JPS541213A - Corrosion resitant aluminium alloy with moderate strength and excellence in extrusion workability - Google Patents
Corrosion resitant aluminium alloy with moderate strength and excellence in extrusion workabilityInfo
- Publication number
- JPS541213A JPS541213A JP6571377A JP6571377A JPS541213A JP S541213 A JPS541213 A JP S541213A JP 6571377 A JP6571377 A JP 6571377A JP 6571377 A JP6571377 A JP 6571377A JP S541213 A JPS541213 A JP S541213A
- Authority
- JP
- Japan
- Prior art keywords
- excellence
- resitant
- corrosion
- aluminium alloy
- moderate strength
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To provide an Al alloy with excellence in extrusion workability and a proper strength which permits use for structure through addition of Zn to an Al-Mg-Si alloy.
COPYRIGHT: (C)1979,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6571377A JPS594494B2 (en) | 1977-06-06 | 1977-06-06 | Medium-strength aluminum alloy with excellent extrudability |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6571377A JPS594494B2 (en) | 1977-06-06 | 1977-06-06 | Medium-strength aluminum alloy with excellent extrudability |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS541213A true JPS541213A (en) | 1979-01-08 |
JPS594494B2 JPS594494B2 (en) | 1984-01-30 |
Family
ID=13294924
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6571377A Expired JPS594494B2 (en) | 1977-06-06 | 1977-06-06 | Medium-strength aluminum alloy with excellent extrudability |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS594494B2 (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4868891A (en) * | 1987-03-27 | 1989-09-19 | Teletec Corporation | Interrupted audio fill-in system for noise reduction and intelligibility enhancement in multi-channel scanning receiver applications |
US6302973B1 (en) * | 1997-08-04 | 2001-10-16 | Corus Aluminium Walzprodukte Gmbh | High strength Al-Mg-Zn-Si alloy for welded structures and brazing application |
JP2011179107A (en) * | 2010-02-05 | 2011-09-15 | Furukawa-Sky Aluminum Corp | Aluminum alloy extrusion material for connectors excellent in extrusion properties and sacrificial anode properties |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6358796U (en) * | 1986-10-06 | 1988-04-19 |
-
1977
- 1977-06-06 JP JP6571377A patent/JPS594494B2/en not_active Expired
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4868891A (en) * | 1987-03-27 | 1989-09-19 | Teletec Corporation | Interrupted audio fill-in system for noise reduction and intelligibility enhancement in multi-channel scanning receiver applications |
US6302973B1 (en) * | 1997-08-04 | 2001-10-16 | Corus Aluminium Walzprodukte Gmbh | High strength Al-Mg-Zn-Si alloy for welded structures and brazing application |
JP2011179107A (en) * | 2010-02-05 | 2011-09-15 | Furukawa-Sky Aluminum Corp | Aluminum alloy extrusion material for connectors excellent in extrusion properties and sacrificial anode properties |
Also Published As
Publication number | Publication date |
---|---|
JPS594494B2 (en) | 1984-01-30 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
AU511765B2 (en) | Cathodic protection using marine aluminum alloy anode with core activator | |
AU7271381A (en) | Corrosion-resistant nickel alloy | |
JPS53100115A (en) | Aluminum alloy for galvanic anode | |
JPS541213A (en) | Corrosion resitant aluminium alloy with moderate strength and excellence in extrusion workability | |
JPS54101706A (en) | High tensile aluminium alloy for bearing | |
AU510657B2 (en) | Ductile corrosion resistant alloy | |
DE3070738D1 (en) | Corrosion resisting copper alloy | |
JPS5333909A (en) | Aluminium alloy with excellent machinability and corrosion resistance | |
JPS53110082A (en) | Copper-clad aluminum wire | |
JPS545810A (en) | Aluminium alloy for casting | |
JPS5419409A (en) | High strength aluminium alloy for die casting | |
JPS54126616A (en) | Aluminum alloy having improved corrosion resistance | |
JPS525487A (en) | Conjunction process of the anode oxidized cable and the electric | |
JPS53135811A (en) | Manufacture of electroductive aluminum alloy | |
JPS5499022A (en) | Aluminium alloy for anode | |
JPS5265707A (en) | Al-zn-mg type alloy and process for producing thereof | |
JPS53122786A (en) | Composite trolley cable | |
Baba | Stress Corrosion Cracking of Al-Zn-Mg Alloys | |
JPS51128824A (en) | Aluminum or aluminum alloy sash fixing method | |
JPS5222518A (en) | Method for compounding zinc-base alloy | |
JPS5314405A (en) | Pump | |
JPS5394230A (en) | Corrosion preventing method of aluminum heat exchanger | |
JPS5416317A (en) | Corrosion resistant aluminum alloy of superior machinability and manufacture therfor | |
JPS5376114A (en) | Manufacture of high strength aluminum alloy wire for electroconductive use | |
Baba et al. | Effects of Homogenizing an Ingot on the Ageing Characteristics and Stress Corrosion Cracking of Al-Zn-Mg and Al-Zn-Mg-Cu Alloys Containing Cr |