JPS63145258U - - Google Patents

Info

Publication number
JPS63145258U
JPS63145258U JP1987037992U JP3799287U JPS63145258U JP S63145258 U JPS63145258 U JP S63145258U JP 1987037992 U JP1987037992 U JP 1987037992U JP 3799287 U JP3799287 U JP 3799287U JP S63145258 U JPS63145258 U JP S63145258U
Authority
JP
Japan
Prior art keywords
layer
solid electrolyte
dense
interconnector
ceramics
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP1987037992U
Other languages
Japanese (ja)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP1987037992U priority Critical patent/JPS63145258U/ja
Publication of JPS63145258U publication Critical patent/JPS63145258U/ja
Pending legal-status Critical Current

Description

【図面の簡単な説明】[Brief explanation of the drawing]

図は本考案の一実施例に係る平板型固体電解質
燃料電池の説明図である。 1……インタコネクタ、2……第1層(ポーラ
ス層)、3……第2層(緻密層)、4……第3層
、5……Oガス通路、6……Hガス通路、7
……燃料側電極層、8……固体電解質膜、9……
電圧発生部、10……シール溝、11,12……
接触面。
The figure is an explanatory diagram of a flat solid electrolyte fuel cell according to an embodiment of the present invention. 1... Interconnector, 2... First layer (porous layer), 3... Second layer (dense layer), 4... Third layer, 5... O2 gas passage, 6... H2 gas passage ,7
...Fuel side electrode layer, 8...Solid electrolyte membrane, 9...
Voltage generating section, 10... Seal groove, 11, 12...
contact surface.

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 酸化ガス用の通路を有するポーラスで耐酸化性
セラミツクスからなる第1層、この第1層と同一
材料で該第1層を中央部に設けた窪みに接着した
緻密な第2層、及び耐還元性の優れたセラミツク
スからなる緻密な第3層の3つの層から構成され
るインタコネクタを有し、前記インタコネクタの
第1層に固体電解質膜及び燃料側電極膜からなる
電圧発生部を設けたことを特徴とする平板型固体
電解質燃料電池。
a first layer of porous, oxidation-resistant ceramics with passages for oxidizing gases; a dense second layer of the same material as this first layer and adhered to a depression in the center of the first layer; and a reduction-resistant layer. The present invention has an interconnector composed of three layers, including a dense third layer made of ceramics with excellent properties, and a voltage generating section consisting of a solid electrolyte membrane and a fuel-side electrode membrane is provided in the first layer of the interconnector. A flat plate solid electrolyte fuel cell characterized by:
JP1987037992U 1987-03-16 1987-03-16 Pending JPS63145258U (en)