JPS5543051B2 - - Google Patents
Info
- Publication number
- JPS5543051B2 JPS5543051B2 JP5547375A JP5547375A JPS5543051B2 JP S5543051 B2 JPS5543051 B2 JP S5543051B2 JP 5547375 A JP5547375 A JP 5547375A JP 5547375 A JP5547375 A JP 5547375A JP S5543051 B2 JPS5543051 B2 JP S5543051B2
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP5547375A JPS51131417A (en) | 1975-05-13 | 1975-05-13 | Process for producing nitrogen- containing low alloy steel material ha ving excellent toughness |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP5547375A JPS51131417A (en) | 1975-05-13 | 1975-05-13 | Process for producing nitrogen- containing low alloy steel material ha ving excellent toughness |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS51131417A JPS51131417A (en) | 1976-11-15 |
| JPS5543051B2 true JPS5543051B2 (enExample) | 1980-11-04 |
Family
ID=12999565
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP5547375A Granted JPS51131417A (en) | 1975-05-13 | 1975-05-13 | Process for producing nitrogen- containing low alloy steel material ha ving excellent toughness |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS51131417A (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0756046B2 (ja) * | 1989-04-08 | 1995-06-14 | 株式会社神戸製鋼所 | 含b鋼の製造方法 |
-
1975
- 1975-05-13 JP JP5547375A patent/JPS51131417A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS51131417A (en) | 1976-11-15 |