JPS56119895A - Method of protecting stress corrosion crack of nuclear reactor pipe - Google Patents
Method of protecting stress corrosion crack of nuclear reactor pipeInfo
- Publication number
- JPS56119895A JPS56119895A JP1512280A JP1512280A JPS56119895A JP S56119895 A JPS56119895 A JP S56119895A JP 1512280 A JP1512280 A JP 1512280A JP 1512280 A JP1512280 A JP 1512280A JP S56119895 A JPS56119895 A JP S56119895A
- Authority
- JP
- Japan
- Prior art keywords
- nuclear reactor
- stress corrosion
- reactor pipe
- corrosion crack
- protecting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E30/00—Energy generation of nuclear origin
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1512280A JPS56119895A (en) | 1980-02-08 | 1980-02-08 | Method of protecting stress corrosion crack of nuclear reactor pipe |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1512280A JPS56119895A (en) | 1980-02-08 | 1980-02-08 | Method of protecting stress corrosion crack of nuclear reactor pipe |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS56119895A true JPS56119895A (en) | 1981-09-19 |
JPS6151757B2 JPS6151757B2 (en) | 1986-11-10 |
Family
ID=11880008
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP1512280A Granted JPS56119895A (en) | 1980-02-08 | 1980-02-08 | Method of protecting stress corrosion crack of nuclear reactor pipe |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS56119895A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0442390U (en) * | 1990-08-01 | 1992-04-10 |
-
1980
- 1980-02-08 JP JP1512280A patent/JPS56119895A/en active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0442390U (en) * | 1990-08-01 | 1992-04-10 |
Also Published As
Publication number | Publication date |
---|---|
JPS6151757B2 (en) | 1986-11-10 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
YU96482A (en) | Framework for placing used up fuel of nuclear reactor | |
GB2147730B (en) | Method and apparatus for determining the nearness to criticality of a nuclear reactor | |
JPS57131096A (en) | Method of operating nuclear reactor | |
DE3269674D1 (en) | Rail apparatus around nuclear reactor pressure vessel and method of installing the same | |
JPS56119895A (en) | Method of protecting stress corrosion crack of nuclear reactor pipe | |
JPS573086A (en) | Method of operating nuclear reactor | |
JPS56147097A (en) | Method of protecting stress corrosion crack in pipe | |
JPS57107495A (en) | Repairing method of pipe | |
JPS56157896A (en) | Method of building bwr type reactor | |
JPS56141592A (en) | Method of building nuclear reactor plant | |
JPS56141593A (en) | Method of building nuclear reactor having prestressed concrete pressure vessel | |
JPS56145395A (en) | Method of cleaning nuclear reactor pipeline | |
JPS56162093A (en) | Method of installing nuclear reactor pressure vessel | |
JPS5737190A (en) | Corrosion protective sealing of pipes | |
JPS56137277A (en) | Method of dismounting radioactive nuclear reactor shield | |
JPS5783786A (en) | Repairing method of leaked pipe | |
GB2022615B (en) | Protecting austenitic stainless steel from stress corrosion cracking | |
JPS5733281A (en) | Corrosion preventing method of service pipe | |
JPS57148287A (en) | Method of building nuclear reactor building | |
JPS5790197A (en) | Method of removing clad in seal bellow portion of nuclear reactor | |
JPS5790484A (en) | Lifting method of long sized riser pipe of submarine pipeline | |
JPS56101596A (en) | Corrosion protecting method and device of coolant feedwater system in nuclear reactor | |
JPS54116286A (en) | Method of checking steel pipe | |
JPS5794694A (en) | Method of detecting nuclear fuel failure | |
JPS57151892A (en) | Method of carrying nuclear reactor pressure vessel |