JPS6248756U - - Google Patents
Info
- Publication number
- JPS6248756U JPS6248756U JP13775385U JP13775385U JPS6248756U JP S6248756 U JPS6248756 U JP S6248756U JP 13775385 U JP13775385 U JP 13775385U JP 13775385 U JP13775385 U JP 13775385U JP S6248756 U JPS6248756 U JP S6248756U
- Authority
- JP
- Japan
- Prior art keywords
- insulating packing
- nonaqueous electrolyte
- metal
- electrolyte battery
- polytrifluorochloroethylene
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
第1図は本考案電池の縦断面図、第2図はポリ
三フツ化塩化エチレン薄膜の装着工程を示す図、
第3図は本考案電池の保存期間と電池内部抵抗と
の関係を示す図である。
1……正極、2……金属ケース、4……負極、
5……金属封口蓋、7……セパレータ、8……絶
縁パツキング、9……ポリ三フツ化塩化エチレン
の薄膜。
FIG. 1 is a longitudinal cross-sectional view of the battery of the present invention, FIG. 2 is a diagram showing the process of attaching a polytrifluorochloroethylene thin film,
FIG. 3 is a diagram showing the relationship between the storage period of the battery of the present invention and the internal resistance of the battery. 1...Positive electrode, 2...Metal case, 4...Negative electrode,
5...Metal sealing lid, 7...Separator, 8...Insulating packing, 9...Thin film of polytrifluorochloroethylene.
Claims (1)
解液を保持したセパレータとよりなる発電要素を
、金属封口蓋と金属ケース及びこれらを絶縁する
絶縁パツキングにより密封した非水電解液電池に
おいて、前記絶縁パツキングの外部露出面をポリ
三フツ化塩化エチレンの薄膜で被覆したことを特
徴とする非水電解液電池。 In a nonaqueous electrolyte battery, a power generation element consisting of a positive electrode, a negative electrode using a light metal as an active material, and a separator holding a nonaqueous electrolyte is sealed with a metal sealing lid, a metal case, and an insulating packing that insulates them. A non-aqueous electrolyte battery characterized in that the externally exposed surface of the insulating packing is coated with a thin film of polytrifluorochloroethylene.