柔らかいオレフィン系熱可塑性
エラストマーなどの軟質ないしは半軟質のブラスッチク
で成形されている。そしてこの滑り止め部材19は底部
材11の成形時における熱に基づいて底部材11に融着
され、この融着て底部材11に一体的に取付けられてい
る。FIG. 1 shows footwear configured as a foot warmer, in which 11 is a sole member, 12 is a footrest, 13 is a heater, 14 is a cushioning material, 15 is an outer fabric, and 16 is a heat retaining cover. The bottom member 11 is integrally molded from thermosetting hard plastic such as polypropylene, polystyrene, ABS resin, etc., and has a recess 17 formed in its lower surface. And this bottom member 11
The anti-slip member 1 is placed on the bottom surface of the
9 is provided, and a convex portion 20 is provided on the lower surface of this anti-slip member 19.
...is formed into a body. The anti-slip member 19 is made of soft or semi-soft brass material such as an olefin thermoplastic elastomer that is softer than the material of the bottom member 11. The anti-slip member 19 is fused to the bottom member 11 based on the heat generated during molding of the bottom member 11, and is integrally attached to the bottom member 11 by this fusion.
製造の工程について述べると、まず、第2図(a)に示
すように、下金型a内に滑り止め部材19の素材である
オレフィン系熱可塑性エラストマーなどの軟質ないしは
半軟質のブラスッチクのシート19aを配置する。この
際、シート19aを予熱しておくことが好ましい。つい
で、同図(b)に示すように、下金型aの上面に上金型
すを閉じ合わせ、これら両全型a、b間のキャビティC
内にゲートdを通して、底部材11の素材である熱硬化
性で硬質のブラスッチ11aの溶液(150〜250°
C)を射出する。すると、このプラスチックllaの熱
でシート19aが適度に軟化し、かつプラスチックll
aの射出圧を受けてシート19aの一部がキャビティC
の内面の凹部C1・・・に落込むように変形し、またプ
ラスチック11aがシート19aを覆うように拡がる。Regarding the manufacturing process, first, as shown in FIG. 2(a), a sheet 19a of soft or semi-soft brass material such as olefin thermoplastic elastomer, which is the material of the anti-slip member 19, is placed in the lower mold a. Place. At this time, it is preferable to preheat the sheet 19a. Next, as shown in the same figure (b), the upper mold is closed on the upper surface of the lower mold a, and the cavity C between the two molds a and b is closed.
A solution (150 to 250°
C) is injected. Then, the sheet 19a is moderately softened by the heat of this plastic lla, and the plastic lla is
A part of the sheet 19a enters the cavity C under the injection pressure of
The plastic sheet 11a deforms so as to fall into the recess C1 on the inner surface of the sheet 19a, and the plastic sheet 11a spreads out to cover the sheet 19a.
そしてプラスチックllaの熱でこのプラスチック11
aと接触するシート19の表面層が溶融し、この溶融で
シート19aがプラスチックllaに融着する。このの
ち同図(c)に示すように、プラスチッllaが凝固し
て底部材11となり、またシート19aが硬化して底部
材11°に一体的に結合する滑り止め部材19となり、
さらにキャビティCの凹部c1・・・に落ち込んだ部分
が凸部20・・・となる。このようにして成形が済んだ
のちに、上金型すを開放して底部材11を滑り止め部材
19と一体にキャビティCから取出す。And with the heat of plastic lla, this plastic 11
The surface layer of sheet 19 in contact with a melts, and this melting fuses sheet 19a to plastic lla. After this, as shown in FIG. 2(c), the plasticilla solidifies to become the bottom member 11, and the sheet 19a hardens to become the anti-slip member 19 that is integrally connected to the bottom member 11°.
Furthermore, the portion depressed into the concave portion c1 of the cavity C becomes the convex portion 20. After the molding is completed in this manner, the upper mold is opened and the bottom member 11 and the anti-slip member 19 are taken out from the cavity C.
滑り止め部材19は軟質ないしは半軟質のプラスチック
であり、したがって床面等、に対する摩擦抵抗が大きく
、このためこの履物を履いて歩行する際にその歩行を軽
快に行なうことができる。しかも、この実施例では、滑
り止め部材19に一体に凸部20・・・を形成するよう
にしたから、さらに摩擦抵抗が増大し、より一層軽快に
歩行することができる。そして各凸部20・・・の成形
に応じてその上面側の部分が凹み、これら凹み部分に底
部材11の素材が介入して密着するから、滑り止め部材
19と底部材11との結合をより強固に保持することが
できる利点がある。The anti-slip member 19 is made of soft or semi-soft plastic, and therefore has a large frictional resistance against the floor surface, etc., so that the wearer can walk easily while wearing this footwear. Moreover, in this embodiment, since the protrusions 20 are integrally formed on the anti-slip member 19, the frictional resistance is further increased, and the user can walk even more easily. As each convex portion 20 is formed, the upper surface side thereof is recessed, and the material of the bottom member 11 intervenes in these recessed portions and comes into close contact with the non-slip member 19 and the bottom member 11. It has the advantage of being able to be held more firmly.
一方、この履物の製造に当たっては、底部材11の成形
時に、その熱を利用して底部材11の下面に滑り止め部
材19を融着して、底部材11に対して滑り止め部材1
9を一体的に取付けるようにしたから、従来のようにい
ちいち接着剤を用いて取付ける場合に比べ、作業能率が
大幅に向上するとともに、接着剤の無駄なはみ出しとい
うようなこともないから、経済的に有利となり、しがも
接着剤の場合のように溶剤を取扱う必要がないから、作
業環境の悪化や公害の問題の発生を排除することができ
る利点がある。On the other hand, in manufacturing this footwear, when the sole member 11 is molded, the anti-slip member 19 is fused to the lower surface of the sole member 11 using the heat, so that the anti-slip member 19 is attached to the bottom member 11.
9 is installed in one piece, compared to the conventional method of attaching each one using adhesive, work efficiency is greatly improved, and there is no needless protrusion of adhesive, making it more economical. Moreover, since there is no need to handle solvents as in the case of adhesives, there is an advantage that deterioration of the working environment and occurrence of pollution problems can be eliminated.
なお、上記実施例においては、この考案を足温器として
使用する履物を対象にして説明したが、必ずしもこのよ
うな履物に適用する場合に限らず、通常−般の履物にお
いても同様に適用することが可能である。In the above embodiments, this invention was explained with reference to footwear used as a foot warmer, but it is not necessarily applicable to such footwear, but can be similarly applied to ordinary footwear. Is possible.
[発明の効果]
以上説明したようにこの発明によれば、作業能率および
経済性の向上を図ることができるとともに、作業環境の
悪化や公害の問題の発生を排除することができるという
効果を奏する。[Effects of the Invention] As explained above, according to the present invention, it is possible to improve work efficiency and economic efficiency, and it is also possible to eliminate the deterioration of the work environment and the occurrence of pollution problems. .
第1図はこの発明の一実施例による履物を示す断面図、
第2図はその製造工程を示す断面図、第3図は従来の履
物を示す断面図である。
11・・・底部材、19・・・滑り止め部材、a、b・
・・金型。
出願人代理人 弁理士 鈴江武彦
第2図FIG. 1 is a sectional view showing footwear according to an embodiment of the present invention;
FIG. 2 is a sectional view showing the manufacturing process, and FIG. 3 is a sectional view showing conventional footwear. 11... Bottom member, 19... Anti-slip member, a, b.
··Mold. Applicant's agent Patent attorney Takehiko Suzue Figure 2
Claims (2)
軟質ないしは半軟質のプラスチック製の滑り止め部材を
、上記底部材の成形時の熱で融着して一体的に取付けた
ことを特徴とする履物。(1) On the bottom surface of the bottom member molded from hard plastic,
Footwear characterized in that a soft or semi-soft plastic anti-slip member is integrally attached by being fused using heat during molding of the sole member.
チックのシートを配置し、この状態で金型内に、熱硬化
性で硬質のプラスチックの溶液を射出し、このプラスチ
ックの熱で上記シートの表面層を溶融させ、この溶融で
上記シートを上記プラスチックに融着して一体化し、上
記プラスチックを底部材として凝固させ、上記シートを
その底部材の下面に配置する滑り止め部材として硬化さ
せることを特徴とした履物の製造方法。(2) Place a thermoplastic, soft or semi-soft plastic sheet in the mold, and in this state, inject a thermosetting, hard plastic solution into the mold, and use the heat of this plastic to The surface layer of the sheet is melted, the melting fuses and integrates the sheet with the plastic, the plastic solidifies as a bottom member, and the sheet hardens as a non-slip member disposed on the underside of the bottom member. A method of manufacturing footwear characterized by: