JPS6328261Y2 - - Google Patents

Info

Publication number
JPS6328261Y2
JPS6328261Y2 JP1982001324U JP132482U JPS6328261Y2 JP S6328261 Y2 JPS6328261 Y2 JP S6328261Y2 JP 1982001324 U JP1982001324 U JP 1982001324U JP 132482 U JP132482 U JP 132482U JP S6328261 Y2 JPS6328261 Y2 JP S6328261Y2
Authority
JP
Japan
Prior art keywords
template
adhesive
groove
opposing surfaces
corner
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP1982001324U
Other languages
Japanese (ja)
Other versions
JPS58104248U (en
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP132482U priority Critical patent/JPS58104248U/en
Publication of JPS58104248U publication Critical patent/JPS58104248U/en
Application granted granted Critical
Publication of JPS6328261Y2 publication Critical patent/JPS6328261Y2/ja
Granted legal-status Critical Current

Description

【考案の詳細な説明】 本考案は、型板用板材の角部を形成するための
溝内における一対の対向面の少なくとも一方に、
各対向面が相互に接合されたとき接着剤を収容す
ることができる程度の接着剤収容溝が形成された
型板用板材に関するものである。
[Detailed Description of the Invention] The present invention provides at least one of a pair of opposing surfaces in a groove for forming a corner of a template plate material.
The present invention relates to a template plate material in which an adhesive storage groove is formed to accommodate an adhesive when the opposing surfaces are joined to each other.

一面側に屈撓層を残して、先鋭な最深部より他
面側に向けて漸次拡大する溝を有し、この溝を形
成する一対の対向面を相互に接着することにより
角部を備えた型板を形成するための型板用板材に
おいて、従来は、前記一対の対向面が共に一様な
平面により形成されていたため、これらの対向面
を相互に接着すると、接着剤が角部の外表面に押
し出されてそのまま凝固し、角部の外観を損ねる
ばかりでなく、型板を使用する際各種の不都合が
生じていた。
It has a groove that gradually expands from the sharpest deepest part toward the other side, leaving a bending layer on one side, and a corner part is provided by bonding a pair of opposing surfaces that form this groove to each other. Conventionally, in a template plate material for forming a template, the pair of opposing surfaces were both formed by a uniform flat surface, so when these opposing surfaces were bonded together, the adhesive would not adhere to the outside of the corner. It is extruded to the surface and solidifies as it is, which not only spoils the appearance of the corner but also causes various inconveniences when using the template.

例えば第1図において、板材1の溝内の対向面
を相互に接着することにより形成された型板Aの
角部には、接着剤2が外表面に押し出されてその
まま凝固している状態が示されているが、このよ
うに接着剤2が型板Aの角部の外表面上で凝固し
ていると、例えば型板Aを部材3の角部に適用し
ようとしても、型板Aの角部と部材3の角部とが
正確に整合して密着し合わず、型板Aの表面と部
材3の表面との間に隙間が生じるという不都合が
ある。
For example, in FIG. 1, the adhesive 2 is extruded to the outer surface and solidified at the corner of the template A, which is formed by adhering the opposing surfaces in the grooves of the plate material 1 to each other. As shown in the figure, if the adhesive 2 has solidified on the outer surface of the corner of the template A in this way, even if you try to apply the template A to the corner of the member 3, for example, the adhesive 2 will not work properly. There is an inconvenience that the corner portion and the corner portion of the member 3 do not align accurately and come into close contact with each other, and a gap is created between the surface of the template A and the surface of the member 3.

そこで本考案の主な目的は、板材の溝内の対向
面を相互に接合しても、接着剤が外表面まで押し
出されることのないような型板用板材を得ること
である。
Therefore, the main object of the present invention is to obtain a plate material for a template in which the adhesive is not pushed out to the outer surface even when opposing surfaces in the groove of the plate material are joined to each other.

以下、図面に従つて本考案の一実施例について
説明する。先ず第2図において、一面側に例えば
塩化ビニール製化粧シートのような比較的薄い屈
撓層5と、例えば合板のような比較的厚い基板層
とよりなる板材4には、一面側に屈撓層5を残し
て、先鋭な最深部より他面側に向けて漸次拡大す
る溝が形成されておる。この溝を形成する一対の
対向面6,6′には、溝の拡大端より対向面6,
6′を切欠した切欠状接着剤収容溝7,7′が形成
され、それぞれ各対向面6,6′が相互に接合さ
れたとき接着剤を収容することができる。
An embodiment of the present invention will be described below with reference to the drawings. First of all, in FIG. 2, a plate material 4 consisting of a relatively thin flexible layer 5 such as a decorative sheet made of vinyl chloride on one side and a relatively thick substrate layer such as plywood has a flexible layer 5 on one side. Leaving the layer 5 intact, a groove is formed that gradually expands from the sharpest deepest part toward the other side. A pair of opposing surfaces 6, 6' forming this groove are provided with opposing surfaces 6, 6' from the enlarged end of the groove.
Notch-like adhesive storage grooves 7, 7' are formed by cutting out 6', and can accommodate adhesive when the respective opposing surfaces 6, 6' are joined to each other.

したがつて、一対の対向面6,6′を相互に接
合することにより第3図のように型板Bを形成す
る際には、一対の対向面6,6′間の接着剤8は
切欠状接着剤収容溝7,7′内に流れ込むことに
よつて、型板Bの角部の外表面まで押し出される
ことはなく、しかも、切欠状接着剤収容溝7,
7′の存在により接着面積が比較的大きくなつて、
型板Bの角部の接合強度が増加する。そして切欠
状接着剤収容溝7,7′は対向面6,6′を切欠し
て形成してあるので、切欠状接着剤収容溝7,
7′は大きく形成され、そのため流れ込む接着剤
を多量に収容できるので、より接合強度が向上す
る。
Therefore, when forming template B as shown in FIG. 3 by bonding the pair of opposing surfaces 6, 6' to each other, the adhesive 8 between the pair of opposing surfaces 6, 6' is notched. By flowing into the notch-shaped adhesive storage grooves 7, 7', it is not pushed out to the outer surface of the corner of the template B, and moreover, the notch-shaped adhesive storage grooves 7, 7'
Due to the presence of 7', the adhesive area becomes relatively large,
The joint strength of the corners of template B increases. Since the notched adhesive accommodating grooves 7, 7' are formed by cutting out the opposing surfaces 6, 6', the notched adhesive accommodating grooves 7, 7' are formed by cutting out the opposing surfaces 6, 6'.
7' is formed large so that a large amount of adhesive can be accommodated, thereby further improving the bonding strength.

また、接着剤が型板Bの角部の外表面まで押し
出されていないことにより、第4図のように、型
板Bを部材9の角部に適用する際、型板Bは完全
に部材9の角部に整合して密着することができ
る。
Furthermore, since the adhesive is not extruded to the outer surface of the corner of template B, when template B is applied to the corner of member 9 as shown in FIG. It can be aligned and closely attached to the corner of No. 9.

以上のように本考案によれば、型板を形成する
ための一対の対向面には、接着剤収容溝を形成す
るようにしたので、一対の対向面を相互に接合し
て型板を形成しても、接着剤が型板角部の外表面
に押し出されるようなことはなく、型板の外観が
損なわれないばかりでなく、角部の接合面積が拡
大されることにより接着強度が増加し、しかも型
板の他の部材の角部に対する適用時にも、型板は
他の部材の角部に完全に整合して密着することが
できる。
As described above, according to the present invention, since the adhesive storage groove is formed in the pair of opposing surfaces for forming the template, the pair of opposing surfaces are bonded to each other to form the template. Even when the adhesive is not pushed out to the outer surface of the template corners, not only does the appearance of the template remain intact, but the adhesive strength is increased by expanding the bonding area of the corners. Moreover, even when the template is applied to a corner of another member, the template can be perfectly aligned and tightly attached to the corner of the other member.

また接着剤収容溝を、対向面に切欠して形成し
たので、多量の接着剤が収容でき、その結果角部
の接合面積がより拡大され、そのため接着強度が
増加する等の利点がある。
Further, since the adhesive storage groove is formed by cutting out the opposing surface, a large amount of adhesive can be stored, and as a result, the bonding area of the corner portion is further expanded, which has the advantage of increasing adhesive strength.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図は従来の型板を他の部材の角部に適用し
た場合の要部横断面図、第2図は本考案の一実施
例に基づく板材の横断面図、第3図は第2図の板
材により形成された型板の横断面図、第4図は第
3図の型板を他の部材の角部に適用した場合の要
部横断面図である。 4……板材、5……屈撓層、6,6′……対向
面、7,7′……切欠状接着剤収容溝、8……接
着剤、B……型板。
FIG. 1 is a cross-sectional view of the main part when a conventional template is applied to the corner of another member, FIG. 2 is a cross-sectional view of a plate material based on an embodiment of the present invention, and FIG. FIG. 4 is a cross-sectional view of a main part when the template of FIG. 3 is applied to a corner of another member. 4... Plate material, 5... Flexible layer, 6, 6'... Opposing surface, 7, 7'... Notched adhesive storage groove, 8... Adhesive, B... Template.

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 一面側に屈撓層を残して、先鋭な最深部より他
面側に向けて漸次拡大する溝を有し、この溝を形
成する一対の対向面を相互に接着することにより
角部を備えた型板を形成するための型板用板材で
あつて、前記一対の対向面には前記溝の拡大端よ
り対向面を切欠した切欠状接着剤収容溝が形成さ
れていることを特徴とする、型板用板材。
It has a groove that gradually expands from the sharpest deepest part toward the other side, leaving a bending layer on one side, and a corner part is provided by bonding a pair of opposing surfaces that form this groove to each other. A template plate material for forming a template, characterized in that a cutout-shaped adhesive storage groove is formed in the pair of opposing surfaces by cutting out the opposing surface from the enlarged end of the groove, Board material for templates.
JP132482U 1982-01-11 1982-01-11 Plate material for template Granted JPS58104248U (en)