JPS58180245A - コンクリ−ト等の静的破砕方法および膨張錠剤 - Google Patents
コンクリ−ト等の静的破砕方法および膨張錠剤Info
- Publication number
- JPS58180245A JPS58180245A JP6200782A JP6200782A JPS58180245A JP S58180245 A JPS58180245 A JP S58180245A JP 6200782 A JP6200782 A JP 6200782A JP 6200782 A JP6200782 A JP 6200782A JP S58180245 A JPS58180245 A JP S58180245A
- Authority
- JP
- Japan
- Prior art keywords
- crushing
- agent
- concrete
- hole
- static
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Disintegrating Or Milling (AREA)
- Piles And Underground Anchors (AREA)
- Working Measures On Existing Buildindgs (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6200782A JPS58180245A (ja) | 1982-04-14 | 1982-04-14 | コンクリ−ト等の静的破砕方法および膨張錠剤 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6200782A JPS58180245A (ja) | 1982-04-14 | 1982-04-14 | コンクリ−ト等の静的破砕方法および膨張錠剤 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS58180245A true JPS58180245A (ja) | 1983-10-21 |
| JPH0148059B2 JPH0148059B2 (cs) | 1989-10-17 |
Family
ID=13187662
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP6200782A Granted JPS58180245A (ja) | 1982-04-14 | 1982-04-14 | コンクリ−ト等の静的破砕方法および膨張錠剤 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS58180245A (cs) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5945379A (ja) * | 1982-09-07 | 1984-03-14 | Denki Kagaku Kogyo Kk | 破砕剤及びそれを用いた破砕工法 |
| JPS6013172A (ja) * | 1983-07-04 | 1985-01-23 | 旭化成株式会社 | コンクリ−ト等の静的破砕方法および膨張錠剤 |
| JPS62195074A (ja) * | 1986-02-21 | 1987-08-27 | Ube Ind Ltd | 静的破砕剤およびその製造方法 |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4943416A (cs) * | 1972-08-31 | 1974-04-24 | ||
| JPS5667059A (en) * | 1979-11-01 | 1981-06-05 | Onoda Cement Co Ltd | Destroying agent for brittle matter |
-
1982
- 1982-04-14 JP JP6200782A patent/JPS58180245A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4943416A (cs) * | 1972-08-31 | 1974-04-24 | ||
| JPS5667059A (en) * | 1979-11-01 | 1981-06-05 | Onoda Cement Co Ltd | Destroying agent for brittle matter |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5945379A (ja) * | 1982-09-07 | 1984-03-14 | Denki Kagaku Kogyo Kk | 破砕剤及びそれを用いた破砕工法 |
| JPS6013172A (ja) * | 1983-07-04 | 1985-01-23 | 旭化成株式会社 | コンクリ−ト等の静的破砕方法および膨張錠剤 |
| US4600154A (en) * | 1983-07-04 | 1986-07-15 | Asahi Kasei Kogyo Kabushiki Kaisha | Static expansive demolition agent in the three-dimensional form and process for demolishing brittle material using the same |
| JPS62195074A (ja) * | 1986-02-21 | 1987-08-27 | Ube Ind Ltd | 静的破砕剤およびその製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0148059B2 (cs) | 1989-10-17 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| IE792109L (en) | Composite material. | |
| MXPA97002294A (en) | Compacted units of ceme mixes | |
| US3723338A (en) | Method of reducing the release of mobile contaminants from granular solids | |
| JPS58180245A (ja) | コンクリ−ト等の静的破砕方法および膨張錠剤 | |
| DE2531056C3 (de) | Verfahren zum Verfestigen einer radioaktive oder toxische Abfallstoffe enthaltenden wäßrigen Lösung | |
| JPS6013172A (ja) | コンクリ−ト等の静的破砕方法および膨張錠剤 | |
| CH662123A5 (it) | Composizione per l'immobilizzazione di residui radioattivi ed impiego della composizione. | |
| DE3833676A1 (de) | Verfahren zur endlagerung von eingebundenen abfallstoffen | |
| KR950001707B1 (ko) | 팽창성 파쇄제 | |
| Le Bescop et al. | Immobilization in cement of ion exchange resins | |
| KR20090080713A (ko) | 방사성 폐기물 과립화 방법 및 처리장치 | |
| JP2001097757A (ja) | ほう酸用セメント固化材、ほう酸のセメント固化方法及びセメント固化体 | |
| JPS5815000B2 (ja) | 放射性廃棄物処理方法 | |
| US5180542A (en) | Container | |
| DE29513889U1 (de) | Recyclingfähiger Leichtbaustoff aus nachwachsenden Rohstoffen | |
| DE814453C (de) | Presslinge aus Bodenverbesserungsmitteln | |
| Lotspeich | Strength and bulk density of compacted mixtures of kaolinite and glass beads | |
| Iwashita et al. | Micro-deformation mechanism of shear banding process based on numerical simulation analyses. | |
| JPS5528858A (en) | Method of producing ornament | |
| JPS62131082A (ja) | 静的破砕方法 | |
| Tvergaard et al. | Fatigue crack evolution in a metal reinforced by short fibres | |
| JPS62179585A (ja) | 静的破砕剤 | |
| JPH0261992B2 (cs) | ||
| JPS6081277A (ja) | 静的破砕方法および静的破砕用膨脹性錠剤 | |
| DE516594C (de) | Verfahren zum Entwickeln von Blausaeure aus Erdalkalicyanverbindungen, insbesondere zu Zwecken der Schaedlingsbekaempfung |