JPS63174399U - - Google Patents
Info
- Publication number
- JPS63174399U JPS63174399U JP4221887U JP4221887U JPS63174399U JP S63174399 U JPS63174399 U JP S63174399U JP 4221887 U JP4221887 U JP 4221887U JP 4221887 U JP4221887 U JP 4221887U JP S63174399 U JPS63174399 U JP S63174399U
- Authority
- JP
- Japan
- Prior art keywords
- foam
- soundproofing material
- utility
- model registration
- compression hardness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
第1図はこの考案の一実施例に関する防音材の
断面図、第2図は織布一例の部分拡大斜視図、第
3図は従来の防音材の断面図である。
22……織布、24……発泡体、26……遮音
層。
FIG. 1 is a sectional view of a soundproofing material according to an embodiment of this invention, FIG. 2 is a partially enlarged perspective view of an example of a woven fabric, and FIG. 3 is a sectional view of a conventional soundproofing material. 22... Woven fabric, 24... Foam, 26... Sound insulation layer.
Claims (1)
防音材において、1インチ当りの平均糸打込本数
が5〜30本である織布を発泡体に埋設したこと
を特徴とする防音材。 (2) 発泡体がウレタンフオームからなる実用新
案登録請求の範囲第1項に記載された防音材。 (3) 発泡体が25%圧縮硬さを5〜10Kg/3
14cm2、75%圧縮硬さ/25%圧縮硬さを3
.5以下、20mm厚の吸音率を500Hzで15
%以上、1KHzで50%以上とするものからな
る実用新案登録請求の範囲第1項または第2項に
記載された防音材。 (4) 織布が寒冷紗からなる実用新案登録請求の
範囲第1項ないし第3項のいずれかに記載された
防音材。[Scope of Claim for Utility Model Registration] (1) In a soundproofing material with a predetermined shape made by laminating a soundproofing layer on a foam, a woven fabric with an average number of yarns per inch of 5 to 30 is applied to the foam. Soundproofing material characterized by being buried. (2) The soundproofing material described in claim 1 of the utility model registration claim, in which the foam is made of urethane foam. (3) The foam has a 25% compression hardness of 5 to 10 kg/3
14cm 2 , 75% compression hardness/25% compression hardness 3
.. 5 or less, the sound absorption coefficient of 20mm thickness is 15 at 500Hz
% or more, and 50% or more at 1 KHz. (4) The soundproofing material described in any one of claims 1 to 3 of the utility model registration claim, in which the woven fabric is made of cheesecloth.