JPS5326932A - Method of producing sealed negative plate for alkaline battery - Google Patents
Method of producing sealed negative plate for alkaline batteryInfo
- Publication number
- JPS5326932A JPS5326932A JP10186376A JP10186376A JPS5326932A JP S5326932 A JPS5326932 A JP S5326932A JP 10186376 A JP10186376 A JP 10186376A JP 10186376 A JP10186376 A JP 10186376A JP S5326932 A JPS5326932 A JP S5326932A
- Authority
- JP
- Japan
- Prior art keywords
- negative plate
- alkaline battery
- producing sealed
- sealed negative
- producing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- Y02E60/12—
Landscapes
- Sealing Battery Cases Or Jackets (AREA)
- Primary Cells (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10186376A JPS5326932A (en) | 1976-08-26 | 1976-08-26 | Method of producing sealed negative plate for alkaline battery |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10186376A JPS5326932A (en) | 1976-08-26 | 1976-08-26 | Method of producing sealed negative plate for alkaline battery |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5326932A true JPS5326932A (en) | 1978-03-13 |
JPS5631052B2 JPS5631052B2 (en) | 1981-07-18 |
Family
ID=14311830
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP10186376A Granted JPS5326932A (en) | 1976-08-26 | 1976-08-26 | Method of producing sealed negative plate for alkaline battery |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5326932A (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS54139229U (en) * | 1978-03-20 | 1979-09-27 | ||
US5306580A (en) * | 1992-03-09 | 1994-04-26 | Eveready Battery Company, Inc. | Electrochemical cell having a coated cup-shaped terminal |
WO1995011527A1 (en) * | 1993-10-22 | 1995-04-27 | Toyo Kohan Co., Ltd. | Surface-treated steel sheet for battery case and battery case |
US7914926B2 (en) | 2005-03-17 | 2011-03-29 | Hitachi Maxell, Ltd. | Flat-shaped battery |
-
1976
- 1976-08-26 JP JP10186376A patent/JPS5326932A/en active Granted
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS54139229U (en) * | 1978-03-20 | 1979-09-27 | ||
US5306580A (en) * | 1992-03-09 | 1994-04-26 | Eveready Battery Company, Inc. | Electrochemical cell having a coated cup-shaped terminal |
WO1995011527A1 (en) * | 1993-10-22 | 1995-04-27 | Toyo Kohan Co., Ltd. | Surface-treated steel sheet for battery case and battery case |
KR100292173B1 (en) * | 1993-10-22 | 2001-06-01 | 다나베 히로까즈 | Surface-treated steel sheet for battery, manufacturing method thereof, battery case, and battery using the battery case |
CN1090384C (en) * | 1993-10-22 | 2002-09-04 | 东洋钢板株式会社 | Surface-treated steel sheet for battery case and battery case |
US7914926B2 (en) | 2005-03-17 | 2011-03-29 | Hitachi Maxell, Ltd. | Flat-shaped battery |
Also Published As
Publication number | Publication date |
---|---|
JPS5631052B2 (en) | 1981-07-18 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5326932A (en) | Method of producing sealed negative plate for alkaline battery | |
JPS5336641A (en) | Method of producing lead battery plate | |
JPS5339440A (en) | Method of producing battery plate | |
JPS531830A (en) | Method of producing lead battery plate | |
JPS5281520A (en) | Method of producing sealed negative plate for alkaline battery | |
JPS531827A (en) | Method of producing lead battery positive plate | |
JPS531829A (en) | Method of producing lead battery plate | |
JPS51116947A (en) | Method of producing cadmium negative plate for sealed alkaline battery | |
JPS52114931A (en) | Method of manufacturing negative electrode plate for alkaline battery | |
JPS531828A (en) | Method of producing lead battery positive plate | |
JPS5281521A (en) | Method of producing sealed negative plate for alkaline battery | |
JPS528435A (en) | Method of producing negative plate for alkaline battery | |
JPS5261736A (en) | Method of producing negative plate for alkaline battery | |
JPS51149540A (en) | Method of producing negative plate for alkaline battery | |
JPS52144745A (en) | Method of producing lead battery plate | |
JPS5271641A (en) | Method of producing lead battery plate | |
JPS5358630A (en) | Method of producing lead battery paste negative plate | |
JPS5441433A (en) | Method of producing cadmium negative plate of alkaline battery | |
JPS5325836A (en) | Method of producing battery plate | |
JPS5342340A (en) | Method of producing battery plate | |
JPS5261737A (en) | Method of producing cadmium negative plate for alkaline battery | |
JPS5253237A (en) | Method of partially charging sealed alkaline battery negative plate | |
JPS5210533A (en) | Method of partially charging negative plate for sealed alkaline battery | |
JPS5340832A (en) | Method of producing lead battery positive plate | |
JPS5353743A (en) | Method of producing lead battery positive plate |