JPS5589831A - Nonsilver photosensitive film - Google Patents
Nonsilver photosensitive filmInfo
- Publication number
- JPS5589831A JPS5589831A JP16542978A JP16542978A JPS5589831A JP S5589831 A JPS5589831 A JP S5589831A JP 16542978 A JP16542978 A JP 16542978A JP 16542978 A JP16542978 A JP 16542978A JP S5589831 A JPS5589831 A JP S5589831A
- Authority
- JP
- Japan
- Prior art keywords
- powder
- film
- nonsilver
- photosensitive
- abrasion resistance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To simply enhance the abrasion resistance of a nonsilver photosensitive film without deteriorating the developability by adhering solid powder to the film surface. CONSTITUTION:On a photosensitive film formed by coating a support made of polyester or the like with a photosensitive nonsilver composition, heat fusible powder of a solid single substance or composition whose primary or secondary transition point is lower than the primary transition point of the film is spread, and the powder surface is adhered to the film surface by partial fusion or dissolution in the residual solvent of the film, or other method. Powder having solubility in low b.p. solvent and suitable for fusion bonding and a matting agent such as silica or alumina may be used in place of the above-mentioned powder. The diameter of the powder is preferably 1-17mu and esp. preferably 1-8mu. 1-1,000, preferably 5-500 particles of the powder are used per m<2> of the film. Thus, the abrasion resistance of the film is enhanced, the vacuum contact time is shorten, and the degree of exhausting a developer is lowered.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16542978A JPS5589831A (en) | 1978-12-27 | 1978-12-27 | Nonsilver photosensitive film |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16542978A JPS5589831A (en) | 1978-12-27 | 1978-12-27 | Nonsilver photosensitive film |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5589831A true JPS5589831A (en) | 1980-07-07 |
Family
ID=15812251
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP16542978A Pending JPS5589831A (en) | 1978-12-27 | 1978-12-27 | Nonsilver photosensitive film |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5589831A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6392005B1 (en) | 2001-03-19 | 2002-05-21 | Nan Ya Plastics Corporation | Manufacturing method for decreasing the cyclic oligomer content in polyester |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS50125805A (en) * | 1974-03-19 | 1975-10-03 | ||
JPS5198505A (en) * | 1975-02-25 | 1976-08-30 | Kankoseihanzaino seihanhoho | |
JPS538128A (en) * | 1976-07-09 | 1978-01-25 | Fuji Photo Film Co Ltd | Photosolubilizable composition |
-
1978
- 1978-12-27 JP JP16542978A patent/JPS5589831A/en active Pending
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS50125805A (en) * | 1974-03-19 | 1975-10-03 | ||
JPS5198505A (en) * | 1975-02-25 | 1976-08-30 | Kankoseihanzaino seihanhoho | |
JPS538128A (en) * | 1976-07-09 | 1978-01-25 | Fuji Photo Film Co Ltd | Photosolubilizable composition |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6392005B1 (en) | 2001-03-19 | 2002-05-21 | Nan Ya Plastics Corporation | Manufacturing method for decreasing the cyclic oligomer content in polyester |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES539118A0 (en) | PROCEDURE FOR THE OBTAINING OF A PLASTIC WATER DISPLAYING MATERIAL. | |
CA1154993A (en) | Prolonged tack toners including an organic polymer, solid plasticizer, conductive metal particles and glass frit | |
JPS5734995A (en) | Heat sensitive recording material | |
JPS5589831A (en) | Nonsilver photosensitive film | |
JPS52133339A (en) | Latent adhesive and its production | |
NO980861L (en) | Granules with rice performance and based on organic acids, process for preparation, and use | |
JPS542741A (en) | Pressure fixing toner | |
JPS5379371A (en) | Manufacture for plasma display panel | |
JPS5319981A (en) | Functional organic material | |
JPS5367706A (en) | Method of cleaning and cleaning agent | |
JPS5372049A (en) | Remoistening adhesive for adhering house furnishing base materials | |
JPS555953A (en) | Remoistening adhesive paper | |
JPS54136632A (en) | Hermetically sealed container | |
JPS5556335A (en) | Manufacturing method of fluorescent lamp | |
JPS55146419A (en) | Display device | |
JPS53142487A (en) | Method of adhering polyester material to rubber | |
JPS5249095A (en) | Method of forming protecting film for gas sensing body | |
JPS5216547A (en) | Bottle holder for electrostatic powder coating of glass bottle for car bonated beverage | |
JPS5432818A (en) | Anti-corrosion coating process for pipe joint part | |
NO905613L (en) | PROCEDURE FOR THE PREPARATION OF FLAMMABLE EXPANDABLE VINYLAROMATIC POLYMER PARTICLES CONTAINING HEXABROMOSYCLODODEKAN. | |
JPS5428629A (en) | Liquid developer for electrostatic latent lmages | |
JPS5226835A (en) | Electrophotographic fixing method | |
JPS5234580A (en) | Method for adhering glass material and base material to construct glas s electric bulb | |
ES2073586T3 (en) | METHOD FOR THE CONFIGURATION OF INDICATIONS. | |
JPS51127673A (en) | Manufacturing process of fluorescent indicator tube |