JPS57177924A - Improving method for residual stress on both surfaces - Google Patents
Improving method for residual stress on both surfacesInfo
- Publication number
- JPS57177924A JPS57177924A JP6338381A JP6338381A JPS57177924A JP S57177924 A JPS57177924 A JP S57177924A JP 6338381 A JP6338381 A JP 6338381A JP 6338381 A JP6338381 A JP 6338381A JP S57177924 A JPS57177924 A JP S57177924A
- Authority
- JP
- Japan
- Prior art keywords
- pipe
- internal pressure
- residual stress
- cooling
- ice
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To eliminate the variance in the effect after execution of a freezing method for the purpose of improving the residual stress on the inside surface of plant pipings and tubular vessels in said method by combining quick heating for the pipe with the stopping of the cooling upon arrival of the intended internal pressure, thereby quickly dropping the pressure in the pipe. CONSTITUTION:The internal pressure in the section W enclosed by the two ice plugs I1, I2 in a pipe T is increased by the growth of the ice to deform the pipe T plastically, whereby a residual stress state is improved. Upon arrival of said internal pressure at the prescribed internal pressure at this time, the cooling is stopped; at the same time, electric current is conducted between the ring-like electrodes E and E mounted on the outer side in the cooling section J-J, that is, the pipe T, so that Joule heat is evolved. The pipe diameter is expanded by the thermal expansion caused by this quick heating of the pipe; at the same time, the binding force of the ice plugs to the pipe wall is decreased by the temp. elevation of the pipe wall and the internal pressure of the pipe is reduced quickly.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6338381A JPS57177924A (en) | 1981-04-28 | 1981-04-28 | Improving method for residual stress on both surfaces |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6338381A JPS57177924A (en) | 1981-04-28 | 1981-04-28 | Improving method for residual stress on both surfaces |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS57177924A true JPS57177924A (en) | 1982-11-01 |
JPS6235458B2 JPS6235458B2 (en) | 1987-08-01 |
Family
ID=13227714
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6338381A Granted JPS57177924A (en) | 1981-04-28 | 1981-04-28 | Improving method for residual stress on both surfaces |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS57177924A (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE3507293A1 (en) * | 1984-03-14 | 1985-09-26 | Voest-Alpine Ag, Linz | METHOD FOR INCREASING THE STRENGTH OF SINGLE-WALLED TUBULAR COMPONENTS, AND APPARATUS FOR CARRYING OUT THIS METHOD |
JP2005320626A (en) * | 2004-04-06 | 2005-11-17 | Hitachi Ltd | Heat treatment method and apparatus therefor |
US7565812B2 (en) | 2005-05-31 | 2009-07-28 | Hitachi-Ge Nuclear Energy, Ltd. | Method for improving residual stress in pipe and apparatus |
-
1981
- 1981-04-28 JP JP6338381A patent/JPS57177924A/en active Granted
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE3507293A1 (en) * | 1984-03-14 | 1985-09-26 | Voest-Alpine Ag, Linz | METHOD FOR INCREASING THE STRENGTH OF SINGLE-WALLED TUBULAR COMPONENTS, AND APPARATUS FOR CARRYING OUT THIS METHOD |
JP2005320626A (en) * | 2004-04-06 | 2005-11-17 | Hitachi Ltd | Heat treatment method and apparatus therefor |
US7565812B2 (en) | 2005-05-31 | 2009-07-28 | Hitachi-Ge Nuclear Energy, Ltd. | Method for improving residual stress in pipe and apparatus |
US7866166B2 (en) | 2005-05-31 | 2011-01-11 | Hitachi-Ge Nuclear Energy, Ltd. | Method for improving residual stress in pipe and apparatus |
Also Published As
Publication number | Publication date |
---|---|
JPS6235458B2 (en) | 1987-08-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5516758A (en) | Frictional pressure welding of small-thickness pipe | |
JPS57177924A (en) | Improving method for residual stress on both surfaces | |
EP0196243A3 (en) | Temperature gradient furnace for materials processing | |
BR9707971A (en) | Socket forming method in a biaxially oriented polyvinyl chloride tubing | |
JPS5775296A (en) | Method for improving residual stress of welded joint part of pipe | |
JPS52130409A (en) | Generating method for residual stress on the inner and outer surfaces of pipe | |
JPS57175094A (en) | Improving method for residual stress in welded joint part of pipes | |
JPS5775281A (en) | Soldering method of pipe joint | |
CN218543451U (en) | Stainless steel water pipe with heat preservation structure | |
CN215215238U (en) | PE pipe convenient to install heat preservation assembly | |
JPS5715193A (en) | Heat insulation pipings for high temperature and high pressure , and its connecting method | |
GB858121A (en) | Pipe couplings | |
JPS5733933A (en) | Manufacture of conveying roller for high temperature object | |
JPS5575890A (en) | Friction pressure welding method of copper pipe and aluminum pipe | |
SU1099177A1 (en) | Method of cryogenic pipeline heat insulation | |
JPS53117813A (en) | High temperature and high pressure piping | |
JPS5699060A (en) | Roll for continuous casting and its manufacture | |
FR2323871A1 (en) | Device for heating or cooling turbine casing joint bolts - uses hollow bodies fitted around bolt shanks to reduce thermal stresses | |
JPS5336721A (en) | Metal pipe having grooves on both surfaces and its preparation method | |
JPS51147051A (en) | The heat pipe manufacturing method | |
SU1514806A1 (en) | Device for heating annular articles | |
JPS56102042A (en) | Encapsulating method for bulb | |
JPS5671534A (en) | Press-fixing of pipe end face | |
JPS5292948A (en) | Cool maintenace method for low temp. piping etc. | |
FR2427441A1 (en) | Thermal insulating clip for metal insulated wall - has metal clips crimped over thermal insulating material blocks to block heat flow path |