JPS5699077A - Method of coupling bottom plate of cylindrical tank - Google Patents

Method of coupling bottom plate of cylindrical tank

Info

Publication number
JPS5699077A
JPS5699077A JP279580A JP279580A JPS5699077A JP S5699077 A JPS5699077 A JP S5699077A JP 279580 A JP279580 A JP 279580A JP 279580 A JP279580 A JP 279580A JP S5699077 A JPS5699077 A JP S5699077A
Authority
JP
Japan
Prior art keywords
open air
bottom plate
cylindrical tank
rainwater
tape
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP279580A
Other languages
Japanese (ja)
Other versions
JPS6325872B2 (en
Inventor
Shizuo Saburi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toyo Kanetsu KK
Original Assignee
Toyo Kanetsu KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toyo Kanetsu KK filed Critical Toyo Kanetsu KK
Priority to JP279580A priority Critical patent/JPS5699077A/en
Publication of JPS5699077A publication Critical patent/JPS5699077A/en
Publication of JPS6325872B2 publication Critical patent/JPS6325872B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE: To realize a method of coupling that forms a sound weld zone by adhering a tape to the welding line of a bottom plate and its circumference and then by insulating the joint part from water and the open air by further coating the tape.
CONSTITUTION: Bottom plates 1 of a cylindrical tank are arrayed successively and after circumferences of welding lines are cleaned, tapes 2 are adhered there and then coated 3 to cover tapes 2 sufficiently. Thus, butt groove 4 or weld overlap part is insulated from rainwater and the open air and adjacent joint parts are welded successively. This method provides the nearly perfect protection of the welding grooves against the rainwater and open air and sound weld zones can be obtained.
COPYRIGHT: (C)1981,JPO&Japio
JP279580A 1980-01-14 1980-01-14 Method of coupling bottom plate of cylindrical tank Granted JPS5699077A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP279580A JPS5699077A (en) 1980-01-14 1980-01-14 Method of coupling bottom plate of cylindrical tank

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP279580A JPS5699077A (en) 1980-01-14 1980-01-14 Method of coupling bottom plate of cylindrical tank

Publications (2)

Publication Number Publication Date
JPS5699077A true JPS5699077A (en) 1981-08-10
JPS6325872B2 JPS6325872B2 (en) 1988-05-27

Family

ID=11539299

Family Applications (1)

Application Number Title Priority Date Filing Date
JP279580A Granted JPS5699077A (en) 1980-01-14 1980-01-14 Method of coupling bottom plate of cylindrical tank

Country Status (1)

Country Link
JP (1) JPS5699077A (en)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2015080353A1 (en) * 2013-11-26 2015-06-04 한국지질자원연구원 High-pressure fluid storage tank and construction method thereof
WO2015080354A1 (en) * 2013-11-26 2015-06-04 한국지질자원연구원 High-pressure fluid storage system and construction method therefor
CN105934554A (en) * 2013-11-26 2016-09-07 韩国地质资源研究院 High-pressure fluid storage tank and construction method thereof

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2015080353A1 (en) * 2013-11-26 2015-06-04 한국지질자원연구원 High-pressure fluid storage tank and construction method thereof
WO2015080354A1 (en) * 2013-11-26 2015-06-04 한국지질자원연구원 High-pressure fluid storage system and construction method therefor
CN105934554A (en) * 2013-11-26 2016-09-07 韩国地质资源研究院 High-pressure fluid storage tank and construction method thereof
CN105940169A (en) * 2013-11-26 2016-09-14 韩国地质资源研究院 High-pressure fluid storage system and construction method therefor

Also Published As

Publication number Publication date
JPS6325872B2 (en) 1988-05-27

Similar Documents

Publication Publication Date Title
AU5951880A (en) Corrosion resistant pipe joint
GB2072289B (en) Flanged pipe joint
JPS5699077A (en) Method of coupling bottom plate of cylindrical tank
GB2130522B (en) Coating of welded pipe joints
GB2055658B (en) Apparatus for resistant butt welding of pipes
AU552048B2 (en) Butt welding pipes
NO874912D0 (en) MACHINE FOR MELTING WELDING OF PIPE PIPES.
AU5070479A (en) Joining pipes under water
AU540434B2 (en) Butt welding of pipes
AU554626B2 (en) Solid phase welding of pipes
JPS57107495A (en) Repairing method of pipe
EP0033350B1 (en) Method for the preparation of improved water and solvent resistant coated substrates
JPS56150688A (en) Joining method of metallic pipes mutually
JPS53119241A (en) Welding method for slightly weldable materials and dehydrogenation apparatus welding
JPS5783779A (en) Joining method of inner face installing type pipe joint
JPS5715185A (en) Flexible joining method of pipe culvert
RU841479C (en) Method of monitoring quality of welded joint
JPS57204387A (en) Method of joining pipe material
JPS51120429A (en) Method for repairing joints of coated steel pipe
JPS5633918A (en) Corrosion preventing method of joint of plastic-coated steel pipe
AU539614B2 (en) Removing flash from the inside surface of welded pipes
JPS579387A (en) Joining method of pipe
JPS5733281A (en) Corrosion preventing method of service pipe
JPS5356133A (en) Method of preventing corrosion of outer surface of weld joints of steel pipes
JPS57110893A (en) Joining method of earthenware pipe