JPS605067U - laminated battery - Google Patents
laminated batteryInfo
- Publication number
- JPS605067U JPS605067U JP1983096550U JP9655083U JPS605067U JP S605067 U JPS605067 U JP S605067U JP 1983096550 U JP1983096550 U JP 1983096550U JP 9655083 U JP9655083 U JP 9655083U JP S605067 U JPS605067 U JP S605067U
- Authority
- JP
- Japan
- Prior art keywords
- current collector
- unit cell
- container
- electrode
- laminated battery
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。(57) [Summary] This bulletin contains application data before electronic filing, so abstract data is not recorded.
Description
第1図は従来の積層電池の断面図、第2図はこの考案に
係る積層電池の一実施例を示す断面図である。
10・・・・・・素電池、12・・・・・・容器、14
・・・・・・陰極合剤、16・・・・・・セパレータ、
18・・・・・・陽極合剤、20・・・発電要素、22
・・・・・・シール剤、24・・・・・・陰極集電体、
26・・・・・・陽極集電体、28・・・・・・凹部。FIG. 1 is a cross-sectional view of a conventional stacked battery, and FIG. 2 is a cross-sectional view showing an embodiment of the stacked battery according to this invention. 10...Battery, 12...Container, 14
...Cathode mixture, 16...Separator,
18... Anode mixture, 20... Power generation element, 22
... Sealing agent, 24 ... Cathode current collector,
26...Anode current collector, 28...Recessed portion.
Claims (1)
合剤を積層状態で装填した素電池を該容器内に収納され
た一方極の集電体と該素電池の下方に位置する他の素電
池の他方極の集電体とをシール材を介在させて溶着して
なる積層電池において、該容器内の底部に該集電体より
僅かに大径の凹部を形成してなることを特徴とする積層
電池。A unit cell in which a cathode mix, a separator, and an anode mix are loaded in a stacked state in a synthetic resin dish-shaped container is housed in the container, and one electrode current collector and the other are located below the unit cell. In a stacked battery formed by welding a current collector of the other electrode of a unit cell with a sealing material interposed, a concave portion having a diameter slightly larger than that of the current collector is formed at the bottom of the container. Characteristic stacked battery.