JPS6213458B2 - - Google Patents

Info

Publication number
JPS6213458B2
JPS6213458B2 JP59279220A JP27922084A JPS6213458B2 JP S6213458 B2 JPS6213458 B2 JP S6213458B2 JP 59279220 A JP59279220 A JP 59279220A JP 27922084 A JP27922084 A JP 27922084A JP S6213458 B2 JPS6213458 B2 JP S6213458B2
Authority
JP
Japan
Prior art keywords
weight
paint
water
rust
waterproof
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP59279220A
Other languages
Japanese (ja)
Other versions
JPS60186562A (en
Inventor
Yasuo Yamanishi
Takaro Nishizawa
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GENTEN KK
Original Assignee
GENTEN KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GENTEN KK filed Critical GENTEN KK
Priority to JP27922084A priority Critical patent/JPS60186562A/en
Publication of JPS60186562A publication Critical patent/JPS60186562A/en
Publication of JPS6213458B2 publication Critical patent/JPS6213458B2/ja
Granted legal-status Critical Current

Description

【発明の詳細な説明】 本発明は、普通の陸屋根の塗装面は勿論のこ
と、特に潮風や海水にさらされる船舶デツキに使
用する特殊な下地保護材を使用した化粧塗料の塗
装面の下地保護方法に関するものである。
DETAILED DESCRIPTION OF THE INVENTION The present invention is intended to protect the base of painted surfaces of decorative paints using a special base protection material used not only for the painted surfaces of ordinary flat roofs, but also for ship decks that are exposed to sea breeze and seawater. It is about the method.

而して、従来の下地保護材や防水防錆材(特公
昭58−58152参照)は大なり小なりのセメントモ
ルタルを素材の一部に採用してあるためにアスフ
アルトの柔軟性を硬化してその凝固過程で割れ目
やピンホールが生じ易い欠点があつた。
Conventional base protection materials and waterproof and rust preventive materials (see Japanese Patent Publication No. 58-58152) use more or less cement mortar as part of the material, which hardens the asphalt's flexibility. The drawback was that cracks and pinholes were likely to occur during the solidification process.

本発明は、このような欠点を解消して、耐候性
や強度が強く、塗装面にして人の歩行や車の走行
に耐えられて割れ目ピンホールを生ずることのな
い普通の陸屋根は勿論のこと、潮風や海水にされ
される船舶デツキ用の化粧塗料の塗装面の下地保
護方法を提供することを目的とする。
The present invention solves these drawbacks, and has strong weather resistance and strength, and the painted surface can withstand walking by people and driving cars, and does not cause cracks or pinholes, as well as ordinary flat roofs. The purpose of the present invention is to provide a method for protecting the base of a painted surface of a decorative paint for ship decks that is exposed to sea breeze and seawater.

以下、本発明の実施例を図面に基づき説明す
る。
Embodiments of the present invention will be described below based on the drawings.

本実施例の下地保護材は、水溶性アスフアルト
を重量12%〜20%、粒径数mm以下の粒骨材や石粉
を重量50%〜70%、水を重量20%〜25%、水性接
着剤を重量1%〜10%及び線等のスサを重量1%
〜5%の割合で混合撹拌した独特のものであり、
図面に示すように、陸屋根や船舶デツキ等の塗装
面1に防水防錆塗料2を塗布した後、この防水防
錆塗料2の上面に前記下地保護材3をコテで厚塗
りし、その上に化粧塗料4を塗布するようにして
用いるものである。
The base protection material of this example consists of 12% to 20% by weight of water-soluble asphalt, 50% to 70% by weight of granular aggregate or stone powder with a grain size of several mm or less, 20% to 25% by weight of water, and water-based adhesive. 1% to 10% by weight of agent and 1% by weight of wire etc.
It is a unique product that is mixed and stirred at a ratio of ~5%,
As shown in the drawing, after applying a waterproof and rust-proofing paint 2 to a painted surface 1 such as a flat roof or ship's deck, the base protection material 3 is thickly applied on the top surface of this waterproof and rust-proofing paint 2 with a trowel, and then It is used by applying the decorative paint 4.

この発明による陸屋根や船舶デツキ用の化粧塗
料の塗装面の下地保護方法によれば、前記下地保
護材3はこれに含有する水性接着剤が下地保護材
の分子間に水溶性アスフアルトの附着力と共に接
着作用を及ぼし、かつその接着剤は均等に撹拌さ
れ、粒骨材やスサ類が、構成素材の素材間の移動
を拘束するので、これらの相乗効果により下地保
護材の耐候性や強度を強化して人の歩行や車の走
行に耐えることができるし、アスフアルトの長期
に亘る柔軟性によりクラツクや割れ目を生じさせ
ることがない。なお、この下地保護材は塗装前は
水分含有率が高いので滑らかに塗布しやすく附着
力も大きいものである。よつて、この下地保護材
3を普通の陸屋根は勿論のこと特に潮風や海水に
さらされる船舶デツキ等に塗布する適当な防水防
錆塗料2の上に塗着すると、収縮によるクラツク
や剥離等が生じないから、防水防錆の塗料2をよ
く保護して陸屋根の防水や船舶デツキ等の防錆を
強化するとともに化粧塗料の安定と耐久力を増加
させる有益な化粧塗料の塗装面の下地保護方法で
ある。
According to the base protection method for the coated surface of a decorative paint for flat roofs and ship decks according to the present invention, the base protection material 3 has a water-based adhesive contained therein, and the adhesion force of the water-soluble asphalt between the molecules of the base protection material. It has an adhesive effect, and the adhesive is evenly stirred, and the granular aggregate and fibers restrain the movement of the constituent materials, so the synergistic effect of these effects strengthens the weather resistance and strength of the base protection material. Asphalt can withstand foot traffic and vehicle traffic, and the long-term flexibility of asphalt prevents it from cracking or cracking. Note that this base protective material has a high moisture content before painting, so it is easy to apply smoothly and has high adhesion. Therefore, if this base protection material 3 is applied on a suitable waterproof and anticorrosive paint 2 that is applied not only to ordinary flat roofs but also to ship decks exposed to sea breezes and seawater, cracks and peeling due to shrinkage can be prevented. This is a useful method for protecting the base of the painted surface of decorative paint, which protects the waterproof and rust-proof paint 2 and strengthens the waterproofing of flat roofs and the rust prevention of ship decks, etc., and increases the stability and durability of the decorative paint. It is.

【図面の簡単な説明】[Brief explanation of the drawing]

図面は本発明下地保護方法の説明断面図を示
す。 1:陸屋根又は船舶デツキの塗装面、2:防水
防錆塗料、3:下地保護材、4:化粧塗料。
The drawing shows an explanatory cross-sectional view of the substrate protection method of the present invention. 1: Painted surface of flat roof or ship deck, 2: Waterproof and rust-proofing paint, 3: Base protection material, 4: Decorative paint.

Claims (1)

【特許請求の範囲】[Claims] 1 塗装面に防水防錆塗料を塗布した後、この防
水防錆塗料上面に、水溶性アスフアルトを重量12
%〜20%、粒径数mm以下の粒骨材や石粉を重量50
%〜70%、水を重量20%%〜25%、水性接着剤を
重量1%〜10%、スサ重量1%〜5%の割合で混
合した下地保護材をコテで厚塗りし、さらに下地
保護材面上に化粧塗料を塗布した陸屋根や船舶デ
ツキ用の化粧塗料の塗装面の下地保護方法。
1 After applying waterproof and rust-proofing paint to the painted surface, apply water-soluble asphalt to the top surface of this waterproof and rust-proofing paint with a weight of 12 kg.
% ~ 20%, granular aggregate or stone powder with a particle size of several mm or less by weight 50
% to 70% by weight, water by weight from 20% to 25%, water-based adhesive from 1% to 10% by weight, and fiberglass from 1% to 5% by weight. A method for protecting the base of a decorative paint surface for flat roofs and ship decks where decorative paint is applied on the protective material surface.
JP27922084A 1984-12-28 1984-12-28 Substrate protecting material of coated surface Granted JPS60186562A (en)