JPS5568179A - Plasma arc starting method - Google Patents

Plasma arc starting method

Info

Publication number
JPS5568179A
JPS5568179A JP13986978A JP13986978A JPS5568179A JP S5568179 A JPS5568179 A JP S5568179A JP 13986978 A JP13986978 A JP 13986978A JP 13986978 A JP13986978 A JP 13986978A JP S5568179 A JPS5568179 A JP S5568179A
Authority
JP
Japan
Prior art keywords
current
gas
arc
time
main
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP13986978A
Other languages
Japanese (ja)
Inventor
Minoru Shimada
Yuji Obara
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Via Mechanics Ltd
Original Assignee
Hitachi Seiko Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hitachi Seiko Ltd filed Critical Hitachi Seiko Ltd
Priority to JP13986978A priority Critical patent/JPS5568179A/en
Publication of JPS5568179A publication Critical patent/JPS5568179A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To suppress the production of double arcs at the starting of main arc and prevent damaging of nozzle by adding dissimilar operating gas after the start of the plasma arc produced in the operating gas flow.
CONSTITUTION: Operating gas PG is beforehand supplied and a main arc 4 is produced at the welding work start point a. While the main current thereof is being detected, the current is shifted from the cutting start current Ip1 of small current to plasma cutting main current Ip. This current shifting involves increasing the current from the current Ip1 to the current Ip during the slow up time Ta and this time Ta is arbitrarily variable. For the gas PG, the operating gas of the same gas is supplied as the initial operating gas PG1 and at the time a, the second operating gases PG2 and PG3' are increased within the shift mode range of the time Ta. Namely, the gas PG is increased in the small current region and therefore rapid unstabilizing of the arc is obviated and the stable main arc shifting and the prevention of the formation of double arcs 6, 6' are accomplished. In the figure, 1 denotes a torch, 2 an electrode, 3 a base metal and 5 a nozzle, respectively.
COPYRIGHT: (C)1980,JPO&Japio
JP13986978A 1978-11-15 1978-11-15 Plasma arc starting method Pending JPS5568179A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP13986978A JPS5568179A (en) 1978-11-15 1978-11-15 Plasma arc starting method

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP13986978A JPS5568179A (en) 1978-11-15 1978-11-15 Plasma arc starting method

Publications (1)

Publication Number Publication Date
JPS5568179A true JPS5568179A (en) 1980-05-22

Family

ID=15255441

Family Applications (1)

Application Number Title Priority Date Filing Date
JP13986978A Pending JPS5568179A (en) 1978-11-15 1978-11-15 Plasma arc starting method

Country Status (1)

Country Link
JP (1) JPS5568179A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2009095843A (en) * 2007-10-15 2009-05-07 Daihen Corp Method of controlling arc start in plasma arc welding

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS4931562A (en) * 1972-07-25 1974-03-22
JPS53119252A (en) * 1977-03-29 1978-10-18 Origin Electric Plasma arc cutting start method

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS4931562A (en) * 1972-07-25 1974-03-22
JPS53119252A (en) * 1977-03-29 1978-10-18 Origin Electric Plasma arc cutting start method

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2009095843A (en) * 2007-10-15 2009-05-07 Daihen Corp Method of controlling arc start in plasma arc welding

Similar Documents

Publication Publication Date Title
JPS56131071A (en) All position tig welding method
JPS5788972A (en) Two electrode arc welding method
CA2330069A1 (en) Method and apparatus for improving plasma arc consumable life
JPS5568179A (en) Plasma arc starting method
JPS5527417A (en) Vertical downward build-up welding method
JPS55117575A (en) Arc welding method
JPS555125A (en) Plasma arc build-up welding method by powder metals or other
SU1699739A1 (en) Method of consumable electrode multiarc welding
JPS56144865A (en) Surface hardening build-up welding method
JPS5554271A (en) Arc starting method in dcsp-tig welding of aluminum material
JPS55120481A (en) Multielectrode welding method
SU659325A1 (en) Method of tuning the operating duty at plasma-arc welding
JPS57165174A (en) Arc starting method
JPS5533833A (en) High speed inclined position submerged arc welding method
JPS5420932A (en) High speed welding method
JPS54110947A (en) Reverse polar plasma arc padding welding
JPS54159361A (en) Preventing method for crack at starting point and toe of weld in mig welding
JPS52147513A (en) Smelting method of low nitrogen steel at steel making arc furnace
JPS53131242A (en) Inert gas arc welding method and welding nozzle
JPS546830A (en) Tig arc welding method
SU572353A1 (en) Method of plasma-arc surface cutting
JPS53124146A (en) Plasma welding method for high nickel steel
JPS5577976A (en) Pulse arc welding method
JPS57209778A (en) Gas shielded arc welding method
JPS5645266A (en) Gas fusion cutting starting method