JPS5424A - Method of forming titanium oxide coating layer on glass surface - Google Patents
Method of forming titanium oxide coating layer on glass surfaceInfo
- Publication number
- JPS5424A JPS5424A JP6490277A JP6490277A JPS5424A JP S5424 A JPS5424 A JP S5424A JP 6490277 A JP6490277 A JP 6490277A JP 6490277 A JP6490277 A JP 6490277A JP S5424 A JPS5424 A JP S5424A
- Authority
- JP
- Japan
- Prior art keywords
- coating layer
- titanium oxide
- glass surface
- oxide coating
- forming titanium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Surface Treatment Of Glass (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6490277A JPS5424A (en) | 1977-06-03 | 1977-06-03 | Method of forming titanium oxide coating layer on glass surface |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6490277A JPS5424A (en) | 1977-06-03 | 1977-06-03 | Method of forming titanium oxide coating layer on glass surface |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5424A true JPS5424A (en) | 1979-01-05 |
JPS5618547B2 JPS5618547B2 (en) | 1981-04-30 |
Family
ID=13271453
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6490277A Granted JPS5424A (en) | 1977-06-03 | 1977-06-03 | Method of forming titanium oxide coating layer on glass surface |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5424A (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5666563A (en) * | 1979-10-23 | 1981-06-05 | Transamerica Delaval Inc | Pressure seal assembly |
JPS57172963U (en) * | 1981-04-27 | 1982-10-30 | ||
US5403368A (en) * | 1991-11-29 | 1995-04-04 | Central Glass Company, Limited | Metal oxide film having minutely roughed surface and method of forming same on glass substrate |
US5730771A (en) * | 1993-03-05 | 1998-03-24 | Glaverbel | Method of manufacturing a corrosion resistant pyrolytically coated glass |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6134336U (en) * | 1984-03-13 | 1986-03-03 | 開司 山口 | Cartridge type fuel tank |
-
1977
- 1977-06-03 JP JP6490277A patent/JPS5424A/en active Granted
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5666563A (en) * | 1979-10-23 | 1981-06-05 | Transamerica Delaval Inc | Pressure seal assembly |
JPS63180773U (en) * | 1979-10-23 | 1988-11-22 | ||
JPH0239088Y2 (en) * | 1979-10-23 | 1990-10-19 | ||
JPS57172963U (en) * | 1981-04-27 | 1982-10-30 | ||
JPS627030Y2 (en) * | 1981-04-27 | 1987-02-18 | ||
US5403368A (en) * | 1991-11-29 | 1995-04-04 | Central Glass Company, Limited | Metal oxide film having minutely roughed surface and method of forming same on glass substrate |
US5730771A (en) * | 1993-03-05 | 1998-03-24 | Glaverbel | Method of manufacturing a corrosion resistant pyrolytically coated glass |
Also Published As
Publication number | Publication date |
---|---|
JPS5618547B2 (en) | 1981-04-30 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS53100978A (en) | Method of forming tin oxide thin film coating layer on supporting body | |
JPS53133236A (en) | Method of forming multiicoating layers on substrate surface | |
JPS5341319A (en) | Method of coating surface of glass or ceramic | |
GB2018234B (en) | Method of coating glass surface with heatreflectice titanium oxide film | |
JPS56152965A (en) | Method of coating surface covered with oxide whisker | |
DE2861479D1 (en) | Method of coating glass surfaces | |
JPS53127534A (en) | Protective method of article surfaces by foullproof coating layer | |
JPS5419435A (en) | Method of forming highhtemperature protective coating layer | |
JPS5651268A (en) | Method of coating surface of glass | |
JPS5425A (en) | Method of chamfering glass substrate | |
JPS53128798A (en) | Method of forming transparent electroconductive coating | |
DE2861480D1 (en) | Method of coating glass surfaces | |
JPS5466914A (en) | Method of making metal oxide coated glass | |
JPS51134711A (en) | Method of producing glass having coating of titanium oxide | |
JPS5424A (en) | Method of forming titanium oxide coating layer on glass surface | |
JPS537716A (en) | Method of surface treatment of glass member | |
JPS5418823A (en) | Method of coating glass surface | |
JPS536314A (en) | Method of forming vapourrplated coating on glass | |
JPS5422426A (en) | Method of forming titanium oxide coating layer on glass surface | |
JPS5453125A (en) | Method of coating on glass surface | |
JPS52919A (en) | Method of depositing thin film of metallic oxide on glass surface | |
JPS5421409A (en) | Method of making tungstenncarbide coating layer | |
JPS5423614A (en) | Method of forming metal oxide coating layer on glass sheet surface | |
JPS532517A (en) | Method of surface treatment of glass substrate | |
JPS546876A (en) | Method of forming colored coat over metal surface |