JPS5511138A - Preventing method for molten slag from running off during tapping - Google Patents

Preventing method for molten slag from running off during tapping

Info

Publication number
JPS5511138A
JPS5511138A JP8320178A JP8320178A JPS5511138A JP S5511138 A JPS5511138 A JP S5511138A JP 8320178 A JP8320178 A JP 8320178A JP 8320178 A JP8320178 A JP 8320178A JP S5511138 A JPS5511138 A JP S5511138A
Authority
JP
Japan
Prior art keywords
kneaded material
molten slag
converter
tapping
running
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP8320178A
Other languages
Japanese (ja)
Other versions
JPS56485B2 (en
Inventor
Toshikuni Kitaura
Masami Akai
Ikuzo Hamazaki
Kenichi Kinoshita
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Sumitomo Metal Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Industries Ltd filed Critical Sumitomo Metal Industries Ltd
Priority to JP8320178A priority Critical patent/JPS5511138A/en
Publication of JPS5511138A publication Critical patent/JPS5511138A/en
Publication of JPS56485B2 publication Critical patent/JPS56485B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE:To prevent molten slag from running off at early stage of tapping, by blocking the tapping hole of a refining vessel such as a converter with kneaded material composed of iron oxide such as mill scale and a binder, then by turning the vessel at the time of tapping in order to bring the kneaded material into contact with molten slag and steel so as to be melted. CONSTITUTION:A tapping hole 5 of a refining vessel 4, e.g., a converter, is blocked with kneaded material 1 composed of iron oxide such as mill scale etc. and a binder such as water glass or water. After completion of refining, the converter 4 is turned around so that the kneaded material 1 comes into contact with molten slag 2, then with molten steel until the converter arrives at the turning end point. Hereby, the kneaded material 1 is melted by the heat of the molten steel and falls off to open the tapping hole 5, so that the molten steel 3 is tapped in a rapid stream and received in a ladle 6.
JP8320178A 1978-07-07 1978-07-07 Preventing method for molten slag from running off during tapping Granted JPS5511138A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP8320178A JPS5511138A (en) 1978-07-07 1978-07-07 Preventing method for molten slag from running off during tapping

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP8320178A JPS5511138A (en) 1978-07-07 1978-07-07 Preventing method for molten slag from running off during tapping

Publications (2)

Publication Number Publication Date
JPS5511138A true JPS5511138A (en) 1980-01-25
JPS56485B2 JPS56485B2 (en) 1981-01-08

Family

ID=13795702

Family Applications (1)

Application Number Title Priority Date Filing Date
JP8320178A Granted JPS5511138A (en) 1978-07-07 1978-07-07 Preventing method for molten slag from running off during tapping

Country Status (1)

Country Link
JP (1) JPS5511138A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS59221903A (en) * 1983-05-31 1984-12-13 日立電線株式会社 Wire and cable
JPS6389558A (en) * 1986-10-02 1988-04-20 Dainichi Color & Chem Mfg Co Ltd Fluororesin composition

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS59221903A (en) * 1983-05-31 1984-12-13 日立電線株式会社 Wire and cable
JPH0126125B2 (en) * 1983-05-31 1989-05-22 Hitachi Cable
JPS6389558A (en) * 1986-10-02 1988-04-20 Dainichi Color & Chem Mfg Co Ltd Fluororesin composition

Also Published As

Publication number Publication date
JPS56485B2 (en) 1981-01-08

Similar Documents

Publication Publication Date Title
JPS5511138A (en) Preventing method for molten slag from running off during tapping
JPS5637249A (en) Glass for slag wool and its preparation
JPS5343019A (en) Refining method for steel with reduced slag formation
JPS51151204A (en) A cupola for melting metal with auxiliary fuel and refining with coke
JPS52108312A (en) Steel making with converter
JPS53117601A (en) Recovering method for valuable metals in stainless steel slag
JPS52134805A (en) Slag discharge prevention during converter tapping
JPS5438213A (en) Refining method for p,s type free cutting steel
JPS52126601A (en) Preliminary treatment of molten metal
JPS5358417A (en) Partitionary treating method for molten steel in steel-making furnace
JPS5741310A (en) Method and device for adding alloy iron during tapping of converter
JPS538310A (en) Reusing method of steel making slag
JPS5647511A (en) Refining steel
JPS52142607A (en) Automatic fluid discharge apparatus
Simmons Steelmaking Improvements Utilizing Ladle Furnace Technology
JPS5218407A (en) Process for treatment of molten iron slag
JPS5390118A (en) Steel-making method using formed synthetic slag and resulting indecreased amount of slag discharged
JPS523517A (en) Method of refining steel by deoxidation of iron oxide in molten steel in furnace with al and desulfurization of iron sulfide with ferro mang anese
JPS5387918A (en) Refining method for low nitrogen steel
JPS52128805A (en) Separation and removal of salg from molten metal
JPS5261109A (en) Converter operation method
JPS53147607A (en) Hole-wrapping machine for pig iron gate
JPS52133004A (en) Method and apparatus for separating molten metal from solid or semi/molten slag
Wasikowski Ladle Desulfurization--Phase I
JPS5244715A (en) Continuous method of refining molten iron alloy by using alkali metal compoun