JPS58191109A - Manufacture of aggregate precious-wood decorative board - Google Patents
Manufacture of aggregate precious-wood decorative boardInfo
- Publication number
- JPS58191109A JPS58191109A JP7494382A JP7494382A JPS58191109A JP S58191109 A JPS58191109 A JP S58191109A JP 7494382 A JP7494382 A JP 7494382A JP 7494382 A JP7494382 A JP 7494382A JP S58191109 A JPS58191109 A JP S58191109A
- Authority
- JP
- Japan
- Prior art keywords
- wiping
- precious
- manufacture
- aggregate
- veneers
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。(57) [Summary] This bulletin contains application data before electronic filing, so abstract data is not recorded.
Description
【発明の詳細な説明】
[目的]
集成化粧単板を使用して集成銘木化粧板を製造る方法に
おいて、特に仕上げにおけるワイピング処理の際のムラ
をなくし、硬質感を与えるような仕上げ状態を実現する
ことを目的とする。[Detailed Description of the Invention] [Objective] In a method of manufacturing laminated decorative wood veneers using laminated decorative veneers, in particular, to eliminate unevenness during wiping processing during finishing and achieve a finish that gives a hard feel. The purpose is to
[背景技術]
集成化粧単板は原料単板を適当枚数接着剤を介して重ね
、型盤に挾んで圧締して一体化してフリッチとなし、こ
れをスライスすることにより製造されている。このスラ
イス単板は大抵の場合0゜3〜0.6mmぐらいである
が、これをツキ板として基板の上に貼着して銘木化粧板
として実用している。[Background Art] Laminated decorative veneers are manufactured by stacking an appropriate number of raw material veneers with an adhesive, sandwiching them between molds and pressing them together to form a flitch, and slicing this. This sliced veneer is usually about 0.3 to 0.6 mm in diameter, and is used as a decorative wood board by pasting it onto a substrate as a veneer.
そして、基板の上に集成化粧単板を貼着した後、そρ、
二面にワイピング処理を施すのであるが、従来の集成化
粧単板の場合は、原料単板の原木材質の相違によりワイ
ピングむらが生し、銘木化粧板の品質を悪くしていた。After pasting the laminated decorative veneer on the board,
Wiping is performed on two sides, but in the case of conventional laminated decorative veneers, uneven wiping occurs due to differences in the quality of the raw wood veneers, which deteriorates the quality of the precious wood decorative veneers.
この発明はかがる事情、−に鑑みてなされた。This invention was made in view of the following circumstances.
なお、ここでワイピング処理とはワイピング剤を集成化
粧単板の表面に塗布し、その塗布面をウェスなとで擦る
か、ブラッシングを行うことを意味する。そして、ワイ
ピング剤とは溶剤と樹脂と顔料の配合物である。Note that the wiping treatment here means applying a wiping agent to the surface of the laminated decorative veneer and rubbing or brushing the applied surface with a cloth. The wiping agent is a mixture of a solvent, a resin, and a pigment.
[発明の開示]
この発明はワイピングを行う前に、基板に貼着した集、
成化粧単板表面に水溶性アクリル樹脂エマルジョンを塗
布し、乾燥し、サンディング処理を施すことを特徴とす
る。[Disclosure of the Invention] The present invention provides a method for removing the adhesive, which is attached to a substrate before wiping.
It is characterized by applying a water-soluble acrylic resin emulsion to the surface of the decorative veneer, drying it, and then sanding it.
ここで使用される集成化粧単板は従来のものをそのまま
使用することが出来る。ワイピング剤も従来のもので足
りる。ワイピング処理の方法も従来の方法でよい。集成
化粧単板の厚みも常法に従う。大体0.3〜Q、5mm
程度の厚みのものを使用する。基板も従来から使用され
ている合板などが使用される。The conventional laminated decorative veneer used here can be used as is. Conventional wiping agents are also sufficient. The wiping process may be performed using a conventional method. The thickness of the laminated decorative veneer also follows the usual method. Approximately 0.3~Q, 5mm
Use one with a certain thickness. The board is also made of plywood, which has been used in the past.
銘木化粧板を製造するにはまず、集成化粧単板が用窓さ
れる。そして、基板に貼着される。つぎに第1次サンデ
ィングが施される。この場合200番ぐらいのサンドペ
ーパーが使用される。もっともサンドペーパーの使用に
限定する趣旨ではなく、サンディングが行えれば他の方
法でもよい。To manufacture decorative wood veneers, laminated decorative veneers are first processed. Then, it is attached to the substrate. Next, primary sanding is performed. In this case, approximately 200-grit sandpaper is used. However, the purpose is not to limit the use to sandpaper, and other methods may be used as long as sanding can be performed.
そしてサンドペーパーの番数も限定する趣旨ではない。And it is not the intention to limit the number of sandpapers.
このサンディングを行った面に前記の水溶性アクリル樹
脂エマルジョンを塗布する。この水溶性アクリル樹脂エ
マルジョンについては何等限定はしない。濃度も任意で
ある。その濃度あるいは所望される塗布厚みに応じて塗
布の条件を調節する。水溶性アクリル樹脂エマルジョン
の塗布の後は乾燥を行う。乾燥の条件も任意である。乾
燥後は第2次サンディングを行う。サンドペーパ−は2
00番ぐらいのものを使用する。もつともサンディング
について限定する趣旨ではない。The water-soluble acrylic resin emulsion described above is applied to the sanded surface. There are no limitations on this water-soluble acrylic resin emulsion. The concentration is also arbitrary. Coating conditions are adjusted depending on the concentration or desired coating thickness. After applying the water-soluble acrylic resin emulsion, it is dried. Drying conditions are also arbitrary. After drying, perform secondary sanding. Sandpaper is 2
Use something around number 00. This is not intended to limit sanding.
以上の前処理の後、通常のワイピング処理を施すのであ
る。つぎに実験例に基づき説明する。After the above pretreatment, a normal wiping process is performed. Next, explanation will be given based on an experimental example.
実験例 以下の表の内容で実験した。Experimental example I conducted an experiment using the contents in the table below.
なお、前記表の内、処理剤Aは水溶性アクリル樹脂エマ
ルジョンであり、それぞれ商品名を表示している。原料
単板の厚みはすべて0.3mであった。In the above table, processing agent A is a water-soluble acrylic resin emulsion, and the product name is indicated for each. The thickness of all raw material veneers was 0.3 m.
第1次サンディングは200番のサンドペーパーを使用
し、処理剤の塗布量は120〜150g/cdトシ、乾
燥はso”c、1時間、第2次サンディングは200番
のサンドペーパーを使用した。For the first sanding, No. 200 sandpaper was used, the amount of treatment agent applied was 120 to 150 g/cd, and the drying was at SO"C for 1 hour. For the second sanding, No. 200 sandpaper was used.
サンディングの後、従来の方法によりワイピングを行い
、無処理のスライス単板とのワイピングむらの差を比較
したところ実施例となるNo3,4.7,8で良好な結
果を得た。After sanding, wiping was performed by a conventional method, and when the difference in wiping unevenness was compared with that of an untreated sliced veneer, good results were obtained for Nos. 3, 4.7, and 8 as examples.
[効果]
この発明はワイピングを行う前に、基板に貼着した集成
化粧単板表面に水溶性アクリル樹脂エマルジョンを塗布
し、乾燥し、サンディング処理を施すことを特徴とする
のでワイピング時のワイピングむらが無くなると共に、
単板に硬質感が付加され、品質の良い銘木化粧板の製造
が可能になった。[Effects] This invention is characterized in that before wiping, a water-soluble acrylic resin emulsion is applied to the surface of the laminated decorative veneer adhered to the substrate, dried, and sanded, thereby reducing uneven wiping during wiping. As soon as the
A hard feel has been added to the veneer, making it possible to manufacture high-quality decorative wood veneers.
Claims (1)
理を施す工程を含む銘木化粧板を製造する方法において
、ワイピングを行う前に、基板に貼着した集成化粧単板
表面に水溶性アクリル樹脂エマルジョンを塗布し、乾燥
し、サンディング処理を施すことを特徴とする集成銘木
化粧板の製法。(1) In a method for manufacturing precious wood decorative veneers that includes a wiping process after pasting a laminated decorative veneer to a substrate, water-soluble adhesive is applied to the surface of the laminated decorative veneer adhered to the substrate before wiping. A method for producing laminated precious wood decorative boards, which is characterized by applying a synthetic acrylic resin emulsion, drying, and sanding.