JPS5561377A - Preventing method for occurrence of cracking in one side butt welding with backing strip - Google Patents

Preventing method for occurrence of cracking in one side butt welding with backing strip

Info

Publication number
JPS5561377A
JPS5561377A JP13238578A JP13238578A JPS5561377A JP S5561377 A JPS5561377 A JP S5561377A JP 13238578 A JP13238578 A JP 13238578A JP 13238578 A JP13238578 A JP 13238578A JP S5561377 A JPS5561377 A JP S5561377A
Authority
JP
Japan
Prior art keywords
backing
butt welding
cracking
backing strip
occurrence
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP13238578A
Other languages
Japanese (ja)
Inventor
Hiroshi Sumita
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toyo Kanetsu KK
Original Assignee
Toyo Kanetsu KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toyo Kanetsu KK filed Critical Toyo Kanetsu KK
Priority to JP13238578A priority Critical patent/JPS5561377A/en
Publication of JPS5561377A publication Critical patent/JPS5561377A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To prevent the occurrence of the captioned cracking by inserting a thin strap between the base metals of the backing strip joint part and backing strips.
CONSTITUTION: Backing strips 3, 3' are positioned slender in the joint direction on the back side of the one side butt welding face of base metals 1, 1'. In the butt portion of the backing strips 3, 3', a thin strap 4 whose top outside circumference is beveled 4' to taper form and whose width is approximately the same as that of th backing strips 3, 3' is so inserted between the base metals 1, 1' and backing stips 3, 3' of the backing strip joint part that it lays across both ends of the backing strips 3, 3'. After the discontinuous parts of the backing strip joint part is repaired, the one side butt welding face of the base metals 1, 1' is welded.
COPYRIGHT: (C)1980,JPO&Japio
JP13238578A 1978-10-27 1978-10-27 Preventing method for occurrence of cracking in one side butt welding with backing strip Pending JPS5561377A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP13238578A JPS5561377A (en) 1978-10-27 1978-10-27 Preventing method for occurrence of cracking in one side butt welding with backing strip

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP13238578A JPS5561377A (en) 1978-10-27 1978-10-27 Preventing method for occurrence of cracking in one side butt welding with backing strip

Publications (1)

Publication Number Publication Date
JPS5561377A true JPS5561377A (en) 1980-05-09

Family

ID=15080141

Family Applications (1)

Application Number Title Priority Date Filing Date
JP13238578A Pending JPS5561377A (en) 1978-10-27 1978-10-27 Preventing method for occurrence of cracking in one side butt welding with backing strip

Country Status (1)

Country Link
JP (1) JPS5561377A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR100634626B1 (en) 2004-11-09 2006-10-16 대우조선해양 주식회사 End-Cracking prevention method for one side automatic butt welding by using chill blocks

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR100634626B1 (en) 2004-11-09 2006-10-16 대우조선해양 주식회사 End-Cracking prevention method for one side automatic butt welding by using chill blocks

Similar Documents

Publication Publication Date Title
JPS5561377A (en) Preventing method for occurrence of cracking in one side butt welding with backing strip
JPS52132485A (en) Drum type flying shear
JPS53149149A (en) Diffusion welding method
JPS53106359A (en) Preventing method for transverse crack in backing strip weld zone
JPS5516754A (en) Welding box pillar by consumed nozzle
JPS56126076A (en) Tig welding method
JPS5315206A (en) Turning over apparatus for steel pieces
JPS56167802A (en) Repairing method of nozzle blade for steam turbine
JPS53113237A (en) Method of forming welding end
JPS56126092A (en) Butt welding method
JPS53113209A (en) Method of preventing scale flaw of alloy steel slab at heating
JPS5372945A (en) Stay-vane in hydraulic turbine stay ring and main plate weld groove
JPS53128548A (en) Method of preventing corrosion of clearance between joined surfaces
JPS571578A (en) Welding method for austenite stainless steel
JPS52132484A (en) Drum type flying shear
JPS52132486A (en) Drum type flying shear
JPS5527449A (en) Tentative fixing method in o press in uo pipe making method
JPS5421939A (en) Automatic butt welding apparatus
JPS54137446A (en) Welding of thick steel plate
Klein Know How--Some Rules About Metal Active Gas Welding
JPS53118259A (en) Continuous cold rolling mill
JPS53131941A (en) Method of forming gap of thick pipe welded portion
van Berlekom What Must be Considered in Submerged-Arc Welding of Corrosion Resistant Austenitic Steels?
JPS5397404A (en) Endless tape
JPS5714474A (en) One-side welding method