JPS57154622A - Magnetic recording medium - Google Patents
Magnetic recording mediumInfo
- Publication number
- JPS57154622A JPS57154622A JP4130281A JP4130281A JPS57154622A JP S57154622 A JPS57154622 A JP S57154622A JP 4130281 A JP4130281 A JP 4130281A JP 4130281 A JP4130281 A JP 4130281A JP S57154622 A JPS57154622 A JP S57154622A
- Authority
- JP
- Japan
- Prior art keywords
- recording medium
- magnetic recording
- magnetic
- perfluoroalkylphosphate
- fluoroplastics
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To improve the durability and the antistatic properties, by allowing a magnetic layer to contain fine powder of fluoroplastics and perfluoroalkylphosphate. CONSTITUTION:Fine powder of fluoroplastics consisting of polytetrafluoroethylene, polyhexafluoropropylene, polytrichlorofluoroethylene, or the like and a perfluoroalkylphosphate which has the surface activity function and is conductive and lubricative are used to make up a magnetic paint, and this magnetic paint is applied and dried on a base material to obtain a magnetic recording medium.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4130281A JPH0248976B2 (en) | 1981-03-20 | 1981-03-20 | JIKIKIROKUBAITAI |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4130281A JPH0248976B2 (en) | 1981-03-20 | 1981-03-20 | JIKIKIROKUBAITAI |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS57154622A true JPS57154622A (en) | 1982-09-24 |
JPH0248976B2 JPH0248976B2 (en) | 1990-10-26 |
Family
ID=12604673
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP4130281A Expired - Lifetime JPH0248976B2 (en) | 1981-03-20 | 1981-03-20 | JIKIKIROKUBAITAI |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH0248976B2 (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6415782A (en) * | 1987-07-10 | 1989-01-19 | Canon Kk | Fixing device |
-
1981
- 1981-03-20 JP JP4130281A patent/JPH0248976B2/en not_active Expired - Lifetime
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6415782A (en) * | 1987-07-10 | 1989-01-19 | Canon Kk | Fixing device |
Also Published As
Publication number | Publication date |
---|---|
JPH0248976B2 (en) | 1990-10-26 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
FR2347986A1 (en) | IMPROVEMENTS FOR THE CONTINUOUS APPLICATION OF POWDER ON CONDUCTIVE AND NON-CONDUCTIVE SUBSTRATES | |
ES548583A0 (en) | PROCEDURE TO FORM AN ADHERENT COATING OF CERAMIC ELECTRO-CATALYTIC MATERIAL ON THE SURFACE OF AN INERT METALLIC SUBSTRATE | |
AU562407B2 (en) | X-y position detector | |
JPS57154622A (en) | Magnetic recording medium | |
JPS57154621A (en) | Magnetic recording medium | |
JPS57154624A (en) | Magnetic recording medium | |
JPS57154623A (en) | Magnetic recording medium | |
JPS5331067A (en) | Sprayer of lubricating material and the like | |
JPS57154619A (en) | Magnetic recording medium | |
JPS5238196A (en) | Electrode coating material | |
JPS57176533A (en) | Magnetic recording medium | |
JPS53128683A (en) | Polyester film having modified surface | |
JPS5439480A (en) | Sliding material | |
DE2966777D1 (en) | Tribological systems composed of sliding surfaces consisting of plastics | |
JPS5419199A (en) | Magnetic recording medium porcess | |
JPS57154625A (en) | Magnetic recording medium | |
JPS57154620A (en) | Magnetic recording medium | |
JPS5290508A (en) | Method of forming fine antiioxidizing silicon carbide coating on carbon material surfaces | |
JPS5266986A (en) | Manufacturing of symmetrical type voltage non-linear resistor | |
JPS5259388A (en) | Grinding tool | |
JPS544940A (en) | Friction material | |
JPS51115842A (en) | Mirror capable of optionally varying curvature | |
SU601293A1 (en) | Antiadhesive composition of rubber and rubber compound crumb | |
JPS5222793A (en) | Resister material | |
JPS5439472A (en) | Sliding material |