JPS62276817A - Aluminum electrolytic capacitor - Google Patents
Aluminum electrolytic capacitorInfo
- Publication number
- JPS62276817A JPS62276817A JP11972986A JP11972986A JPS62276817A JP S62276817 A JPS62276817 A JP S62276817A JP 11972986 A JP11972986 A JP 11972986A JP 11972986 A JP11972986 A JP 11972986A JP S62276817 A JPS62276817 A JP S62276817A
- Authority
- JP
- Japan
- Prior art keywords
- capacitor element
- foil
- aluminum electrolytic
- capacitor
- adhesive tape
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。(57) [Summary] This bulletin contains application data before electronic filing, so abstract data is not recorded.
Description
【発明の詳細な説明】
3、発明の詳細な説明
産業上の利用分野
本発明はアルミ電解コンデンサに関するものであり、さ
らに詳しく言えば、アルミ電解コンデンサに用いられる
コンデンサ素子の改良に関するものである。DETAILED DESCRIPTION OF THE INVENTION 3. Detailed Description of the Invention Field of Industrial Application The present invention relates to aluminum electrolytic capacitors, and more specifically, to improvements in capacitor elements used in aluminum electrolytic capacitors.
従来の技術
従来のアルミ電解コンデンサは、高純度のアルミニウム
箔を粗面化し表面積を拡大した後、陽極酸化により誘電
体酸化皮膜を形成した陽極箔と、アルミニウム箔を粗面
化して形成した陰極箔とをセパレータと共に巻回し、駆
動用電解液を含浸してコンデンサ素子を構成し、このコ
ンデンサ素子を有底筒状のケースに収納し、開放端を封
口体により封口して完成品としていた。Conventional technology Conventional aluminum electrolytic capacitors consist of an anode foil made by roughening high-purity aluminum foil to expand its surface area and then forming a dielectric oxide film through anodization, and a cathode foil made by roughening aluminum foil. The capacitor element was wound together with a separator and impregnated with a driving electrolyte to form a capacitor element, and the capacitor element was housed in a bottomed cylindrical case, and the open end was sealed with a sealing body to complete the finished product.
従来のこのようなアルミ電解コンデンサにおいて、その
コンデンサ素子としては、第8図、第9図に示すように
陰極箔1.陰極箔2をセパレータ3を介して巻回し、そ
の外周の上部に巻きもどり防止の粘着テープ4を巻付け
て構成されていた。In such a conventional aluminum electrolytic capacitor, the capacitor element includes a cathode foil 1, as shown in FIGS. 8 and 9. It was constructed by winding a cathode foil 2 with a separator 3 in between, and wrapping an adhesive tape 4 around the upper part of the outer circumference to prevent unwinding.
発明が解決しようとする問題点
このような従来のアルミ電解コンデンサにおいては、コ
ンデンサ素子の全長が長くなると、第10図に示すよう
に、粘着テープ4を巻きつけている以外の陰極箔2とセ
パレータ3が折返る部分5ができやすくなり、この折返
る部分5より破損が起ったり、駆動用電解液を含浸後、
封口体を合体させ、有底筒状のケースに収納する際、開
口端にひっかかったシして、生産性の向上、特に生産ス
ピードの向上に大きな限外要因となっていた。Problems to be Solved by the Invention In such conventional aluminum electrolytic capacitors, as the total length of the capacitor element increases, as shown in FIG. 3 is likely to form a folded part 5, and damage may occur from this folded part 5. After impregnating with driving electrolyte,
When the sealing bodies are combined and housed in a bottomed cylindrical case, they tend to get caught on the open end, which is a major impediment to improving productivity, especially production speed.
このような場合、一般的には第11図、第12図に示す
ように、コンデンサ素子の上端部および下端部に最低2
ケ所以上に粘着テープ4を巻きつけだシ、あるいは、は
ぼコンデンサ素子全域に亘って粘着テープ4を巻きつけ
ていた。In such a case, as shown in FIGS. 11 and 12, at least two
The adhesive tape 4 is wound more than once, or over the entire area of the capacitor element.
しかしながら、これらの方法では、粘着テープ4の費用
がかさばる上、巻取機の構造をも複雑にし、工数も増え
る欠点があった。However, these methods have disadvantages in that the cost of the adhesive tape 4 is large, the structure of the winding machine is complicated, and the number of man-hours is increased.
本発明はこのような問題点を解決するものであり、コン
デンサ素子の全長が長くなっても、巻きもどり防止の粘
着テープの幅を広げたり、複数本巻き付けたりしなくて
もよい、コンデンサ素子を提供するものである。The present invention solves these problems and provides a capacitor element that does not require increasing the width of the adhesive tape or wrapping multiple pieces of adhesive tape to prevent unwinding even if the overall length of the capacitor element becomes longer. This is what we provide.
問題点を解決するだめの手段
上記問題点を解決するために本発明は、高純度アルミニ
ウム箔を電気化学的に粗面化し、陽柩化成により誘電体
酸化皮膜を形成した陽極箔と陰極箔とをセパレータと共
に巻回し、陽極箔より長く巻回する陰極箔とセパレータ
の最終端を斜めに切断し、この切断部の突出部を巻きも
どり防止の粘着テープを巻き付けて、コンデンサ素子を
形成した構成とするものである。Means for Solving the Problems In order to solve the above problems, the present invention provides an anode foil and a cathode foil in which the surface of high-purity aluminum foil is electrochemically roughened and a dielectric oxide film is formed by positive chemical formation. is wound together with a separator, the cathode foil wound longer than the anode foil and the final end of the separator are cut diagonally, and the protrusion of this cut is wrapped with adhesive tape to prevent unwinding to form a capacitor element. It is something to do.
作用
このような構成とすることにより、折返り部分をあらか
じめ削除していることになり、折返りの発生防止ができ
ることになる。Effect: With this configuration, the folded portion is removed in advance, and folding can be prevented from occurring.
実施例 以下、本発明の一実施例につき説明する。Example An embodiment of the present invention will be described below.
第1図〜第3図に示すように、高純度アルミニウム箔を
電気化学的に粗面化し陽極化成により誘電体酸化皮膜を
形成した陽極箔6と陰極箔7とをセパレータ8と共に巻
回し、陽極箔6よυ長く巻回する陰極箔7とセパレータ
8の最終端を右上より左下にかけて斜めに切断し、巻き
もどυ防止の粘着テープ9を切断部の突出部の位置する
上部に巻き付けて、コンデンサ素子1oを形成する。As shown in FIGS. 1 to 3, an anode foil 6 and a cathode foil 7, which are made by electrochemically roughening high-purity aluminum foil and forming a dielectric oxide film by anodization, are wound together with a separator 8, and the anode The final ends of the cathode foil 7 and separator 8, which are wound longer than the foil 6, are cut diagonally from the upper right to the lower left, and the adhesive tape 9 to prevent unwinding is wrapped around the upper part of the cut part where the protruding part is located. An element 1o is formed.
このコンデンサ素子10の陽極箔6.陰極箔7から引出
リード11.12が引出されており、このコンデンサ素
子1oに駆動用電解液を含浸し、これを有底筒状のアル
ミニウムなどからなるケース13に収納し、上記引出リ
ード11.12を接続するターミナル14.15をもつ
封口体16を上記ケース13の開口部に封着してアルミ
電解コンデンサとしている。Anode foil 6 of this capacitor element 10. Output leads 11 and 12 are drawn out from the cathode foil 7, and the capacitor element 1o is impregnated with a driving electrolyte and housed in a bottomed cylindrical case 13 made of aluminum or the like. A sealing body 16 having terminals 14 and 15 for connecting the capacitors 12 and 12 is sealed to the opening of the case 13 to form an aluminum electrolytic capacitor.
又、第4図、第5図に示すように、コンデンサ素子1o
として上述の実施例とは逆に、陰極箔7とセパレータ8
の最終端を左上より右下にかけて斜めに切断し、巻きも
どり防止の粘着テープ9をコンデンサ素子1Qの下部に
巻き付けて、コンデンサ素子10を形成する。Moreover, as shown in FIGS. 4 and 5, the capacitor element 1o
As opposed to the above-mentioned embodiment, the cathode foil 7 and the separator 8
The final end of the capacitor element 1Q is cut diagonally from the upper left corner to the lower right corner, and an adhesive tape 9 to prevent unwinding is wrapped around the lower part of the capacitor element 1Q to form a capacitor element 10.
他に、陰極箔7とセパレータ8の最終端の切断を粘着テ
ープ9を巻き付ける部分のみほぼテープ1j冨の寸法を
垂直に切断し、他は斜めに切断しても効果は同じで有り
、その実施例を第6図、第7図に示す。Alternatively, the final ends of the cathode foil 7 and the separator 8 can be cut perpendicularly to the width of the tape 1j only at the part where the adhesive tape 9 is wrapped, and the other parts cut diagonally; the effect is the same, and the method is Examples are shown in FIGS. 6 and 7.
発明の効果
以」二のように本発明によれば、コンデンサ素子の全長
が長くなっても、コンデンサ素子の巻きもどり防止の粘
着テープの使用本数を増やしたり、幅を広くした粘着テ
ープを使用する必要がなく、テープの材料費アップを防
ぐ上、巻取機械も簡素な設計でよく、工数も増やすこと
なく、コスト及び生産性に大きく貢献する工業的価値の
大なるものである。Effects of the Invention According to the present invention, even if the total length of the capacitor element becomes longer, the number of adhesive tapes used to prevent the capacitor element from unwinding can be increased, and adhesive tape with a wider width can be used. This eliminates the need for this method, prevents an increase in tape material costs, requires a simple design of the winding machine, and does not increase the number of man-hours, which is of great industrial value and greatly contributes to cost and productivity.
第1図は本発明のアルミ電解コンデンサの一実施例を示
す断正面図、第2図は同コンデンサに用いるコンデンサ
素子の斜視図、第3図は同コンデンサ素子の分解斜視図
、第4図は他の実施例のコンデンサ素子の斜視図、第5
図は同コンデンサ素子の分解斜視図、第6図、第7図は
さらに他のコンデンサ素子の釦視図、第8図は従来のア
ルミ電解コンデンサに用いるコンデンサ素子の斜視図、
第9図は同コンデンサ素子の分解斜視図、第1Q図は同
コンデンサ素子の問題点を示す斜視図、第11図、第1
2図は他の従来のコンデンサ素子を示す1、+視図であ
る。
6・・・陽極箔、7・・・陰極箔、8・・・・・セパレ
ータ、9・・・・・・粘着テープ、10・・・・・コン
デンサ素子、13・・・・・ケース、16・・・封口体
。
代理人の氏名 弁理士 中 尾 敏 男 ほか1名第1
図
第2図 箔3図
第4図 第5図
第6図 第7図
箸8図 第9図
第10口
第11図
第12図Fig. 1 is a sectional front view showing one embodiment of an aluminum electrolytic capacitor of the present invention, Fig. 2 is a perspective view of a capacitor element used in the capacitor, Fig. 3 is an exploded perspective view of the capacitor element, and Fig. 4 is a perspective view of the capacitor element used in the capacitor. Perspective view of a capacitor element of another embodiment, No. 5
The figure is an exploded perspective view of the same capacitor element, Figures 6 and 7 are button views of other capacitor elements, and Figure 8 is a perspective view of a capacitor element used in a conventional aluminum electrolytic capacitor.
Figure 9 is an exploded perspective view of the same capacitor element, Figure 1Q is a perspective view showing problems with the same capacitor element, Figure 11, Figure 1
FIG. 2 is a 1,+ view showing another conventional capacitor element. 6... Anode foil, 7... Cathode foil, 8... Separator, 9... Adhesive tape, 10... Capacitor element, 13... Case, 16 ...Sealed body. Name of agent: Patent attorney Toshio Nakao and 1 other person No. 1
Figure 2 Foil 3 Figure 4 Figure 5 Figure 6 Figure 7 Chopsticks 8 Figure 9 Figure 10 Mouth 11 Figure 12
Claims (1)
電体酸化皮膜を形成した陽極箔と陰極箔とをセパレータ
と共に巻回し最終端を斜めに切断し、巻きもどり防止の
ための粘着テープを巻きつけてコンデンサ素子を構成し
、このコンデンサ素子に駆動用電解液を含浸し有底筒状
のケースに収納し、このケースの開放端を封口体と共に
封口してなるアルミ電解コンデンサ。The anode foil and cathode foil, which are made by roughening high-purity aluminum foil and forming a dielectric oxide film through anodizing, are wound together with a separator, the final end is cut diagonally, and an adhesive tape is wrapped to prevent unwinding. An aluminum electrolytic capacitor that consists of a capacitor element, impregnated with a driving electrolyte, housed in a bottomed cylindrical case, and sealed with a sealing body at the open end of the case.