JPS5425216A - Heat-treatment method for ni-based alloy - Google Patents
Heat-treatment method for ni-based alloyInfo
- Publication number
- JPS5425216A JPS5425216A JP9107977A JP9107977A JPS5425216A JP S5425216 A JPS5425216 A JP S5425216A JP 9107977 A JP9107977 A JP 9107977A JP 9107977 A JP9107977 A JP 9107977A JP S5425216 A JPS5425216 A JP S5425216A
- Authority
- JP
- Japan
- Prior art keywords
- based alloy
- heat
- treatment method
- treatment
- inconel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To increase resistance to intercrystalline stress corrosion cracking through the development of metal carbides in the grain boundary by a specified heat-treatment of a corrosion resistant Ni-based alloy such as inconel 600.
COPYRIGHT: (C)1979,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9107977A JPS5425216A (en) | 1977-07-29 | 1977-07-29 | Heat-treatment method for ni-based alloy |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9107977A JPS5425216A (en) | 1977-07-29 | 1977-07-29 | Heat-treatment method for ni-based alloy |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5425216A true JPS5425216A (en) | 1979-02-26 |
Family
ID=14016493
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP9107977A Pending JPS5425216A (en) | 1977-07-29 | 1977-07-29 | Heat-treatment method for ni-based alloy |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5425216A (en) |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS55125263A (en) * | 1979-03-20 | 1980-09-26 | Sumitomo Metal Ind Ltd | Manufacture of cr-containing ni alloy |
EP0109350A2 (en) | 1982-11-10 | 1984-05-23 | Mitsubishi Jukogyo Kabushiki Kaisha | Nickel-chromium alloy |
US4512820A (en) * | 1980-05-30 | 1985-04-23 | Hitachi, Ltd. | In-pile parts for nuclear reactor and method of heat treatment therefor |
JPS6267158A (en) * | 1985-09-18 | 1987-03-26 | Mitsubishi Heavy Ind Ltd | Method for preventing damage of heat exchanger tube by corrosion |
JPH03100148A (en) * | 1989-09-13 | 1991-04-25 | Sumitomo Metal Ind Ltd | Heat treatment for high cr-ni-base alloy |
KR100792395B1 (en) | 2007-09-14 | 2008-01-08 | 주식회사 삼진금속 | Menufacturing process of inconel tension stud bolt for a gas turbine |
-
1977
- 1977-07-29 JP JP9107977A patent/JPS5425216A/en active Pending
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS55125263A (en) * | 1979-03-20 | 1980-09-26 | Sumitomo Metal Ind Ltd | Manufacture of cr-containing ni alloy |
JPS5952699B2 (en) * | 1979-03-20 | 1984-12-21 | 住友金属工業株式会社 | Method for producing Ni-based alloy containing Cr |
US4512820A (en) * | 1980-05-30 | 1985-04-23 | Hitachi, Ltd. | In-pile parts for nuclear reactor and method of heat treatment therefor |
EP0109350A2 (en) | 1982-11-10 | 1984-05-23 | Mitsubishi Jukogyo Kabushiki Kaisha | Nickel-chromium alloy |
JPS6267158A (en) * | 1985-09-18 | 1987-03-26 | Mitsubishi Heavy Ind Ltd | Method for preventing damage of heat exchanger tube by corrosion |
JPH03100148A (en) * | 1989-09-13 | 1991-04-25 | Sumitomo Metal Ind Ltd | Heat treatment for high cr-ni-base alloy |
KR100792395B1 (en) | 2007-09-14 | 2008-01-08 | 주식회사 삼진금속 | Menufacturing process of inconel tension stud bolt for a gas turbine |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5431062A (en) | Manufacture of structure superior in stress corrosion cracking resistivity | |
JPS5425216A (en) | Heat-treatment method for ni-based alloy | |
JPS5260217A (en) | Watch case | |
JPS51143518A (en) | Wear resistant iron-base sintered alloy for rocker arm | |
JPS5335620A (en) | Heat-resisting ni base cast alloy | |
JPS5365783A (en) | Corrosion loss measuring method for metal in corrosive environment | |
JPS5367618A (en) | Copper alloy with excellent bending property, stress corrosion crackingresistance and workability | |
JPS538404A (en) | Means for preventing corrosion of turbine blade | |
JPS5348103A (en) | Manufacturing method for total-flow turbine blade | |
JPS5337513A (en) | Anti-corrosion material for chloroprence manufacturing plant | |
JPS5220324A (en) | Ni-base alloy excellent in both weldability and hot workability | |
JPS51148612A (en) | Process for the production of corrosion- resisting cu-alloy | |
JPS5210818A (en) | High ni-fe alloy of good productivity | |
JPS5370021A (en) | Wear resistant high permeability alloy | |
JPS5236510A (en) | Stress corrosion cracking resistant high silicon tough steel | |
JPS5428238A (en) | Watchcase | |
JPS52103307A (en) | Lightweight hard alloy for parts of hot rolling equipment | |
JPS539218A (en) | Abrasion resisting alloy | |
JPS5285910A (en) | High strength aluminium alloy of excellent stress corrosion cracking r esistence and hot workability | |
JPS53139098A (en) | Nuclear fuel element | |
JPS52102814A (en) | Corrosion resistant, high tensile al alloy for electroconductive use | |
JPS5210822A (en) | Stress corrosion cracking resistant high nickel alloy | |
JPS5273204A (en) | Fabrication of turbine blade | |
JPS5351102A (en) | Productn of corrosin resistant alloy | |
JPS52109414A (en) | Brilliant, corrosion resistant al alloy for die casting |