JPS61182915U - - Google Patents
Info
- Publication number
- JPS61182915U JPS61182915U JP6650785U JP6650785U JPS61182915U JP S61182915 U JPS61182915 U JP S61182915U JP 6650785 U JP6650785 U JP 6650785U JP 6650785 U JP6650785 U JP 6650785U JP S61182915 U JPS61182915 U JP S61182915U
- Authority
- JP
- Japan
- Prior art keywords
- sprayed
- wear
- sliding surface
- magnetic head
- resistant material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
第1図は本考案の一実施例のテープ摺動面に酸
化チタンを溶射したヘツドのテープ摺動面を示す
正面図である。 2……録音―再生間のシールドバン、3……録
音及び再生コア、4……酸化チタン溶射面。
化チタンを溶射したヘツドのテープ摺動面を示す
正面図である。 2……録音―再生間のシールドバン、3……録
音及び再生コア、4……酸化チタン溶射面。
Claims (1)
- 高硬度・耐摩耗性材がテープ摺動面に溶射され
た磁気ヘツドにおいて、テープ摺動面上のコアあ
るいはシールドバンと溶射面との間のすき間を潤
滑性・耐摩性を有する物質で充てんしたことを特
徴とする磁気ヘツド。