JPS60110638A - Bottle made of saturated polyester resin - Google Patents
Bottle made of saturated polyester resinInfo
- Publication number
- JPS60110638A JPS60110638A JP59141840A JP14184084A JPS60110638A JP S60110638 A JPS60110638 A JP S60110638A JP 59141840 A JP59141840 A JP 59141840A JP 14184084 A JP14184084 A JP 14184084A JP S60110638 A JPS60110638 A JP S60110638A
- Authority
- JP
- Japan
- Prior art keywords
- polyester resin
- saturated polyester
- bottle
- bottle made
- legs
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。(57) [Summary] This bulletin contains application data before electronic filing, so abstract data is not recorded.
Description
【発明の詳細な説明】
本発明は二軸延伸ブロー成形により肉薄に形成された透
明な飽和ポリエステル樹脂製機にμqするもので、二軸
延伸が十分でなし4頭部および底部等がオーデコロン、
香水等の香料やアルコール系液体等のアルコール系成分
を含有する内容物を収容してもクレージングや熱変形を
生じることのない飽和ポリエステル樹脂製機を得ること
を目的とするものである。DETAILED DESCRIPTION OF THE INVENTION The present invention is a transparent saturated polyester resin machine formed thinly by biaxial stretching blow molding.
The object of the present invention is to obtain a saturated polyester resin machine that does not cause crazing or thermal deformation even when containing contents containing fragrances such as perfumes and alcoholic components such as alcoholic liquids.
特に、壜の底部は二軸延伸による吹込み成形の特質から
その中央部分で二輪延伸が十分得られず、つまり分子の
配向および結晶化傾向が十分得られず、前記したクレー
ジングや熱変形を牛じゃすい。In particular, due to the characteristic of blow molding using biaxial stretching, the bottom of the bottle cannot be sufficiently stretched in the center, which means that sufficient molecular orientation and crystallization tendency cannot be obtained, which prevents the above-mentioned crazing and thermal deformation. Jasui.
本発明は、二軸延伸により肉薄に形成された透明な飽和
ポリエステル樹脂製機において、増体下端に、壜胴部の
下端周縁部分と増体底部の周縁部分が下方に屈曲された
突出部分とによって形成された脚部を有し、該脚部を除
いて増体底部の全体が熱処理による結晶化の白化部とさ
れているという構成であり、これによってオーデコロン
、香水等の香料やアルコール系液体等のアルコール系成
分を含有する内容物を収容しても底部がクレージングや
熱変形を生じることがない等の効果を達成しうるもので
ある。The present invention provides a transparent saturated polyester resin machine formed thinly by biaxial stretching, in which a protruding portion is provided at the lower end of the bottle body and a peripheral edge portion of the bottom of the bottle is bent downward. It has legs formed by It is possible to achieve the effect that the bottom part does not undergo crazing or thermal deformation even when containing contents containing alcohol-based components such as the following.
以下図面に基づいて、本発明の詳細な説明する○
第1図に示すように、飽和ポリエステル樹脂装填は、魚
体1の胴部2の下端周縁部3と、魚体底部40周縁部分
が下方に屈曲された突出部5とによって、脚部6が形成
されている。前記底部4は二軸延伸ブロー成形の特質ふ
ら脚部6より底部の中心部分に近づくに従って延伸の度
合が少なく、それゆえ脚部6に比べてオーデコロン、香
水等の香料やアルコール系液体等のアルコール成分を含
有する内容物に対する耐物性が弱く、クレーソングや熱
変形を生じやすい状態となっている。The present invention will be described in detail below based on the drawings. As shown in FIG. A leg portion 6 is formed by the protruding portion 5 . The bottom part 4 has a characteristic of biaxial stretch blow molding, and the degree of stretching is smaller as it gets closer to the center of the bottom part than the leg part 6, and therefore, compared to the leg part 6, it is less likely to be stretched than the leg part 6. It has poor resistance to contents containing ingredients, and is prone to clay songs and thermal deformation.
そこで、本発明の魚体は、前記脚部6を除いて底部4全
体を熱処理による結晶化の白化部(点線で示す部分〕と
したものである。Therefore, in the fish body of the present invention, the entire bottom portion 4 except for the leg portions 6 is made into a whitened portion (the portion shown by the dotted line) due to crystallization due to heat treatment.
前記白化部を有するポリエステル樹脂装填を形成するに
は、第2図に示すような完成形壮の口頚部を有する有底
筒状の透明な中111素利Pを射出成形したのち、該中
間素材Pの底部中心部分、すなわち、該中間索−材Pが
二軸延伸されて魚体に形成された時該魚体の底部となる
部分に相当する中心部分をヒータ等により例えば]]キ
O℃〜160°013〜5分1?tT加し、引き続きこ
れを常温にまで徐冷して結晶化による白化をなさしめ、
次いで該中間素材Pを二軸延伸ブロー成形して、第1図
に示すような脚部を除いて底部が白化した魚体を形成す
る。In order to form the polyester resin filling having the whitened portion, after injection molding a bottomed cylindrical transparent medium P having a full-sized mouth and neck as shown in FIG. 2, the intermediate material is The center part of the bottom of P, that is, the center part corresponding to the part that will become the bottom of the fish body when the intermediate rope material P is biaxially stretched and formed into a fish body, is heated to 0°C to 160°C using a heater or the like. °013 ~ 5 minutes 1? tT, and then slowly cooled to room temperature to cause whitening due to crystallization.
Next, the intermediate material P is biaxially stretched and blow molded to form a fish body with a whitened bottom except for the legs as shown in FIG.
なお、飽和ポリエステル樹脂はガラス転移点温度が約7
0°Cであり、これ以上かつ結晶化温度以下の温度帯域
で適宜時間加熱し、放置すると、温度と時間との相関関
係により結晶化して白化現象を生ずる。また前記魚体の
成形において、中間素材は底部中心部分を白化した後二
軸延伸するものであるから、その白化は延伸性が失われ
ない程度に白化せしめることが必要である。Note that the glass transition temperature of saturated polyester resin is approximately 7.
If the temperature is 0°C and is heated for an appropriate period of time in a temperature range above this temperature and below the crystallization temperature and left to stand, crystallization occurs due to the correlation between temperature and time, resulting in a whitening phenomenon. Further, in the molding of the fish body, the intermediate material is biaxially stretched after whitening the bottom center portion, so it is necessary to whiten the material to an extent that the stretchability is not lost.
上記魚体は、底部が二軸延伸ブロー成形の特質からその
延伸が十分なされなくとも、該底部を結晶化による白化
部とすることによって、オーデコロン、香水等の香料や
アルコール系成分を含有する内容物を収容しても、壜底
部がクレーソングを生起したり、熱変形を生じることが
ない。Even if the bottom part of the fish body is not sufficiently stretched due to the characteristics of biaxial stretch blow molding, by making the bottom part a white part due to crystallization, the contents containing perfumes such as cologne, perfume, etc. and alcoholic components can be stored. Even when the bottle is stored, the bottom of the bottle will not form clay songs or undergo thermal deformation.
第1図は、本発明の飽和ポリエステル樹脂装填の断面図
、第2図は前記飽和ポリエステル樹脂製穆を成形するた
めの中間素材の断面図である。
1:@体、2:胴部、3;下端周縁部、4:底部、5:
突出部、6:脚部。
第1図 第2図FIG. 1 is a sectional view of the saturated polyester resin loading according to the present invention, and FIG. 2 is a sectional view of an intermediate material for molding the saturated polyester resin smear. 1: @Body, 2: Body, 3: Lower edge, 4: Bottom, 5:
Projection, 6: Leg. Figure 1 Figure 2
Claims (1)
ル樹脂製機において、増体下端に、壜胴部の下端周縁部
分と増体底部の周縁部グカー下方に屈曲された突出部分
とによって形成された脚部を有し、該脚部を除いて増体
底部の全体が熱処理による結晶化の白化部とされてl/
Xることを特徴とする飽和ポリエステル樹脂製機。In a transparent saturated polyester resin machine formed thinly by biaxial stretching, the lower end of the bottle body is formed by a lower peripheral edge portion of the bottle body and a protruding portion bent downward from the peripheral edge of the bottom of the expanded bottle. It has legs, and the entire bottom of the increase except for the legs is a whitened part due to crystallization due to heat treatment.
A saturated polyester resin manufacturing machine characterized by