JPS5321797A - Titanic acid barium semiconductor ceramic material - Google Patents
Titanic acid barium semiconductor ceramic materialInfo
- Publication number
- JPS5321797A JPS5321797A JP9633476A JP9633476A JPS5321797A JP S5321797 A JPS5321797 A JP S5321797A JP 9633476 A JP9633476 A JP 9633476A JP 9633476 A JP9633476 A JP 9633476A JP S5321797 A JPS5321797 A JP S5321797A
- Authority
- JP
- Japan
- Prior art keywords
- ceramic material
- titanic acid
- semiconductor ceramic
- acid barium
- barium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Thermistors And Varistors (AREA)
- Compositions Of Oxide Ceramics (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9633476A JPS5321797A (en) | 1976-08-11 | 1976-08-11 | Titanic acid barium semiconductor ceramic material |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9633476A JPS5321797A (en) | 1976-08-11 | 1976-08-11 | Titanic acid barium semiconductor ceramic material |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5321797A true JPS5321797A (en) | 1978-02-28 |
Family
ID=14162107
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP9633476A Pending JPS5321797A (en) | 1976-08-11 | 1976-08-11 | Titanic acid barium semiconductor ceramic material |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5321797A (ja) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS61232993A (ja) * | 1985-04-08 | 1986-10-17 | Tokyo Keiki Co Ltd | 自動操船装置 |
US5453262A (en) * | 1988-12-09 | 1995-09-26 | Battelle Memorial Institute | Continuous process for production of ceramic powders with controlled morphology |
-
1976
- 1976-08-11 JP JP9633476A patent/JPS5321797A/ja active Pending
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS61232993A (ja) * | 1985-04-08 | 1986-10-17 | Tokyo Keiki Co Ltd | 自動操船装置 |
JPH0438635B2 (ja) * | 1985-04-08 | 1992-06-25 | ||
US5453262A (en) * | 1988-12-09 | 1995-09-26 | Battelle Memorial Institute | Continuous process for production of ceramic powders with controlled morphology |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5324600A (en) | Nonnreducing dielectric ceramic composition | |
AU500991B2 (en) | Ceramic material | |
NZ192707A (en) | Wafers manufacture | |
JPS52147607A (en) | Manufacture of ceramic materials | |
IE801825L (en) | Semiconductor manufacture | |
JPS52140512A (en) | Manufacture of high ionnconductive ceramics | |
JPS5325899A (en) | Dielectric ceramic composition | |
GB1543551A (en) | Calcining solid materials | |
JPS5321797A (en) | Titanic acid barium semiconductor ceramic material | |
JPS5329599A (en) | Dielectric ceramic composition | |
JPS54124972A (en) | Semiconductor lead material | |
JPS52118597A (en) | Semiconductor ceramic base | |
JPS5546524A (en) | Barium titanate semiconductor porcelain | |
JPS531897A (en) | Titanic acid barium semiconductor ceramic material | |
JPS531896A (en) | Titanic acid barium semiconductor porcelain material | |
JPS5375495A (en) | Semiconductor ceramic material in barium titanate group | |
JPS5321796A (en) | Titanic acid barium semiconductor ceranic material | |
JPS5378906A (en) | Batch type rotary kiln | |
JPS53114100A (en) | Ceramic material for reduction type semiconductor condenser | |
ZA754942B (en) | Ceramic material | |
JPS5378907A (en) | Batch type rotary kiln | |
JPS5659675A (en) | Manufacture of barium titanate semiconductor ceramic | |
JPS5659678A (en) | Manufacture of barium titanate semiconductor ceramic | |
JPS53104898A (en) | Ceramic material for semiconductor | |
JPS533408A (en) | Manufacture of superrhard heattresisting ceramic materials |