JPS5417343A - Preventing method for ratigue crack caused in corrosive circumference - Google Patents
Preventing method for ratigue crack caused in corrosive circumferenceInfo
- Publication number
- JPS5417343A JPS5417343A JP8192877A JP8192877A JPS5417343A JP S5417343 A JPS5417343 A JP S5417343A JP 8192877 A JP8192877 A JP 8192877A JP 8192877 A JP8192877 A JP 8192877A JP S5417343 A JPS5417343 A JP S5417343A
- Authority
- JP
- Japan
- Prior art keywords
- ratigue
- corrosive
- circumference
- preventing method
- crack caused
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To simply, cheaply prevent the generation of the fatigue crack, by placting the metallic zinc nearby, or contacting to, the the weld zone or the portion, in which the stress is concentrating, of the steel parts of discontinuous shape.
COPYRIGHT: (C)1979,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8192877A JPS5417343A (en) | 1977-07-11 | 1977-07-11 | Preventing method for ratigue crack caused in corrosive circumference |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8192877A JPS5417343A (en) | 1977-07-11 | 1977-07-11 | Preventing method for ratigue crack caused in corrosive circumference |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5417343A true JPS5417343A (en) | 1979-02-08 |
Family
ID=13760115
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP8192877A Pending JPS5417343A (en) | 1977-07-11 | 1977-07-11 | Preventing method for ratigue crack caused in corrosive circumference |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5417343A (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58103098U (en) * | 1981-12-30 | 1983-07-13 | 日本ゼオン株式会社 | Fireproof flexible sound insulation sheet |
JPS58113099U (en) * | 1982-01-27 | 1983-08-02 | 日本ゼオン株式会社 | Fire-retardant sound-insulating plywood |
JPS6065463U (en) * | 1983-10-14 | 1985-05-09 | エヌ・オー・ケー・メグラステイツク株式会社 | pulley |
-
1977
- 1977-07-11 JP JP8192877A patent/JPS5417343A/en active Pending
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58103098U (en) * | 1981-12-30 | 1983-07-13 | 日本ゼオン株式会社 | Fireproof flexible sound insulation sheet |
JPS6331118Y2 (en) * | 1981-12-30 | 1988-08-19 | ||
JPS58113099U (en) * | 1982-01-27 | 1983-08-02 | 日本ゼオン株式会社 | Fire-retardant sound-insulating plywood |
JPS6331119Y2 (en) * | 1982-01-27 | 1988-08-19 | ||
JPS6065463U (en) * | 1983-10-14 | 1985-05-09 | エヌ・オー・ケー・メグラステイツク株式会社 | pulley |
JPH0122995Y2 (en) * | 1983-10-14 | 1989-07-13 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS51138511A (en) | Method for regulating the hardness of metallic tita nium | |
JPS5417343A (en) | Preventing method for ratigue crack caused in corrosive circumference | |
JPS5321021A (en) | Solution treatment method for pipe | |
JPS5365783A (en) | Corrosion loss measuring method for metal in corrosive environment | |
JPS53104531A (en) | Surface processing method decreasing stress corrosion cracking | |
JPS5413433A (en) | Welding method for stainless steel | |
JPS53130242A (en) | Welding method for manufacture of thick-walled large diameter welded steel pipe | |
JPS53149136A (en) | Corrosion preventing method for buried metal product | |
JPS53108838A (en) | Austenitic stainless steel welded joint | |
JPS53106361A (en) | Submerged arc welding method for steel plate | |
JPS5397964A (en) | Preparation of electric welded steel tube | |
JPS53131245A (en) | Welding method for martensitic stainless steel | |
JPS51120985A (en) | Method of ion plating a metal surface | |
JPS5411846A (en) | Welding means with low weld crack susceptibility and method of making same | |
JPS5411045A (en) | Preventing method for crack initiation of deposited metal | |
JPS5398621A (en) | Method of preventing corrosion of vehicle body | |
JPS5364809A (en) | Manufacturing method of crankshaft of compressor | |
JPS53134555A (en) | Outer blade for electric razor and its preparation method | |
JPS5351116A (en) | Forging method for heat resisting steel | |
JPS5413438A (en) | Percussion welding method | |
JPS53147643A (en) | Fillet weld coupling method with excellence in fatigue characteristic | |
JPS53142341A (en) | Welded structure | |
JPS51149817A (en) | Sprocket for vehicles | |
JPS5413434A (en) | Corrosion preventing method for welded steel tube | |
JPS5395142A (en) | Welding method of low alloy steel |